Evaluation and Comparison of Mechanical Properties of Lithium Disilicate-Based CAD/CAM Blocks

被引:0
|
作者
Zulkiffli, Sofya [1 ]
Take, Yeoh Oon [1 ]
Yahya, Noor Azlin [1 ]
Kutty, Muralithran Govindan [1 ]
机构
[1] Univ Malaya, Fac Dent, Dept Restorat Dent, Kuala Lumpur 50603, Malaysia
来源
SAINS MALAYSIANA | 2024年 / 53卷 / 01期
关键词
CAD/CAM; flexural strength; lithium disilicate; microhardness; microstructure; FLEXURAL RESISTANCE; FRACTURE-TOUGHNESS; GLASS-CERAMICS; HEAT-TREATMENT; MICROSTRUCTURE; CRYSTALLIZATION; STRENGTH; EVOLUTION; BEHAVIOR;
D O I
10.17576/jsm-2024-5301-17
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Lithium disilicate are commonly used in dental restoration due to its aesthetic and mechanical performance. However, the patent expiration of the IPS emax system has led to the emergence of other variations of the system. Data and studies concerning mechanical properties of these recent lithium disilicate-based CAD/CAM are scarce and it warrants for an investigation to provide scientific evidence to support its routine use. The aim of this study was to investigate and compare the mechanical properties of lithium disilicate-based CAD/CAM blocks from four different brands. Four CAD/CAM lithium disilicate brands were investigated; IPS emax, Mazic Claro, Cameo, and Tessera. Specimens (n=10) were prepared accordingly; for flexural strength (16 x 4 x 1.2 mm) and microhardness test (15 x 13 x 2 mm). One specimen from each brand was analysed for the microstructure, elemental composition and distribution before and after heat treatment using scanning electron microscope and energy dispersive x-ray spectroscopy. The three-point flexural strength test (n=10) and microhardness test (n=10) was performed. Data were analysed using one-way ANOVA and Dunnett's T3 test. The results showed that the highest mean flexural strength was from Group 4 Tessera (540.52 +/- 143.33 MPa). For microhardness, the highest mean was from Group 1 Mazic Claro (667.70 +/- 9.41 HV). Within the four groups, statistically significant difference is noted for flexural strength and microhardness. As a conclusion, Tessera demonstrated significantly higher flexural strength than IPS emax and Cameo. Mazic and Tessera demonstrated significantly higher microhardness than IPS emax and Cameo. All materials tested were above the threshold of 300 MPa.
引用
收藏
页码:217 / 229
页数:13
相关论文
共 50 条
  • [1] Comparison of dimensional accuracy of lithium disilicate CAD/CAM ceramics
    Yamamoto, K.
    Murata, Y.
    Nagaoka, K.
    Akiyama, S.
    Hokii, Y.
    Fusejima, F.
    JOURNAL OF OSSEOINTEGRATION, 2022, 14 (04) : 205 - 208
  • [2] Comparative evaluation of the mechanical properties of CAD/CAM dental blocks
    Ruizhi Yin
    Yu-Kyoung Kim
    Yong-Seok Jang
    Jung-Jin Lee
    Min-Ho Lee
    Tae-Sung Bae
    Odontology, 2019, 107 : 360 - 367
  • [3] Comparative evaluation of the mechanical properties of CAD/CAM dental blocks
    Yin, Ruizhi
    Kim, Yu-Kyoung
    Jang, Yong-Seok
    Lee, Jung-Jin
    Lee, Min-Ho
    Bae, Tae-Sung
    ODONTOLOGY, 2019, 107 (03) : 360 - 367
  • [4] Physicochemical surface characterizations of four dental CAD/CAM lithium disilicate-based glass ceramics on HF etching: An XPS study
    Franca, Rodrigo
    Bebsh, Muna
    Haimeur, Asmaa
    Fernandes, Ana Carla
    Sacher, Edward
    CERAMICS INTERNATIONAL, 2020, 46 (02) : 1411 - 1418
  • [5] Effects of heat treatment temperature on microstructure and mechanical properties of lithium disilicate-based glass-ceramics
    Kamnoy, Manlika
    Pengpat, Kamonpan
    Intatha, Uraiwan
    Eitssayeam, Sukum
    CERAMICS INTERNATIONAL, 2018, 44 : S121 - S124
  • [6] CAD/CAM-based Implant Abutments Made of Lithium Disilicate
    Kurbad, A.
    Kurbad, S.
    INTERNATIONAL JOURNAL OF COMPUTERIZED DENTISTRY, 2013, 16 (02) : 125 - 141
  • [7] Mechanical properties of composite resin blocks for CAD/CAM
    Lauvanutanon, Sasipin
    Takahashi, Hidekazu
    Shiozawa, Maho
    Iwasaki, Naohiko
    Asakawal, Yuya
    Oki, Meiko
    Finger, Werner J.
    Arksornnukit, Mansuang
    DENTAL MATERIALS JOURNAL, 2014, 33 (05) : 705 - 710
  • [8] Properties of New Partially Crystallized Lithium Disilicate CAD-CAM Materials
    Wells, J. M.
    Johnson, J. W.
    Lien, W.
    Raimondi, C.
    Caballero, M.
    Gibbons, T. F.
    Vandewalle, K. S.
    OPERATIVE DENTISTRY, 2025, 50 (01) : 93 - 100
  • [9] Shade match comparison of CAD-CAM single crowns to a lithium disilicate crown
    Li, Rui
    Lin, Yu-Chun
    Sadid-Zadeh, Ramtin
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2024, 33 (03): : 246 - 251
  • [10] Comparative Evaluation of Mechanical Properties and Wear Ability of Five CAD/CAM Dental Blocks
    Yin, Ruizhi
    Jang, Yong-Seok
    Lee, Min-Ho
    Bae, Tae-Sung
    MATERIALS, 2019, 12 (14):