摘要
A 3D numerical model of heat transfer and fluid flow of molten pool in the process of laser wire deposition was presented by computational fluid dynamics technique. The simulation results of the deposition morphology were also compared with the experimental results under the condition of liquid bridge transfer mode. Moreover, they showed a good agreement. Considering the effect of recoil pressure, the morphology of the deposit metal obtained by the simulation was similar to the experiment result. Molten metal at the wire tip was peeled off and flowed into the molten pool, and then spread to both sides of the deposition layer under the recoil pressure. In addition, the results of simulation and high-speed charge-coupled device presented that a wedge transition zone, with a length of similar to 6 mm, was formed behind the keyhole in the liquid bridge transfer process, where the height of deposited metal decreased gradually. After solidification, metal in the transition zone retained the original melt morphology, resulting in a decrease in the height of the tail of the deposition layer.
引用
收藏
页码:661 / 673
页数:13
相关论文
共 50 条
  • [1] Underwater wire-feed laser deposition of the Ti-6Al-4V titanium alloy
    Fu, Yunlong
    Guo, Ning
    Zhou, Li
    Cheng, Qi
    Feng, Jicai
    MATERIALS & DESIGN, 2020, 186
  • [2] Effect of manganese on grain morphology and microstructure of Ti-6Al-4V alloy by laser wire deposition
    Wang, Xiang
    Zhang, Lin-Jie
    Na, Suck-Joo
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 1141 - 1151
  • [3] Laser Wire Deposition of a Large Ti-6Al-4V Space Component
    Chekir, N.
    Sixsmith, J. J.
    Tollett, R.
    Brochu, M.
    WELDING JOURNAL, 2019, 98 (06) : 172S - 180S
  • [5] Microstructure and properties of Ti-6Al-4V titanium alloy prepared by underwater wire feeding laser deposition
    Guo, Ning
    Wu, Di
    Yu, Mengqiu
    Yin, Peng
    Cheng, Qi
    Wang, Guanghui
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 73 : 269 - 278
  • [6] BOUND METAL DEPOSITION OF Ti-6Al-4V ALLOY
    Tuncer, Nihan
    Reidy, John P.
    Jorgensen, Luke
    Bose, Animesh
    INTERNATIONAL JOURNAL OF POWDER METALLURGY, 2024, 60 (01):
  • [7] Laser Deposition of Ti-6Al-4V Wire with WC Powder for Functionally Graded Components
    Farayibi, P. K.
    Folkes, J. A.
    Clare, A. T.
    MATERIALS AND MANUFACTURING PROCESSES, 2013, 28 (05) : 514 - 518
  • [8] Laser gas nitriding of Ti-6Al-4V alloy
    Xue, L
    Islam, MU
    Koul, AK
    Wallace, W
    Bibby, M
    MATERIALS AND MANUFACTURING PROCESSES, 1997, 12 (05) : 799 - 817
  • [9] Laser Powder Cladding of Ti-6Al-4V / Alloy
    Ali, Samar Reda Al-Sayed
    Hussein, Abdel Hamid Ahmed
    Nofal, Adel Abdel Menam Saleh
    Elnaby, Salah Elden Ibrahim Hasseb
    Elgazzar, Haytham Abdelrafea
    Sabour, Hassan Abdel
    MATERIALS, 2017, 10 (10):
  • [10] Laser shock processing of Ti-6Al-4V alloy
    Yilbas, BS
    Gondal, MA
    Arif, AMF
    Shuja, SZ
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2004, 218 (05) : 473 - 482