共 50 条
Accelerated Formation of Oxide Layers on Zircaloy-4 Utilizing Air Oxidation and Comparison with Water-Corroded Oxide Layers
被引:1
|作者:
Muthu, Shanmugam Mannan
[1
]
Lee, Hyeon-Bae
[1
]
Okonkwo, Bright O.
[2
]
Wang, Dong
[1
,3
]
Jang, Changheui
[1
]
Na, Taehyung
[4
]
机构:
[1] Korea Adv Inst Sci & Technol, Dept Nucl & Quantum Engn, 291 Daehak Ro, Daejeon 34141, South Korea
[2] Inst Corros Sci & Technol, Guangzhou 510530, Peoples R China
[3] Xi An Jiao Tong Univ, Sch Nucl Sci & Technol, State Key Lab Multiphase Flow Power Engn, Shaanxi Key Lab Adv Nucl Energy & Technol, Xian 710049, Peoples R China
[4] Korea Hydro & Nucl Power Co Ltd, Cent Res Inst, Daejeon 34101, South Korea
来源:
关键词:
Zircaloy-4;
spent fuel cladding;
oxide layer;
corrosion;
oxidation;
ADDED MODIFIED ZIRCALOY-4;
CORROSION BEHAVIOR;
PRESSURIZED-WATER;
ALLOYS;
D O I:
10.3390/ma16247589
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
For the dry storage of Canada Deuterium Uranium (CANDU) spent nuclear fuels, the integrity of Zircaloy-4 fuel cladding has to be verified. However, the formation of similar to 10 mu m-thick oxide layers in typical CANDU reactor operating conditions takes several years, which makes sample preparation a slow process. To overcome such limitations, in this study, an accelerated formation of an oxide layer on Zircaloy-4 cladding tube was developed with a combination of high-temperature water corrosion (HT-WC) and air oxidation (AO). First, Zircaloy-4 tubes were corroded in oxygenated (2 ppm dissolved oxygen) high-temperature water (360 degree celsius/19.5 MPa) for 500 h. Then, the tubes were air-oxidized at 500 degree celsius for 30 h. Finally, the tubes were corroded again in HT-WC for 500 h to produce similar to 10 mu m-thick oxide layers. The morphology and characteristics of the oxide layer in each step were analyzed using X-ray diffraction, scanning and transmission electron microscopy. The results showed that the oxide layer formed in the accelerated method was comparable to that formed in HT-WC in terms of morphology and oxide phases. Thus, the accelerated oxide formation method can be used to prepare an oxidized Zircaloy-4 cladding tube for CANDU fuel integrity analysis.