Influence of the Anodizing Time on the Microstructure and Immersion Stability of Tartaric-Sulfuric Acid Anodized Aluminum Alloys

被引:13
|
作者
Raffin, Florian [1 ]
Echouard, Jacques [2 ]
Volovitch, Polina [1 ,3 ]
机构
[1] PSL Univ, Inst Rech Chim Paris IRCP, Chim ParisTech CNRS, 11 Rue Pierre & Marie Curie, F-75005 Paris, France
[2] Safran Landing Syst, 7 Rue Gen Valerie Andre, F-78140 Velizy Villacoublay, France
[3] PSL Univ, Ecole Polytech, Inst Photovolta Ile Defrance IPVF, UMR 9006,CNRS,IP Paris,Chim ParisTech, F-91120 Palaiseau, France
关键词
TSA anodizing; aluminum alloy; electrochemical impedance spectroscopy; corrosion protection; OXIDE-FILMS; BEHAVIOR; AA2024-T3; TEMPERATURE; OXIDATION;
D O I
10.3390/met13050993
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Tartaric-sulfuric acid anodizing (TSA) has been selected by the aerospace industry to replace Cr(VI)-based anodizing treatments of aluminum alloys. Modification of the bath composition can result in the necessity to revise the process conditions, including the time necessary to obtain the desired properties of the anodized layer. This study focuses on the microstructure and immersion stability of the pilot scale anodized AA2024 aluminum alloy, with anodizing times of 25 min and 45 min. The layer structure was characterized by scanning electron microscopy (SEM) and glow discharge optical emission spectrometry (GD-OES). The electrochemical impedance spectroscopy (EIS) was used to evaluate the corrosion resistance and immersion stability of the samples in 0.01 M NaCl solution. The density of pores formed in the 45 min anodized samples was higher which correlated with higher impedance modulus at equivalent immersion time and higher thickness of the oxide layer. Contact angle measurements demonstrated better wettability of the 45 min anodized sample. The results suggest that 45 min anodizing offers higher corrosion resistance and better initial adhesion with subsequent post-treatment such as sealing or painting.
引用
收藏
页数:13
相关论文
共 31 条
  • [1] Addition of molybdate ions to the anodizing bath to improve the corrosion resistance of clad 2024-T3 alloy anodized in tartaric-sulfuric acid
    Almeida, Thassia Felix de
    Ramirez, Oscar Mauricio Prada
    Lanzutti, Alex
    Rodrigues, Cleber Lima
    Brabetz, Manfred
    Kremmer, Thomas M.
    Hammer, Peter
    Melo, Hercilio Gomes de
    SURFACE & COATINGS TECHNOLOGY, 2024, 482
  • [2] Corrosion protection of clad 2024 aluminum alloy anodized in tartaric-sulfuric acid bath and protected with hybrid sol-gel coating
    Capelossi, V. R.
    Poelman, M.
    Recloux, I.
    Hernandez, R. P. B.
    de Melo, H. G.
    Olivier, M. G.
    ELECTROCHIMICA ACTA, 2014, 124 : 69 - 79
  • [3] Influence of Fluorozirconic Acid on Sulfuric Acid Anodizing of Aluminum
    Elaish, R.
    Curioni, M.
    Gowers, K.
    Kasuga, A.
    Habazaki, H.
    Hashimoto, T.
    Skeldon, P.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (13) : C831 - C839
  • [4] Anodic Film Formation on AA 2099-T8 Aluminum Alloy in Tartaric-Sulfuric Acid
    Ma, Y.
    Zhou, X.
    Thompson, G. E.
    Curioni, M.
    Hashimoto, T.
    Skeldon, P.
    Thomson, P.
    Fowles, M.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2011, 158 (02) : C17 - C22
  • [5] The influence of "Light green" additive on the anodizing of aluminum in sulfuric acid
    Dimogerontakis, T
    Tsangaraki-Kaplanoglou, I
    PLATING AND SURFACE FINISHING, 2003, 90 (05): : 80 - 82
  • [6] ANODIZING OF ALUMINUM-ALLOYS IN BORIC AND SULFURIC-ACID-SOLUTIONS
    JUANTO, S
    GERVASI, CA
    REAL, SG
    VILCHE, JR
    ANALES DE LA ASOCIACION QUIMICA ARGENTINA, 1987, 75 (01): : 55 - 62
  • [7] Effect of Cerium Addition to a Hydrothermal Treatment on the Corrosion Protection of the Tartaric-Sulfuric Acid Anodized AA2524-T3
    Terada, Maysa
    Queiroz, Fernanda M.
    Costenaro, Helen
    Ayusso, Victor H.
    Olivier, Marjorie
    Costa, Isolda
    de Melo, Hercilio G.
    CORROSION, 2019, 75 (09) : 1110 - 1117
  • [8] Ce post-treatment for increased corrosion resistance of AA2024-T3 anodized in tartaric-sulfuric acid
    Ramirez, Oscar Mauricio Prada
    Tunes, Matheus Araujo
    Mennucci, Marina Martins
    Starykevich, Maksim
    Neves, Cristina
    Ferreira, Mario G. S.
    Pogatscher, Stefan
    De Melo, Hercilio Gomes
    CORROSION SCIENCE, 2022, 204
  • [9] Morphological and semiconductive properties of the anodic oxide layers made on Fe3Al alloy by anodizing in tartaric-sulfuric acid mixture
    del Olmo, Ruben
    Lazinska, Magdalena
    Czerwinski, Mateusz
    Durejko, Tomasz
    Michalska-Domanska, Marta
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [10] Surface and Electrochemical Characteristics of Novel Chromate-Free Mn-V Oxyanion Sealed Tartaric-Sulfuric Acid Anodized Coating
    Yoganandan, G.
    Balaraju, J. N.
    Manikandanath, N. T.
    Ezhilselvi, V.
    Srivastava, Meenu
    Nagacharan, K. V.
    Anilchandra, A. R.
    Manjunatha, C. M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (11) : 6175 - 6188