摘要
Utilizing oxo-degradable additives is an alternate, efficient method of managing plastic trash. To prepare the polymer chain for microorganisms to break down the fragments over time, oxo-degradation of plastics involves breaking the chain into small pieces. In this study, a film with a thickness of 35 mu m is created by mixing a mixture of linear low-density polyethylene (LLDPE) and d2w grade master batch (pro-oxidant). This thickness falls within the range of specifications for linear low-density polyethylene (LLDPE) films manufactured in petrochemical businesses. Additionally, is the study investigates how the mechanical characteristics of linear low-density polyethylene (LLDPE) are affected by the addition of a d2w pro-oxidant additive at five different weight percentages (0, 0.5, 1, 2, and 3% w/w). After thermal processing for films in an oven for one to seven days, the progress of LLDPE film is monitored by FTIR analysis to check for the presence of the carbonyl group by assessing the mechanical properties of the film. Tensile strength at break, tensile strength at yield, elongation at break, and elongation at yield are the mechanical qualities that are measured. Both the machine direction (MD) and the transverse direction (TD) are used to measure all properties. Following seven days of exposure to the oven at 70 degrees C, the mechanical properties of the film deteriorated. Both in the machine and transverse directions (MD and TD), the tensile strength at break dropped by 46.62% and 31.8%, respectively. Both in the machine and transverse directions (MD and TD), the tensile strength at yield dropped by 22% and 36.36%, respectively. Both machine and transverse elongation at break (MD and TD) were reduced by 21% and 38.36%, respectively. Following the addition of pro-oxidant and after thermo-oxidative treatment in an oven at 70 degrees C for 7 days, the results of the FTIR measurement for LLDPE did not significantly alter.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Degradation of polyethylene film samples containing oxo-degradable additives
    Yashchuk, O.
    Portillo, F. S.
    Hermida, E. B.
    [J]. 11TH INTERNATIONAL CONGRESS ON METALLURGY & MATERIALS SAM/CONAMET 2011, 2012, 1 : 439 - 445
  • [2] Polyethylene-Based Oxo-Degradable Nanocomposite Film
    A. A. Atakhanov
    I. Kh. Turdikulov
    N. Sh. Ashurov
    [J]. Russian Journal of Applied Chemistry, 2022, 95 : 1161 - 1168
  • [3] Polyethylene-Based Oxo-Degradable Nanocomposite Film
    Atakhanov, A. A.
    Turdikulov, I. Kh.
    Ashurov, N. Sh.
    [J]. RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2022, 95 (08) : 1161 - 1168
  • [4] Evaluation of the rate of abiotic and biotic degradation of oxo-degradable polyethylene
    Portillo, Florencia
    Yashchuk, Oxana
    Hermida, Elida
    [J]. POLYMER TESTING, 2016, 53 : 58 - 69
  • [5] Oxo-degradable plastics: degradation, environmental impact and recycling
    Thomas, Noreen L.
    Clarke, Jane
    McLauchlin, Andrew R.
    Patrick, Stuart G.
    [J]. PROCEEDINGS OF THE INSTITUTION OF CIVIL ENGINEERS-WASTE AND RESOURCE MANAGEMENT, 2012, 165 (03) : 133 - 140
  • [6] Adverse effects of oxo-degradable plastic leachates in freshwater environment
    Simona Schiavo
    Maria Oliviero
    Salvatore Chiavarini
    Sonia Manzo
    [J]. Environmental Science and Pollution Research, 2020, 27 : 8586 - 8595
  • [7] Thermal degradation kinetics of oxo-degradable PP/PLA blends
    Mandal, Dev K.
    Bhunia, Haripada
    Bajpai, Pramod K.
    [J]. JOURNAL OF POLYMER ENGINEERING, 2019, 39 (01) : 58 - 67
  • [8] Biodegradation of oxidized high-density polyethylene and oxo-degradable plastic using microalgae Dunaliella salina
    Hadiyanto, Hadiyanto
    Khoironi, Adian
    Dianratri, Inggar
    Huda, Khoirul
    Suherman, Suherman
    Muhammad, Fuad
    [J]. ENVIRONMENTAL POLLUTANTS AND BIOAVAILABILITY, 2022, 34 (01) : 469 - 481
  • [9] Adverse effects of oxo-degradable plastic leachates in freshwater environment
    Schiavo, Simona
    Oliviero, Maria
    Chiavarini, Salvatore
    Manzo, Sonia
    [J]. ENVIRONMENTAL SCIENCE AND POLLUTION RESEARCH, 2020, 27 (08) : 8586 - 8595
  • [10] INFLUENCE OF PROOXIDANT NATURE ON EVOLUTION OF FORMALDEHYDE FROM OXO-DEGRADABLE POLYETHYLENE
    Korchagin, Vladimir, I
    Surkova, Alena M.
    Studenikina, Lubov N.
    Protasov, Artem, V
    [J]. IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII KHIMIYA I KHIMICHESKAYA TEKHNOLOGIYA, 2019, 62 (02): : 101 - 107