Quality of the Ceramic and Ni-Cr Alloy Joint after Al2O3 Abrasive Blasting

被引:1
|
作者
Klimek, Leszek [1 ]
Wolowiec-Korecka, Emilia [1 ]
Czepulkowska-Pawlak, Weronika [1 ]
Kula, Zofia [2 ]
机构
[1] Lodz Univ Technol, Fac Mech Engn, Inst Mat Sci & Engn, B Stefanowskiego 1-15, PL-90537 Lodz, Poland
[2] Med Univ Lodz, Dept Dent Technol, Pomorska 251, PL-92213 Lodz, Poland
关键词
abrasive blasting; metal-ceramic bond strength; shear strength; Ni-Cr alloy; thermocycles; AIRBORNE-PARTICLE ABRASION; FLEXURAL STRENGTH; COBALT-CHROMIUM; BOND STRENGTH; TITANIUM; METAL; PORCELAIN; GOLD;
D O I
10.3390/ma16103800
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The purpose of this in vitro study was to determine the effect of airborne-particle abrasion process parameters on the strength of the Ni-Cr alloy-ceramic bond. One hundred and forty-four Ni-Cr disks were airborne-particle abraded with 50, 110 and 250 mu m Al2O3 at a pressure of 400 and 600 kPa. After treatment, the specimens were bonded to dental ceramics by firing. The strength of the metal-ceramic bond was determined using the shear strength test. The results were analyzed with three-way analysis of variance (ANOVA) and the Tukey honest significant difference (HSD) test ( alpha = 0.05). The examination also considered the thermal loads (5000 cycles, 5-55 degrees C) to which the metal-ceramic joint is subjected during exploitation. There is a close correlation between the strength of the Ni-Cr alloy-dental ceramic joint and the alloy roughness parameters after abrasive blasting: Rpk (reduced peak height), Rsm (the mean spacing of irregularities), Rsk (skewness of the profile) and RPc (peak density). The highest strength of the Ni-Cr alloy surface bonding with dental ceramics under operating conditions is provided by abrasive blasting under 600 kPa pressure with 110 mu m Al2O3 particles (p < 0.05). Both the abrasive blasting pressure and the particle size of the Al2O3 abrasive significantly affect the joint's strength (p < 0.05). The most optimal blasting parameters are 600 kPa pressure with 110 mu m Al2O3 particles (p < 0.05). They allow the highest bond strength between the Ni-Cr alloy and dental ceramics to be achieved.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Effect of SiC Abrasive Blasting Parameters on the Quality of the Ceramic and Ni-Cr Dental Alloy Joint
    Wolowiec-Korecka, Emilia
    Czepulkowska-Pawlak, Weronika
    Kula, Zofia
    Klimek, Leszek
    MATERIALS, 2022, 15 (03)
  • [2] The Condition of Ni-Cr Alloy Surface After Abrasive Blasting with Various Parameters
    Czepulkowska, Weronika
    Wolowiec-Korecka, Emilia
    Klimek, Leszek
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (03) : 1439 - 1444
  • [3] The Condition of Ni-Cr Alloy Surface After Abrasive Blasting with Various Parameters
    Weronika Czepułkowska
    Emilia Wołowiec-Korecka
    Leszek Klimek
    Journal of Materials Engineering and Performance, 2020, 29 : 1439 - 1444
  • [4] The Surface Condition of Ni-Cr after SiC Abrasive Blasting for Applications in Ceramic Restorations
    Czepulkowska-Pawlak, Weronika
    Wolowiec-Korecka, Emilia
    Klimek, Leszek
    MATERIALS, 2020, 13 (24) : 1 - 12
  • [5] Effect of Ni-Cr Alloy Surface Abrasive Blasting on Its Wettability by Liquid Ceramics
    Czepulkowska-Pawlak, Weronika
    Klimek, Leszek
    Makowka, Marcin
    Wolowiec-Korecka, Emilia
    MATERIALS, 2021, 14 (08)
  • [6] Regeneration of Ni and Ni-Cr/Al2O3 catalysts for methane reforming reactions
    Nichio, NN
    Quincoces, CE
    Moral, P
    González, MG
    CATALYST DEACTIVATION 2001, PROCEEDINGS, 2001, 139 : 263 - 269
  • [7] Diffusion bonding of Al alloy to Al2O3 ceramic
    Feng, JC
    Wang, DY
    Li, ZR
    Liu, HJ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 : 1 - 4
  • [8] Diffusion bonding of Al alloy to Al2O3 ceramic
    Feng, Ji-Cai
    Wang, Da-Yong
    Li, Zhuo-Ran
    Liu, Hui-Jie
    Transactions of Nonferrous Metals Society of China (English Edition), 2003, 13 (SPEC. ISS.): : 1 - 4
  • [9] EFFECT OF CR2O3 VOLATILIZATION ON OXIDATION KINETICS OF A NI-CR ALLOY
    ECER, GM
    MEIER, GH
    SCRIPTA METALLURGICA, 1973, 7 (11): : 1189 - 1194
  • [10] Laser cladding of Ni-Cr/Al2O3 composite coatings on AISI 304 stainless steel
    Feng, J
    Ferreira, MGS
    Vilar, R
    SURFACE & COATINGS TECHNOLOGY, 1997, 88 (1-3): : 212 - 218