Study of the Erosive-abrasive Wear Resistance of Fe-14%Cr-2.8%C High Chromium Cast Iron

被引:0
|
作者
Franco Junior, Adonias Ribeiro [1 ]
Caceres, Jaime Alberto Sanchez [1 ]
da Rocha, Diego Loubach [1 ]
机构
[1] Inst Fed Espirito Santo, Vitoria, ES, Brazil
关键词
high chromium cast iron; austenite destabilization; martensite/austenite ratio; impeller-tumbler test; SECONDARY CARBIDES; PRECIPITATION;
D O I
10.1590/1980-5373-MR-2023-0242
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High chromium cast irons (HCCIs) are widely applied in the mining industry as components of equipment for iron ore transportation, in which their surfaces are subjected to abrasive and erosive wear. The present work evaluated the erosion-abrasion behavior of a HCCI possessing different amounts of austenite and martensite, using a laboratory impeller-tumbler wear test apparatus and iron ore pellets as abrasive material. The results showed that the wear dominant mechanism on the worn surface of the as-cast material depends upon the material microstructure. For HCCI destabilized at 930 and 990 degrees C, the matrix has high martensite/austenite ratio and finely dispersed secondary carbides, offering high abrasion-erosion wear resistance. The absence of fractured eutectic carbides indicates that such matrix has hardness and load bearing capacity, enough for mitigating a significant plastic deformation during the impact pellets. For HCCI destabilized at 1050 degrees C, the matrix has a low martensite/austenite ratio and coalesced secondary carbides, leading to high wear rates during erosion-abrasion tests.
引用
收藏
页码:1 / 5
页数:7
相关论文
共 50 条
  • [1] The Abrasive Wear Resistance of Chromium Cast Iron
    Kopycinski, D.
    Piasny, S.
    Kawalec, M.
    Madizhanova, A.
    ARCHIVES OF FOUNDRY ENGINEERING, 2014, 14 (01) : 63 - 66
  • [2] Microstructural and Erosive Wear Characteristics of a High Chromium Cast Iron
    Fortini, Annalisa
    Suman, Alessio
    Vulpio, Alessandro
    Merlin, Mattia
    Pinelli, Michele
    COATINGS, 2021, 11 (05)
  • [3] Abrasive Wear Behavior and Mechanism of High Chromium Cast Iron
    Ting SUN
    Ren-bo SONG
    Xu WANG
    Peng DENG
    Chun-jing WU
    Journal of Iron and Steel Research(International), 2015, 22 (01) : 84 - 90
  • [4] Abrasive Wear Behavior and Mechanism of High Chromium Cast Iron
    Sun, Ting
    Song, Ren-bo
    Wang, Xu
    Deng, Peng
    Wu, Chun-jing
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2015, 22 (01) : 84 - 90
  • [5] Abrasive wear behavior and mechanism of high chromium cast iron
    Ting Sun
    Ren-bo Song
    Xu Wang
    Peng Deng
    Chun-jing Wu
    Journal of Iron and Steel Research International, 2015, 22 : 84 - 90
  • [6] Effect of TiBAl inoculation on abrasive wear resistance of high Cr white cast iron
    Teker, Tanju
    Yilmaz, S. Osman
    Kerkut, Erhan
    MATERIALS TESTING, 2019, 61 (07) : 690 - 694
  • [7] Effect of Cr:C ratio on open three-body wear resistance of squeeze cast high chromium cast iron
    Liu, Shaohua
    Li, Jinzhi
    Su, Xianglin
    Cui, Senlin
    Zhang, Haifeng
    Ren, Zhiheng
    TRIBOLOGY INTERNATIONAL, 2025, 202
  • [8] Effect of surface Cr/C infiltration on microstructure, mechanical properties and wear resistance of high chromium cast iron
    Chen, Peng
    Wu, Zhao-yang
    Yi, Yan-liang
    Huang, Jian-bin
    Shang, Tao
    Li, Wei
    CHINA FOUNDRY, 2022, 19 (03) : 218 - 224
  • [9] Effect of surface Cr/C infiltration on microstructure, mechanical properties and wear resistance of high chromium cast iron
    Peng Chen
    Zhao-yang Wu
    Yan-liang Yi
    Jian-bin Huang
    Tao Shang
    Wei Li
    China Foundry, 2022, 19 : 218 - 224
  • [10] Effect of surface Cr/C infiltration on microstructure, mechanical properties and wear resistance of high chromium cast iron
    Peng Chen
    Zhao-yang Wu
    Yan-liang Yi
    Jian-bin Huang
    Tao Shang
    Wei Li
    ChinaFoundry, 2022, 19 (03) : 218 - 224