Study on the interface damage of CRTS II track slab under high- and low-temperature cycles based on acoustic emission

被引:4
|
作者
Qin, Lei [1 ,2 ,5 ]
Wang, Haibo [1 ]
Zhao, Chong [1 ]
Chu, Xuanxuan [6 ]
Shi, Feifan [1 ]
Guo, Chengchao [1 ,2 ,3 ,4 ,5 ]
Wang, Fuming [1 ,2 ,3 ,4 ,5 ]
机构
[1] Sun Yat Sen Univ, Sch Civil Engn, Guangzhou 510275, Peoples R China
[2] Southern Marine Sci & Engn Guangdong Lab Zhuhai, Zhuhai, Peoples R China
[3] Guangdong Key Lab Ocean Civil Engn, Guangzhou, Peoples R China
[4] Guangdong Res Ctr Underground Space Exploitat Tech, Guangzhou, Peoples R China
[5] Southern Inst Infrastructure Testing & Rehabil Tec, Huizhou, Peoples R China
[6] Univ Nottingham, Nottingham Transportat Engn Ctr, Nottingham NG7 2RD, England
关键词
CRTS II slab track; Composite specimen; High-low temperature cycle; Interface bond strength; Acoustic emission; CRUMB RUBBER CONCRETE; MECHANICAL-PROPERTIES; BEHAVIOR; STRESS; CEMENT; STABILITY; EVOLUTION; STRENGTH; FAILURE; BEAM;
D O I
10.1016/j.conbuildmat.2023.132742
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
China Railway Track System (CRTS) II slab tracks have been widely used in high-speed railway construction. Interface debonding between the track slab and cement-emulsified asphalt (CA) mortar is one of the typical diseases of the CRTS II slab tracks. Properly evaluating the interfacial strength of the track slab and CA mortar under high-and low-temperature cycles is crucial for optimizing the repair in engineering practices. In this study, the track slab and CA mortar (TSCAM) composite specimens were prepared for high-low temperature cycle (HLTC) tests. Then, the shear and tensile tests were carried out to study the interlayer bonding properties of TSCAM under different HLTCs. In addition, the acoustic emission (AE) technique was employed to monitor the signals generated in the specimen during the tests. Furthermore, the AE parameters were analyzed, including ringing counts, energy, b-value and amplitude-frequency. The results show that the number of HLTCs signifi-cantly contributed to the deterioration of the interface bond strength between the track slab and the CA mortar. The interface normal bond strength showed a higher decrease than the tangential bond strength with the increase of HLTCs. In addition, the relationships of the shear and tensile bond strength of the TSCAM composite specimen with HLTC were deduced. The tangential and normal bond strength degradation properties of the composite were well fitted by the function of quadratic polynomial and power exponents, respectively. The AE activities of the composite specimens in the shear and tensile tests were gradually reduced with increased HLTC. The AE signals were the strongest when the specimen failed along the interface. Furthermore, the intensity of AE events during the shear test was higher than that during the tensile test under the same HLTC. The overall b-values of the shear and tensile specimens without HLTC were the largest and did not change significantly with the increase of HLTC. The amplitude range of the peak frequency gradually decreased as the HLTC increased. The amplitude and peak frequency of the tensile test was smaller than that of the shear test under the same HLTC. This indicates that the AE technique can monitor the interface damage evolution pattern of the TSCAM composite specimen throughout the tests.
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Study on the interface damage of CRTS II slab track under temperature load
    Li, Yang
    Chen, Jinjie
    Wang, Jianxi
    Shi, Xianfeng
    Chen, Long
    STRUCTURES, 2020, 26 : 224 - 236
  • [2] Interface damage and arching mechanism of CRTS II slab track under temperature load
    Cui, Xuhao
    Du, Bowen
    Xiao, Hong
    Zhou, Rui
    Guo, Gaoran
    Liu, Hanlin
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 291
  • [3] Structural damage analysis of CRTS II slab track with various interface models under temperature combinations
    Zhou, Rui
    Zhu, Xuan
    Huang, Jiaqi
    Zhou, Haijun
    Liu, Hanlin
    Ma, Cong
    Zhang, Lihai
    ENGINEERING FAILURE ANALYSIS, 2022, 134
  • [4] Study on the interface damage of CRTS II slab track under temperature load (vol 26, pg 224, 2020)
    Li, Yang
    Chen, Jinjie
    Wang, Jianxi
    Shi, Xianfeng
    Chen, Long
    STRUCTURES, 2020, 28 : 2174 - 2174
  • [5] Experimental study on interface performance of CRTS II slab ballastless track under temperature loading
    Yao, Guowen
    Song, Anxiang
    Zhang, Gaofeng
    Liu, Wenpeng
    Qin, Tao
    Yu, Xuanrui
    Ran, Chongyang
    Tang, Yang
    STRUCTURES, 2024, 62
  • [6] Study on the mechanical performance and interface damage of CRTS II slab track with debonding repairment
    Xu, Yude
    Yan, Daobin
    Zhu, Wenjun
    Zhou, Yu
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 257
  • [7] Accumulative Damage of the Interface between CRTS II Track Slab and CA Mortar Layer under Cyclic Temperature Loads
    Zhao, Chunfa
    Feng, Yang
    Liu, Jianchao
    RAILWAY DEVELOPMENT, OPERATIONS, AND MAINTENANCE: PROCEEDINGS OF THE FIRST INTERNATIONAL CONFERENCE ON RAIL TRANSPORTATION 2017 (ICRT 2017), 2018, : 1109 - 1116
  • [8] Study on the causes of interface damage of CRTS II slab ballastless track CA mortar based on grouting operation
    Xie, Kaize
    Dai, Weiwu
    Wang, Qi
    Zhao, Zhenhang
    Zhao, Weigang
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 438
  • [9] High- and low-temperature fracture behavior of pervious asphalt mixtures under different freeze–thaw cycles based on acoustic emission technique
    Tianmin Wang
    Yu Chen
    Changqi Zhu
    Haifeng Liu
    Chenghao Ma
    Xing Wang
    Ru Qu
    Arabian Journal of Geosciences, 2022, 15 (19)
  • [10] Experimental Study and Numerical Analysis of Structural Performance of CRTS II Slab Track under Extreme High Temperature
    Song, Anxiang
    Yao, Guowen
    Yu, Xuanrui
    Wang, Yuerui
    Wu, Yifei
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2022, 2022