Investigating the effect of compatibilizers on environmental stress cracking resistance in polypropylene/low density polyethylene blends

被引:0
|
作者
Benayache, Walid [1 ,3 ]
Benaniba, Mohamed Tahar [1 ]
Laradji, Mohamed [2 ]
Benachour, Djaafar [1 ]
机构
[1] Ferhat Abbas Univ Setif 1, Lab Multiphase Polymer Mat, Setif, Algeria
[2] Univ Memphis, Dept Phys & Mat Sci, Memphis, TN USA
[3] Ferhat Abbas Univ Setif 1, Lab Multiphase Polymer Mat, Setif 19000, Algeria
关键词
Blends; compatibilization; polyolefin; environmental stress crack resistance; IGEPAL CA 630; MECHANICAL-PROPERTIES; MORPHOLOGY; BEHAVIOR;
D O I
10.1080/10601325.2024.2332356
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The present study focuses on the effect of octylphenoxy poly(ethyleneoxy)ethanol (IGEPAL CA 630) on the environmental stress cracking resistance (ESCR) of blends of polypropylene (PP) and low-density polyethylene (LDPE) at different weight fractions without and with the addition of two compatibilizers, corresponding to styrene-ethylene-butylene-styrene (SEBS) copolymer and styrene-ethylene-butylene maleate (SEBS-g-MA). Compression molding was used after mixing the melt in a Brabender internal mixer to create the blends. ESCR of the blends was determined by exposing the blends to a solution of IGEPAL CA 630 the presence of stress. Mechanical (tensile) and thermal properties are extracted to evaluate the effect of adding the compatibilizers SEBS and SEBS-g-MA to the blend. In the environmental stress cracking (ESCR) tests, the time to failure increases with increasing PP content, despite PP's greater resistance to ESCR than LDPE. The addition of SEBS-g-MA to the blend significantly improves the flexibility and ESCR performance of PP/LDPE blends with specific weight fractions.
引用
收藏
页码:305 / 312
页数:8
相关论文
共 50 条
  • [1] Compatibilizers for low density polyethylene/polypropylene blends
    Andreopoulos, AG
    Tarantili, PA
    Anastassakis, P
    JOURNAL OF MACROMOLECULAR SCIENCE-PURE AND APPLIED CHEMISTRY, 1999, 36 (09): : 1113 - 1122
  • [2] THE EFFECT OF COMPATIBILIZERS ON THE MORPHOLOGY OF ISOTACTIC POLYPROPYLENE LINEAR LOW-DENSITY POLYETHYLENE BLENDS
    FLARIS, V
    WASIAK, A
    WENIG, W
    JOURNAL OF MATERIALS SCIENCE, 1993, 28 (06) : 1685 - 1688
  • [3] Environmental stress cracking resistance of blends of high-density polyethylene with other polyethylenes
    Schellenberg, J
    Fienhold, G
    POLYMER ENGINEERING AND SCIENCE, 1998, 38 (09): : 1413 - 1419
  • [4] Adhesion of olefin block copolymers to polypropylene and high density polyethylene and their effectiveness as compatibilizers in blends
    Lin, Yijian
    Marchand, Gary R.
    Hiltner, Anne
    Baer, Eric
    POLYMER, 2011, 52 (07) : 1635 - 1644
  • [5] EFFECTS OF COMPATIBILIZERS ON THE MECHANICAL PROPERTIES OF LOW DENSITY POLYETHYLENE/LIGNIN BLENDS
    Luo, Feng
    Ning, Nan-ying
    Chen, Long
    Su, Run
    Cao, Jing
    Zhang, Qin
    Fu, Qiang
    Zhao, Shu-gao
    CHINESE JOURNAL OF POLYMER SCIENCE, 2009, 27 (06) : 833 - 842
  • [6] EFFECTS OF COMPATIBILIZERS ON THE MECHANICAL PROPERTIES OF LOW DENSITY POLYETHYLENE/LIGNIN BLENDS
    张琴
    傅强
    Chinese Journal of Polymer Science, 2009, 27 (06) : 833 - 842
  • [8] Polymer Network Mobility and Environmental Stress Cracking Resistance of High Density Polyethylene
    Cheng, Joy J.
    Polak, Maria A.
    Penlidis, Alexander
    POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2009, 48 (12) : 1252 - 1261
  • [9] Compatibilizers based on polypropylene grafted with itaconic acid derivatives. Effect on polypropylene/polyethylene terephthalate blends
    Yazdani-Pedram, M
    Vega, H
    Retuert, J
    Quijada, R
    POLYMER ENGINEERING AND SCIENCE, 2003, 43 (04): : 960 - 964
  • [10] Influence of micromolecular structure on environmental stress cracking resistance of high density polyethylene
    Cheng, Joy J.
    Polak, Maria A.
    Penlidis, Alexander
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2011, 26 (04) : 582 - 593