The influence of grinding process on the mechanical behavior of SiC/SiC composite tubes under uniaxial tension

被引:5
|
作者
Morel, C. [1 ,2 ,3 ]
Baranger, E. [2 ]
Lamon, J. [2 ]
Marques, C. [1 ]
Le Bras, S. [1 ]
Braun, J. [4 ]
Lorrette, C. [1 ]
机构
[1] Univ Paris Saclay, CEA, Serv Rech Mat & Proc Avances, F-91191 Gif Sur Yvette, France
[2] Univ Paris Saclay, CentraleSupelec, CNRS, LMPS Lab Mecan,ENS Paris Saclay, 4 Ave Sci, F-91190 Gif Sur Yvette, France
[3] Univ Toulouse, Inst Clement Ader, CNRS, UMR 5312, 3 Rue Caroline Aigle, F-31400 Toulouse, France
[4] CEA, DAM, BP16, F-37260 Monts, France
关键词
Ceramic-matrix composites (CMCs); Mechanical properties; Defects; Grinding process; CERAMIC-MATRIX COMPOSITES; HYSTERESIS MEASUREMENTS; CONSTITUENT PROPERTIES; FIBER; DAMAGE; FRACTURE;
D O I
10.1016/j.jeurceramsoc.2023.07.067
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiC/SiC composites are candidates of interest for fuel cladding applications in pressurized light-water reactors. In this study, fuel cladding tubes were made by filament winding and the matrix was deposited by CVI (Chemical Vapour Infiltration), which results in surface irregularities and waviness defects. This paper examines the influence of grinding steps on the mechanical behavior of tube specimens. Different depths of inner and outer surface grinding are carried out from a reference grade. Cyclic tensile tests are then performed. Elastic behavior analysis shows that the machining of tubes does not cause pre-damage. Analysis of unload-reload cycles indicates that the internal slippage does not depend on the seal coat thickness and that the surface quality weakly influences damage in the loading direction. Damage in the shear plane and ultimate failure strength strongly depend on the inner seal coat thickness.
引用
收藏
页码:91 / 106
页数:16
相关论文
共 50 条
  • [1] The influence of internal defects on the mechanical behavior of filament wound SiC/SiC composite tubes under uniaxial tension
    Morel, C.
    Baranger, E.
    Lamon, J.
    Braun, J.
    Lorrette, C.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (05) : 1797 - 1807
  • [2] In-plane mechanical behavior and failure mode of a 2D-SiC/SiC composite under uniaxial dynamic compression
    Wang, Yanpei
    Li, Yulong
    Suo, Tao
    Luan, Xingang
    Zhou, Ding
    Zakir, Sheikh Muhammad
    Chen, Chunyang
    Liu, Huifang
    Duan, Yu
    CERAMICS INTERNATIONAL, 2018, 44 (16) : 20058 - 20068
  • [3] Fracture of SiC tubes under combined tension/torsion
    Wang, FH
    Lu, MX
    Zheng, XL
    Pan, YJ
    INTERNATIONAL JOURNAL OF FRACTURE, 1996, 80 (2-3) : R49 - R54
  • [4] Tension-tension fatigue behavior of a PIP SiC/SiC composite at elevated temperature in air
    Luo, Zheng
    Cao, He
    Ren, Hu
    Zhou, Xingui
    CERAMICS INTERNATIONAL, 2016, 42 (02) : 3250 - 3260
  • [5] Molecular dynamics simulation of β-SiC nanowire under uniaxial tension
    Han, Tongwei
    He, Pengfei
    Wang, Jian
    Zheng, Bailin
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2009, 23 (04): : 337 - 342
  • [6] Hermetic SiC-SiC composite tubes
    Kowbel, W
    Liu, Y
    Bruce, C
    Withers, JC
    Kolaya, LE
    Lewis, N
    ADVANCES IN CERAMIC MATRIX COMPOSITES IV, 1999, 96 : 77 - 88
  • [7] Influence of the carbon interface on the mechanical behavior of SiC/SiC composites
    Fellah, C.
    Braun, J.
    Sauder, C.
    Sirotti, F.
    Berger, M-H
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2020, 133
  • [8] Anisotropic damage behavior of SiC/SiC composite tubes: Multiaxial testing and damage characterization
    Bernachy-Barbe, Fabien
    Gelebart, Lionel
    Bornert, Michel
    Crepin, Jerome
    Sauder, Cedric
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 76 : 281 - 288
  • [9] Influence of SiC coating thickness on mechanical properties of SiCf/SiC composite
    Yu, Haijiao
    Zhou, Xingui
    Zhang, Wei
    Peng, Huaxin
    Zhang, Changrui
    JOURNAL OF NUCLEAR MATERIALS, 2013, 442 (1-3) : 53 - 59
  • [10] Stress rupture of SiC/SiC composite tubes under high-temperature steam
    Koyanagi, Takaaki
    Karakoc, Omer
    Hawkins, Charles
    Lara-Curzio, Edgar
    Deck, Christian
    Katoh, Yutai
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2023, 20 (03) : 1658 - 1666