Critical Current Degradation and Joint Resistance Rise of REBCO Tape and Coil During Heat Treatment

被引:0
|
作者
Peng, Weihang [1 ]
Li, Ke [2 ]
Nan, Jinrui [3 ]
Wang, Yawei [1 ]
Fu, Yutong [1 ]
Yang, Longhao [1 ]
Zhao, Yue [1 ]
Jin, Zhijian [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Elect Informat & Elect Engn, Shanghai 200240, Peoples R China
[2] State Grid Corp China, East China Branch, Shanghai 200120, Peoples R China
[3] Beijing Inst Technol, Sch Mech Engn, Beijing 10081, Peoples R China
基金
中国国家自然科学基金;
关键词
Heat treatment; Copper; Resistance heating; Degradation; Superconducting magnets; Superconducting films; Resistance; REBCO; heat treatment; critical current degradation; coil joint resistance;
D O I
10.1109/TASC.2023.3344412
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
High temperature superconducting (HTS) REBCO tape has great advantages on high field magnets due to its high critical current density and superior mechanical strength. It is inevitably exposed to high temperatures during certain stages of coil manufacturing, such as joint welding and coil impregnation, which can potentially result in a decrease in the critical current of the coils and an increase in the joint resistance. In this paper, this issue is studied by measurement using three post-processing types of REBCO tapes: copper-plated tapes, tin-coated tapes, and copper-laminated tapes. To simulate possible heat treatment conditions, the samples are heated to between 105 C-degrees and 265 C-degrees in different atmospheres for durations ranging from 1 min to 4 h, and then the critical current of the tapes and coils are investigated at 77 K. Its influences on the REBCO-to-Skeleton joint resistance are also investigated. The results show that heat treatments below 185 C-degrees with a duration of less than 60 min are suitable for common heat treatment processes due to a critical current degradation of less than 5%. For short heat treatment (duration < 60 min), the tin-coated tape may have a smaller critical current decay. The REBCO-to-Skeleton joint resistance of coils increases with increasing heat treatment temperature and duration, and an internal joint welding method is proposed that has little effect on the critical current of the coil (degradation < 3%).
引用
收藏
页码:1 / 6
页数:6
相关论文
共 50 条
  • [1] Experimental study on the an-isotropic critical current of REBCO tape
    Ma, Hongjun
    Zhang, Jingfeng
    Zhang, Shuqing
    Zhang, Xintao
    Liu, Huajun
    Liu, Fang
    Shi, Yi
    Jin, Huan
    REVIEW OF SCIENTIFIC INSTRUMENTS, 2024, 95 (03):
  • [2] REBCO Soldered Lap Joint Resistance Versus Length and Tape Manufacturer
    Marshall, William. S.
    Abraimov, Mikhail
    Lu, Jun
    Gavin, Noah
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2025, 35 (05)
  • [3] Resistance and Voltage-Current Characteristics of REBCO Superconducting Joint
    Takeda, Yasuaki
    Nishijima, Gen
    Kitaguchi, Hitoshi
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2025, 35 (05)
  • [4] Influence of Edge Crack Propagation on Critical Current Degradation of REBCO Tape Studied by Phase-Field Fracture Method and Current Shunting Model
    Jiang, Zhaofei
    Huang, Yiqun
    Jiang, Donghui
    Chen, Wenge
    Kuang, Guangli
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2023, 33 (02)
  • [5] Quench transient current and quench propagation limit in pancake wound REBCO coils as a function of contact resistance, critical current, and coil size
    Markiewicz, Denis
    Painter, Thomas
    Dixon, Iain
    Bird, Mark
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2019, 32 (10):
  • [6] Axial Compressive Stress Dependence of Critical Current of REBCO Double-Pancake Coil
    Nagasaki, Yoh
    Sasaki, Satoshi
    Maruyama, Masaki
    Miyagi, Daisuke
    Tsuda, Makoto
    Miura, Hideaki
    Yokoyama, Shoichi
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2021, 31 (05)
  • [7] Critical current degradation behaviour of various REBCO tapes under uniaxial strain
    Xiao, Guanyu
    Zhou, Chao
    Qin, Jinggang
    Jin, Huan
    Liu, Haihong
    Zhao, Chuanyi
    FUSION ENGINEERING AND DESIGN, 2023, 190
  • [8] Critical current degradation of commercial REBCO coated conductors under thermomechanical loads
    Lucas, Celia
    Cayado, Pablo
    Rijckaert, Hannes
    Konstantopoulou, Konstantina
    Nardelli, Davide
    Senatore, Carmine
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2024, 37 (12):
  • [9] Critical Current Estimation of HTS Coil Considering the Tape Inhomogeneity and Different Criteria
    Gong, Tianyong
    Ma, Guangtong
    Xiao, Ling
    Li, Jing
    Zhou, Pengbo
    Xie, Pengyang
    Liu, Boqiang
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2022, 32 (06)
  • [10] AC Loss Characteristics of a Double Pancake Coil Wound With Multifilamentary REBCO Tape With High Inter-Filament Resistance
    Oishi, Ryoma
    Jingami, Koudai
    Nishida, Yuji
    Himeno, Yuuki
    Kashiwagi, Ryota
    Sasa, Hiromasa
    Yoshida, Koichi
    Miyazaki, Hiroshi
    Iwakuma, Masataka
    Hirose, Hishiro T.
    Izumi, Teruo
    Machi, Takato
    Nakamura, Miyuki
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2025, 35 (05)