Effect of surface treatments on optical, topographical and mechanical properties of CAD/CAM reinforced lithium silicate glass ceramics

被引:5
|
作者
Al-Johani, Hanan [1 ,2 ]
Haider, Julfikar [1 ,3 ]
Silikas, Nick [1 ,4 ]
Satterthwaite, Julian [1 ]
机构
[1] Univ Manchester, Sch Med Sci, Div Dent, Manchester, England
[2] King Abdulaziz Univ, Dept Restorat Dent, Fac Dent, Div Biomat, Jeddah, Saudi Arabia
[3] Manchester Metropolitan Univ, Dept Engn, Manchester, England
[4] Univ Manchester, Sch Med Sci, Coupland 3 Bldg,Oxford Rd, Manchester M13 9PL, England
关键词
CAD/CAM Ceramic; Lithium disilicate; Zirconia-reinforced lithium silicate; Lithium aluminum disilicate; Surface treatment; Acid neutralization; Photometry; Topography; Biaxial flexural strength; MICROTENSILE BOND STRENGTH; 3 BALLS TEST; HYDROFLUORIC-ACID; FLEXURAL STRENGTH; PARTICLE ABRASION; RESIN BOND; TRANSLUCENCY; THICKNESS; ADHESION; RESPECT;
D O I
10.1016/j.dental.2023.07.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To investigate the effect of different surface treatments on optical, topographical and mechanical properties of CAD/CAM lithium silicate-based glass ceramics (LSC's) and their combined effect on the output of a light curing unit (LCU). Methods: Four CAD/CAM LSC's were investigated: Lithium Disilicate (Emax CAD; EC), Zirconia-reinforced silicates (Vita Suprinity; VS and Celtra Duo;CD) and Lithium Aluminum Disilicate (CEREC Tessera; CT). Ceramic specimens (n = 240) were divided into six subgroups according to their surface treatment: (a) Control, (b) Hydrofluoric acid (HF) 5%, (c) HF 5% + Neutralizing agent (N), (d) HF 9%, (e) HF 9% +N and (f) Self-etching ceramic primer (SEP). Irradiance, power and radiant exposure of a LCU were measured with MARC-LC following ceramic specimen interposition. Direct light transmission (T%) and absorbance (Abs%) of the specimens were measured with UV-Vis spectrophotometry. Roughness (Sa, Sq) and wettability (theta degrees) were measured with optical profilometry and sessile drop profile analysis, respectively. Biaxial flexural strength (sigma) of the ceramic specimens was measured by the ball-on-three-balls method and ceramic specimens were examined microscopically. Statistical analyses was performed by two-way ANOVA followed by post hoc multiple comparisons (alpha = 0.05). Results: Acid neutralization decreased T% and increased Abs% in all LSC's and highest T% was exhibited with VS. Neutralized EC, VS and CD displayed higher Sa in HF9, while neutralized CT displayed higher Sa in HF5. Self-etch primer significantly reduced theta degrees (p < 0.001). sigma was observed in the followed ascending order: HF9 +N < HF9 < HF5 +N < HF5 < SEP < Control for all LSC's. Significance: Optical, topographical and mechanical properties of the CAD/CAM ceramic blocks were strongly dependent on the type of surface treatment. Results of neutralization post-etching indicate promising potential for future investigations.
引用
下载
收藏
页码:779 / 789
页数:11
相关论文
共 50 条
  • [1] Lithium disilicate and zirconia reinforced lithium silicate glass-ceramics for CAD/CAM dental restorations: biocompatibility, mechanical and microstructural properties after crystallization
    Mavriqi, Luan
    Valente, Francesco
    Murmura, Giovanna
    Sinjari, Bruna
    Macri, Monica
    Trubiani, Oriana
    Caputi, Sergio
    Traini, Tonino
    JOURNAL OF DENTISTRY, 2022, 119
  • [2] The Effect of Different Surface Treatments on the Micromorphology and the Roughness of Four Dental CAD/CAM Lithium Silicate-Based Glass-Ceramics
    Bebsh, Muna
    Haimeur, Asmaa
    Franca, Rodrigo
    CERAMICS-SWITZERLAND, 2021, 4 (03): : 467 - 475
  • [3] Effect of Thermocycling, Surface Treatments and Microstructure on the Optical Properties and Roughness of CAD-CAM and Heat-Pressed Glass Ceramics
    Vasiliu, Roxana-Diana
    Porojan, Sorin Daniel
    Birdeanu, Mihaela Ionela
    Porojan, Liliana
    MATERIALS, 2020, 13 (02)
  • [4] Effect of repeated firing on the topographical, optical, and mechanical properties of fully crystallized lithium silicate-based ceramics
    Al-Johani, Hanan
    Haider, Julfikar
    Silikas, Nick
    Satterthwaite, Julian
    JOURNAL OF PROSTHETIC DENTISTRY, 2024, 131 (04): : 741.e1 - 741.e11
  • [5] Effect of solarization on mechanical properties of lithium silicate glass-ceramics
    Mohaghegh, E.
    Yekta, B. Eftekhari
    Marghusian, V. K.
    Khosraviani, A.
    JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2017, 53 (02) : 385 - 390
  • [6] Effect of solarization on mechanical properties of lithium silicate glass-ceramics
    E. Mohaghegh
    B. Eftekhari Yekta
    V. K. Marghusian
    A. Khosraviani
    Journal of the Australian Ceramic Society, 2017, 53 : 385 - 390
  • [7] Microstructural and mechanical analysis of two CAD-CAM lithium disilicate glass-reinforced ceramics
    Tavares, Lucas do Nascimento
    Zancope, Karla
    Almeida Silva, Anielle Christine
    Araujo Raposo, Luis Henrique
    Soares, Carlos Jose
    das Neves, Flavio Domingues
    BRAZILIAN ORAL RESEARCH, 2020, 34
  • [8] The Effect of Surface Treatments on the Mechanical and Optical Behaviors of CAD/CAM Restorative Materials
    Kurtulmus-Yilmaz, Sevcan
    Cengiz, Esra
    Ongun, Salim
    Karakaya, Izgen
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (02): : E496 - E503
  • [9] Load effect on the mechanical behaviour of zirconia-reinforced lithium silicate glass ceramics
    Alao, Abdur-Rasheed
    Haziq, Muhammad
    CERAMICS INTERNATIONAL, 2021, 47 (01) : 1353 - 1363
  • [10] Influence of microstructure on optical properties of CAD-CAM lithium disilicate glass-ceramics
    Pecho, Oscar E.
    Alvarez-Lloret, Pedro
    Ionescu, Ana M.
    Cardona, Juan C.
    Ghinea, Razvan
    Sánchez-Sánchez, Purificación
    Perez, Maria M.
    Della Bona, Alvaro
    Dental Materials, 2024, 40 (11) : 1927 - 1936