Low-Temperature Diffusion of Au and Ag Nanolayers for Cu Bonding

被引:1
|
作者
Lee, Sangmin [1 ]
Park, Sangwoo [1 ]
Kim, Sarah Eunkyung [1 ]
机构
[1] Seoul Natl Univ Sci & Technol, Dept Semicond Engn, Seoul 01811, South Korea
来源
APPLIED SCIENCES-BASEL | 2024年 / 14卷 / 01期
基金
新加坡国家研究基金会;
关键词
Cu bonding; 3D packaging; Au nanolayer; Ag nanolayer; hybrid bonding; PASSIVATION; INTERFACE;
D O I
10.3390/app14010147
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
With the recent rapid development of IT technology, the demand for multifunctional semiconductor devices capable of high performance has increased rapidly, and the miniaturization of such devices has also faced limitations. To overcome these limitations, various studies have investigated three-dimensional packaging methods of stacking devices, and among them, hybrid bonding is being actively conducted during the bonding process. studies of hybrid bonding during the bonding process are active. In this study, Cu bonding using a nano passivation layer was carried out for Cu/SiO2 hybrid bonding applications, with Au and Ag deposited on Cu at the nano level and used as a protective layer to prevent Cu oxidation and to achieve low-temperature Cu bonding. Au was deposited at about 12 nm, and Ag was deposited at about 15 nm, with Cu bonding carried out at 180 degrees C for 30 min, after which an annealing process was conducted at 200 degrees C for one hour. After bonding, the specimen was diced into a 1 cm x 1 cm chip, and the bonding interface was analyzed using SEM and TEM. Additionally, the 1 cm x 1 cm chip was diced into 2 mm x 2 mm specimens to measure the shear strength of the bonded chip, and the average shear strength of Au and Ag was found to be 5.4 and 6.6 MPa, respectively. The degree of diffusion between Au-Cu and Ag-Cu was then investigated; the diffusion activation energy when Au diffuses to Cu was 6369.52 J/mol, and the diffusion activation energy when Ag diffuses to Cu was 17,933.21 J/mol.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Effect of Evaporated and Sputtered Au Nanolayers on Cu Surface for Low-Temperature Cu-to-Cu Bonding
    Lee, Sangmin
    Park, Sangwoo
    Choi, Junyoung
    Kim, Sarah Eunkyung
    2024 International Conference on Electronics Packaging, ICEP 2024, 2024, : 299 - 300
  • [2] The Effect of an Ag Nanofilm on Low-Temperature Cu/Ag-Ag/Cu Chip Bonding in Air
    Kim, Yoonho
    Park, Seungmin
    Kim, Sarah Eunkyung
    APPLIED SCIENCES-BASEL, 2021, 11 (20):
  • [3] Low-Temperature Au-Au Bonding Using Nanoporous Au-Ag Sheets
    Mimatsu, Hayata
    Mizuno, Jun
    Kasahara, Takashi
    Saito, Mikiko
    Nishikawa, Hiroshi
    Shoji, Shuichi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2013, 52 (05)
  • [4] A Low-Temperature Bonding Process Using Mixed Cu–Ag Nanoparticles
    Y. Morisada
    T. Nagaoka
    M. Fukusumi
    Y. Kashiwagi
    M. Yamamoto
    M. Nakamoto
    Journal of Electronic Materials, 2010, 39 : 1283 - 1288
  • [5] Low-Temperature Diffusion Behavior of Ti in Cu/Ti-Ti/Cu Bonding
    Park, Seungmin
    Kim, Yoonho
    Kim, Sarah Eunkyung
    JOURNAL OF ELECTRONIC MATERIALS, 2022, 51 (05) : 2617 - 2623
  • [6] Low-Temperature Diffusion Behavior of Ti in Cu/Ti-Ti/Cu Bonding
    Seungmin Park
    Yoonho Kim
    Sarah Eunkyung Kim
    Journal of Electronic Materials, 2022, 51 : 2617 - 2623
  • [7] A Low-Temperature Bonding Process Using Mixed Cu-Ag Nanoparticles
    Morisada, Y.
    Nagaoka, T.
    Fukusumi, M.
    Kashiwagi, Y.
    Yamamoto, M.
    Nakamoto, M.
    JOURNAL OF ELECTRONIC MATERIALS, 2010, 39 (08) : 1283 - 1288
  • [8] AUGER-SPECTROSCOPY MEASUREMENT OF LOW-TEMPERATURE AG DIFFUSION IN AU-AG COUPLES
    ABRAMOFF, M
    DOBISZ, L
    LAGALLY, MG
    CLEMETSON, D
    HORNBOSTEL, L
    KUCKUK, J
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (08) : C348 - C348
  • [9] Low-temperature Au/Si wafer bonding
    Jing, E.
    Xiong, B.
    Wang, Y.
    ELECTRONICS LETTERS, 2010, 46 (16) : 1143 - U72
  • [10] LOW-TEMPERATURE GETTERING OF CU, AG, AND AU ACROSS A WAFER OF SI BY AL
    THOMPSON, RD
    TU, KN
    APPLIED PHYSICS LETTERS, 1982, 41 (05) : 440 - 442