Low cycle fatigue and creep-fatigue performance of 316SS formed by selective laser melting

被引:2
|
作者
Pan, Lingfeng [1 ,2 ]
Ding, Peishan [1 ,2 ]
Kong, Dezhou [1 ,2 ]
Liu, Lijun [1 ,2 ,3 ]
Zheng, Xiaotao [1 ,2 ,3 ]
机构
[1] Wuhan Inst Technol, Sch Mech & Elect Engn, Hubei Prov Key Lab Chem Equipment Intensificat & I, Wuhan, Peoples R China
[2] Wuhan Inst Technol, Hubei Prov Engn Technol Res Ctr Green Chem Equipme, Sch Mech & Elect Engn, Wuhan, Peoples R China
[3] Wuhan Inst Technol, Sch Mech & Elect Engn, Hubei Prov Key Lab Chem Equipment Intensificat & I, Wuhan 430205, Peoples R China
基金
中国国家自然科学基金;
关键词
SLM; LCF; ratcheting; creep; 316SS; SLM PROCESS PARAMETERS; MECHANICAL-PROPERTIES; STEEL; MICROSTRUCTURE; BEHAVIOR; HARDNESS;
D O I
10.1080/09603409.2023.2205761
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The fatigue and creep-fatigue properties of 316SS formed by selective laser melting (SLM) were investigated, considering the effects of different peak stresses, stress rates and peak-holding times on the ratcheting and creep-ratcheting behaviour of SLM 316 SS specimens at different sampling angles (0 degrees, 90 degrees) and high temperatures (550 degrees C, 650 degrees C, 750 degrees C). Results show that the 90 degrees specimens exhibited better fatigue life than that of the 0 degrees specimens. Moreover, the ratcheting evolution can be divided into three stages, but the first stage is very short and the main ratcheting behaviour takes place in the second and third stages. Interestingly, it was found that at stress rates above 10 MPa/s, the ratcheting evolution curves are highly overlapping. Furthermore, the creep-fatigue interaction promotes the evolution of material damage. Besides, creep increases the total strain of 316SS even with a short dwell time (0.5 min).
引用
收藏
页码:230 / 240
页数:11
相关论文
共 50 条
  • [1] Low cycle fatigue and creep-fatigue response of the 316Ti stainless steel
    Krovvidi, S. C. S. P. Kumar
    Goyal, Sunil
    Bhaduri, A. K.
    FRATTURA ED INTEGRITA STRUTTURALE, 2019, 13 (48): : 577 - 584
  • [2] Creep Fatigue Analysis of the 316SS Monolith in the MegaPower Heat Pipe Reactor
    Wang, Yong
    Liang, Lichuang
    Tian, Jun
    Su, Dongchuan
    Li, Hui
    Jiang, Naibin
    NUCLEAR TECHNOLOGY, 2024, 210 (11) : 2115 - 2132
  • [3] Creep-fatigue test of a SA 316SS structure and comparative damage evaluations based upon elastic and inelastic approaches
    Kim, Jong-Bum
    Lee, Hyeong-Yeon
    Park, Chang-Gyu
    Lee, Jae-Han
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2008, 85 (08) : 550 - 556
  • [4] LOW-CYCLE FATIGUE AND CREEP-FATIGUE BEHAVIOR OF A 316-L STAINLESS-STEEL
    SIMON, S
    IBABE, JMR
    FUENTES, M
    ZEITSCHRIFT FUR METALLKUNDE, 1993, 84 (10): : 708 - 715
  • [5] High temperature low cycle fatigue and creep-fatigue interaction behaviour of 316 and 316(N) weld metals and their weld joints
    Valsan, M
    Nagesha, A
    Rao, KBS
    Mannan, SL
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2002, 55 (05): : 341 - 348
  • [6] Characterization of low-cycle fatigue and creep-fatigue induced damage in a 316L stainless steel
    Simon, Sergio
    Rodriguez Ibabe, Jose M.
    Fuentes, Manuel
    Zeitschrift fuer Metallkunde/Materials Research and Advanced Techniques, 1994, 85 (04): : 273 - 281
  • [7] Low cycle fatigue and creep-fatigue interaction behaviour of 316L(N) stainless steel and its welds
    Valsan, M.
    Nagesha, A.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2010, 63 (2-3) : 209 - 215
  • [9] Creep and Creep-fatigue Behaviour of 316 Stainless Steel
    Holmstrom, Stefan
    Pohja, Rami
    Nurmela, Asta
    Moilanen, Pekka
    Auerkari, Pertti
    6TH INTERNATIONAL CONFERENCE ON CREEP, FATIGUE AND CREEP-FATIGUE INTERACTION, 2013, 55 : 160 - 164
  • [10] CHARACTERIZATION OF LOW-CYCLE FATIGUE AND CREEP-FATIGUE INDUCED DAMAGE IN A 316L STAINLESS-STEEL
    SIMON, S
    IBABE, JMR
    FUENTES, M
    ZEITSCHRIFT FUR METALLKUNDE, 1994, 85 (04): : 273 - 281