The microstructural evolution, mechanical and dielectric properties of BNW/SiO2 ceramics

被引:6
|
作者
Duan, Wenjiu [1 ]
Yang, Hualong [3 ]
Yang, Zhihua [3 ]
Li, Bo [1 ,2 ]
Jia, Dechang [3 ]
Zhou, Yu [3 ]
机构
[1] Tsinghua Univ, Tsinghua Shenzhen Int Grad Sch, Shenzhen 518055, Peoples R China
[2] Tsinghua Univ, Sch Mat Sci & Engn, State Key Lab New Ceram & Fine Proc, Beijing 100084, Peoples R China
[3] Harbin Inst Technol, Inst Adv Ceram, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
关键词
BN whisker; Microstructural evolution; Strengthening and toughening mechanisms; Dielectric properties; NITRIDE; BN; PERFORMANCE; SIZE;
D O I
10.1016/j.ceramint.2022.12.046
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The boron nitride reinforced fused silica (BN/SiO2) ceramics are excellent high-temperature wave-transparent candidates, but encumbered by the unsatisfactory reliability and economy until now. Herein, promising BN whisker reinforced SiO2 (BNW/SiO2) ceramics are fabricated via hot-pressing, aiming to provide fundamental insight into their microstructural evolution, mechanical and dielectric properties. The densification behaviour and microstructural evolution are characterized by step-testing the sintering temperature and the BNW content, determining that SiO2 matrix undergoes crystal nucleus breeding (<= 1300 degrees C), followed by nucleation and growth (>1300 degrees C), and BNW presents a uniform and stable structure (<= 1350 degrees C) and skin-core structure (1450 degrees C), respectively. The underlying strengthening and toughening mechanisms are elucidated through constructing a multilevel porosity dependence of mechanical behaviour associated with the BNW content. Compared with 5 wt. % BNW/SiO2 ceramic sintered at 1350 degrees C (S5-1350), the lightweight 20 wt. % BNW/SiO2 ceramic sintered at 1300 degrees C (S20-1300) exhibits 619.1% higher machinability parameter while maintaining the mechanical prop-erties. Moreover, the lightweight S20-1300 possesses a low dielectric constant (epsilon) of 3.77, loss tangent (tan delta) of 1.25 x 10-3 and coefficient of thermal expansion (CTE) of 1.34 x 10-6 K-1. The insights obtained from this study would help to advance the application of BN/SiO2 ceramics in high-temperature radome.
引用
收藏
页码:11968 / 11977
页数:10
相关论文
共 50 条
  • [1] Effect of SiO2 additive on the mechanical and dielectric properties of PZFNTU ceramics
    Huang, HT
    Hing, P
    FERROELECTRICS, 1999, 229 (1-4) : 291 - 296
  • [2] Preparation and dielectric properties of SiO2/silicate-1 ceramics
    Xiaobing Yang
    Huaping Xiong
    Xuetao Luo
    Journal of Porous Materials, 2017, 24 : 367 - 371
  • [3] Preparation and dielectric properties of SiO2/silicate-1 ceramics
    Yang, Xiaobing
    Xiong, Huaping
    Luo, Xuetao
    JOURNAL OF POROUS MATERIALS, 2017, 24 (02) : 367 - 371
  • [4] Dielectric properties of barium titanate ceramics modified by SiO2 and by BaO-SiO2
    Shen, Z. J.
    Chen, W. P.
    Qi, J. Q.
    Wang, Y.
    Chan, H. L. W.
    Chen, Y.
    Jiang, X. P.
    PHYSICA B-CONDENSED MATTER, 2009, 404 (16) : 2374 - 2376
  • [5] Improvement of Dielectric and Mechanical Properties of Epoxy/SiO2 Nanocomposites
    Al-Sawafi, Ameer B.
    Abdulzahra, Nura Anwer
    Odah, Jafer Fahdel
    12TH INTERNATIONAL CONFERENCE ON THE DEVELOPMENTS IN ESYSTEMS ENGINEERING (DESE 2019), 2019, : 77 - 82
  • [6] Effect of SiO2 content on the microstructure, mechanical and dielectric properties of Si3N4 ceramics
    Lee, Seung Jun
    Baek, Seungsu
    CERAMICS INTERNATIONAL, 2016, 42 (08) : 9921 - 9925
  • [7] Synthesis and Microwave Dielectric Properties of MgO–TiO2–SiO2 Ceramics
    O. V. Ovchar
    O. I. V'yunov
    D. A. Durilin
    Yu. D. Stupin
    A. G. Belous
    Inorganic Materials, 2004, 40 : 1116 - 1121
  • [8] Microstructural evolution and dielectric properties of SiO2-doped CaCU3Ti4O12 ceramics
    Kim, Kang-Min
    Kim, Sun-Jung
    Lee, Jong-Heun
    Kim, Doh-Yeon
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (13-15) : 3991 - 3995
  • [9] Influence of SiO2 addition on mechanical and lipophilic properties of silicon nitride ceramics
    Tokuda, Tarou
    Wang, Rongguang
    Kido, Mitsuo
    Okada, Shin
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2007, 71 (01) : 128 - 134
  • [10] Ceramics with adjustable dielectric properties based on the system SrO - TiO2 - SiO2
    Lisachuk, Georgy
    Kryvobok, Ruslan
    Pitak, Yaroslav
    Lapuzina, Olena
    Gusarova, Irina
    Lisachuk, Lidiya
    Grebenyuk, Andrey
    PRZEGLAD ELEKTROTECHNICZNY, 2018, 94 (01): : 163 - 166