Influence of cooling rate on the microstructure and mechanical properties of Al-Cu-Li-Mg-Zn alloy

被引:7
|
作者
Yang, Qingbo [1 ,2 ]
Shi, Wenjing [1 ]
Wang, Miao [2 ]
Jia, Lina [1 ,2 ]
Wang, Wenbo [2 ]
Zhang, Hu [1 ,2 ]
机构
[1] Beihang Univ, Res Inst Frontier Sci, Beijing 100191, Peoples R China
[2] Beihang Univ, Ningbo Inst Technol, Res Ctr Lightweight Mat, Ningbo 315100, Peoples R China
关键词
Al-Cu-Li alloy; Cooling rate; Mechanical property; Microstructure; Secondary phase; HOT TEARING SUSCEPTIBILITY; GRAIN-SIZE; VOLUME FRACTION; BEHAVIOR; SOLIDIFICATION; MICROSEGREGATION; MORPHOLOGY; CORROSION; PHASE; FE;
D O I
10.1016/j.jmrt.2023.06.094
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work investigated the influence of cooling rate (0.04, 0.87, 15.2 and 156.2 K/s) on the microstructure and compressive properties of Al-4Cu-3Li-0.7 Mg-1Zn alloys fabricated by several casting molds. The experiment results revealed that the microstructure cooled at low cooling rates of 0.04, 0.87 and 15.2 K/s is composed of a-Al, a(Al)+T2, q (Al2Cu), T1 phases and core-shell configuration (Al13Fe4/Al7Cu2Fe phase). This core-shell structure is observed for the first time in an Al-Cu-Li alloy. However, T1 and core-shell configuration vanish at the high cooling rate of 156.2 K/s due to the insufficient diffusion time of Cu, Li and Fe elements. As the cooling rate increases, the average secondary dendrite arm spacing (SDAS) decreases significantly from 110.3 to 7.5 mm and the relationship between SDAS and cooling rate has been established. The average diameter/thickness of the a(Al)+ T2, Al2Cu and Al13Fe4/Al7Cu2Fe phases decreases dramatically from 16.9 to 1.0 mm, 8.1 to 0.8 mm and 7.5 to 0.7 mm with the increase of cooling rate, respectively. Fine spherical Al13Fe4/Al7Cu2Fe and Al2Cu phases are beneficial to the improvement of comprehensive compressive properties. Additionally, the solute concentration in the matrix decreases, while the hot-tear resistance and volume fraction of secondary phases increase with increasing cooling rate. The empirical equations are established between (compressive properties, SDAS) and cooling rate. The fracture failure is responsible for the initial hot tearing at low cooling rates, the a(Al)+T2 or Al2Cu or Al13Fe4/Al7Cu2Fe phases at the moderate cooling rate, and the a(Al)+T2 phase at the high cooling rate. (c) 2023 Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND
引用
收藏
页码:3151 / 3166
页数:16
相关论文
共 50 条
  • [1] Improvement of microstructure and mechanical properties of Al-Cu-Li-Mg-Zn alloys through water-cooling centrifugal casting technique
    YANG, Qing-bo
    SHI, Wen-jing
    LIU, Wen
    WANG, Miao
    WANG, Wen-bo
    JIA, Li-na
    ZHANG, Hu
    Transactions of Nonferrous Metals Society of China (English Edition), 2024, 34 (11): : 3486 - 3503
  • [2] Effect of cooling aging on microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy
    Liu, Yan
    Jiang, Daming
    Li, Bingqing
    Yang, Wenshu
    Hu, Jie
    MATERIALS & DESIGN, 2014, 57 : 79 - 86
  • [3] Influence of Zr on the microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy
    Yang, Shoujie
    Xie, Youhua
    Dai, Shenglong
    Yan, Minggao
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1069 - +
  • [4] Effect of cooling rate on microstructure and mechanical properties of an Al-5.0Mg-3.0Zn-1.0Cu cast alloy
    Tang, Hua-Ping
    Wang, Qu-Dong
    Lei, Chuan
    Ye, Bing
    Wang, Kui
    Jiang, Hai-Yan
    Ding, Wen Jiang
    Zhang, Xiang-Feng
    Lin, Zhen
    Zhang, Ji-Bin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 801 : 596 - 608
  • [5] Effect of cooling rate on microstructure and mechanical properties of squeeze cast Al-Cu-Mg alloy
    Gan, Y.
    Zhang, D.
    Zhang, W.
    Li, Y.
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2015, 28 (01) : 50 - 58
  • [6] Influence of Cu/Mg ratio on microstructure and mechanical properties of Al–Zn–Mg–Cu alloys
    Shilong Wei
    Richu Wang
    Hui Zhang
    Chunting Xu
    Ying Wu
    Yan Feng
    Journal of Materials Science, 2021, 56 : 3472 - 3487
  • [7] Microstructure and Mechanical Properties of Superlight Mg-Li-Al-Zn Wrought Alloy
    Xu Tiancai
    Peng Xiaodong
    Jiang Junwei
    Wei Guobing
    Zhang Bao
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (08) : 1815 - 1820
  • [8] Microstructure and mechanical properties of superlight Mg-Li-Al-Zn wrought alloy
    Xu, Tiancai
    Peng, Xiaodong
    Jiang, Junwei
    Wei, Guobing
    Zhang, Bao
    Peng, Xiaodong, 1815, Science Press (43): : 1815 - 1820
  • [9] Influence of Cu/Mg ratio on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys
    Wei, Shilong
    Wang, Richu
    Zhang, Hui
    Xu, Chunting
    Wu, Ying
    Feng, Yan
    JOURNAL OF MATERIALS SCIENCE, 2021, 56 (04) : 3472 - 3487
  • [10] Effect of ECAP temperature on microstructure and mechanical properties of Al–Zn–Mg–Cu alloy
    M.H.Shaeri
    M.Shaeri
    M.Ebrahimi
    M.T.Salehi
    S.H Seyyedein
    Progress in Natural Science:Materials International, 2016, 26 (02) : 182 - 191