Comprehensive microstructural and mechanical characterization of transient liquid phase bonded austenitic stainless steel by Ni-Cr-Si-B amorphous interlayer

被引:5
|
作者
Naalchian, M. [1 ]
Kasiri-Asgarani, M. [1 ]
Bakhsheshi-Rad, H. R. [1 ]
Manshaee, J. [1 ]
机构
[1] Islamic Azad Univ, Adv Mat Res Ctr, Dept Mat Engn, Najafabad Branch, Najafabad, Iran
关键词
Transient liquid phase bonded austenitic; stainless steel; Amorphous interlayer; Microstructural; Mechanical property; ISOTHERMAL SOLIDIFICATION COMPLETION; BONDING TEMPERATURE; JOINTS; SUPERALLOYS; PARAMETERS; PROPERTY; BORIDES; ALLOY; TIME;
D O I
10.1016/j.ijpvp.2023.105078
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, along with the joining of the gas turbine fuel nozzle part from austenitic stainless steel 316L alloy with BNi-2 interlayer by the transient liquid phase bonding process, microstructure test, shear strength and tensile strength tests have been placed. Bonding at a temperature of 1080 degrees C and a holding time of 45 min has led to the completion of isothermal solidification in the bonding zone. Microstructural and phase investigations showed that austenitic stainless steel 316L undergoes phase transformation after exposure to temperature conditions and the delta ferrite phase is formed as separate areas due to the diffusion of the solid state of ferrite-forming elements, and the grains of the base metal are 32 mu m have reached 43 mu m, which has caused a decrease in the shear strength of the base metal from 362 MPa to 347 MPa. Despite the completion of isothermal solidification in the joint centerline due to the boron diffusion of the solid state into the base metal and achieving the maximum shear strength of the joint (402 MPa), two generations of boride deposits have been formed. The first-generation borides based on nickel-iron-chromium-molybdenum are formed during heating up to the bonding temperature, and the second-generation boride deposits are based on iron-chromium-molybdenum, which were deposited in situ during the isothermal solidification stage. The microhardness test confirms the uniform distribution of hardness in each of the bonding zones, which feedback was determined in the tensile strength test. The tensile strength of the bonded sample was 485 MPa, which is approximately 82 % of stainless steel 316L. In both shear and tensile tests, the presence of small dimples indicates the ductile failure of the joint samples in base metal.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Diffusion brazing of Nicrofer 5520 (IN-617) superalloy using an amorphous Ni-Cr-Si-B interlayer: Microstructural characterization and mechanical properties
    Nasajpour, Ali
    Mirsalehi, Seyyed Ehsan
    Farzadi, Ali
    KOVOVE MATERIALY-METALLIC MATERIALS, 2022, 60 (02): : 89 - 107
  • [2] Microstructural and mechanical characterizations of steel tubes joined by transient liquid phase bonding using an amorphous Fe-B-Si interlayer
    Di Luozzo, Nicolas
    Doisneau, Beatrice
    Boudard, Michel
    Fontana, Marcelo
    Arcondo, Bibiana
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 : S18 - S22
  • [3] Characterization of transient-liquid-phase-bonded joints in a duplex stainless steel with a Ni-Cr-B insert alloy
    Yuan, Xinjian
    Kim, Myung Bok
    Kang, Chung Yun
    MATERIALS CHARACTERIZATION, 2009, 60 (11) : 1289 - 1297
  • [4] Microchemical and microstructural studies in a PTA weld overlay of Ni-Cr-Si-B alloy on AISI 304L stainless steel
    Sudha, C.
    Shankar, P.
    Rao, Rn. Subba
    Thirumurugesan, R.
    Vijayalakshmi, M.
    Raj, Baldev
    SURFACE & COATINGS TECHNOLOGY, 2008, 202 (10): : 2103 - 2112
  • [5] Interfacial morphology of duplex stainless steel joints brazed with Ni-Cr-Si-B filler metal
    Lee, HK
    Kang, CY
    Woo, CS
    Kim, SH
    Kim, DU
    DESIGNING, PROCESSING AND PROPERTIES OF ADVANCED ENGINEERING MATERIALS, PTS 1 AND 2, 2004, 449-4 : 889 - 892
  • [6] Transient liquid phase bonding of carbon steel tubes using a Cu interlayer: Characterization and comparison with amorphous Fe-B-Si interlayer bonds
    Di Luozzo, Nicolas
    Boudard, Michel
    Doisneau, Beatrice
    Fontana, Marcelo
    Arcondo, Bibiana
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 : S13 - S17
  • [7] Transient liquid-phase bonding of superalloy K465 using a Ni–Cr–Fe–B–Si amorphous interlayer alloy
    Ji-De Liu
    Bo Li
    Yuan Sun
    Tao Jin
    Xiao-Feng Sun
    Zhuang-Qi Hu
    Rare Metals, 2020, 39 : 408 - 412
  • [8] Transient liquid phase bonding of steel using an Fe–B interlayer: microstructural analysis
    N. Di Luozzo
    M. Fontana
    B. Arcondo
    Journal of Materials Science, 2008, 43 : 4938 - 4944
  • [9] Transient liquid-phase bonding of superalloy K465 using a Ni-Cr-Fe-B-Si amorphous interlayer alloy
    Ji-De Liu
    Bo Li
    Yuan Sun
    Tao Jin
    Xiao-Feng Sun
    Zhuang-Qi Hu
    RareMetals, 2020, 39 (04) : 408 - 412
  • [10] Transient liquid-phase bonding of superalloy K465 using a Ni-Cr-Fe-B-Si amorphous interlayer alloy
    Liu, Ji-De
    Li, Bo
    Sun, Yuan
    Jin, Tao
    Sun, Xiao-Feng
    Hu, Zhuang-Qi
    RARE METALS, 2020, 39 (04) : 408 - 412