Phase Transformations and Properties Evolution of Alumina-Based Refractory Castables Containing ZnO and SiO2

被引:0
|
作者
Fini, D. S. [1 ]
de Mauro, C. L. C. [1 ]
Bezerra, B. P. [1 ,2 ]
Luz, A. P. [1 ,2 ]
机构
[1] Univ Fed Sao Carlos, Dept Engn Mat, Rod Washington Luiz,km 235, BR-13565905 Sao Carlos, SP, Brazil
[2] Univ Fed Sao Carlos, Programa Posgrad Ciencia & Engn Mat, Sao Carlos, SP, Brazil
关键词
Alumina; refractory castable; corrosion; AL2O3-MGO;
D O I
10.1590/1980-5373-MR-2022-0417
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Although most of the studies presented in the literature are focused on MgAl2O4 formation and its role on alumina-based refractories performance, ZnO has been reported as a promising spinel inducer. Aiming to investigate the influence of ZnAl2O4 (ZA) and MgAl2O4 (MA) generation on the properties of alumina-based castables, three vibratable compositions containing calcium aluminate cement or hydratable alumina as binders and 1 wt% of silica fume, were evaluated in this work. Flexural strength, apparent porosity, hot elastic modulus, corrosion cup-tests, thermodynamic simulations, were carried out to analyze the performance of such ceramics. The results indicated that ZnAl2O4 was mainly formed above 800 degrees C, favoring an earlier sintering of the samples. Besides that, the softening of the castables was observed above 1200 degrees C, which resulted in the elastic modulus decay of the samples during their first heating cycle due to the formation of SiO2-rich liquid phase in the resulting microstructure. Cement-free samples obtained after calcination (600 degrees C for 5h) presented enhanced corrosion resistance when placed in contact with molten slag at 1500 degrees C. Although, silica fume addition to the castables negatively affected their corrosion performance, it helped to counterbalance the expansion associated with the spinel and calcium aluminates formation.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Spinel-containing alumina-based refractory castables
    Braulio, M. A. L.
    Rigaud, M.
    Buhr, A.
    Parr, C.
    Pandolfelli, V. C.
    CERAMICS INTERNATIONAL, 2011, 37 (06) : 1705 - 1724
  • [2] Effect of submicron spinel powders on the microstructure evolution and properties of alumina-based refractory castables
    Chen, Pingan
    Wang, Yulong
    Li, Xiangcheng
    Zhu, Boquan
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2017, 14 (04) : 748 - 758
  • [3] Conventional and microwave-assisted sintering of ZnO-containing CAC-bonded alumina-based refractory castables
    Borges, O. H.
    Cardoso, A. L. F.
    Moreira, M. H.
    Klein-Gunnewiek, R. F.
    Pandolfelli, V. C.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (14) : 6562 - 6570
  • [4] Rheology of alumina-based graphite-containing castables
    Ye, F
    Rigaud, M
    Jia, Q
    Zhong, X
    ADVANCES IN REFRACTORIES FOR THE METALLURGICAL INDUSTRIES IV, 2004, : 841 - 854
  • [5] Rheology of Alumina-Based Graphite-Containing Castables
    M. Rigaud
    China'sRefractories, 2005, (01) : 3 - 8
  • [6] Boron sources as sintering additives for alumina-based refractory castables
    Giovannelli Maizo, I. D.
    Luz, A. P.
    Pagliosa, C.
    Pandolfelli, V. C.
    CERAMICS INTERNATIONAL, 2017, 43 (13) : 10207 - 10216
  • [7] ZnO and MgO as inducers of spinel-like phase formation on alumina-based castables
    Borges, O. H.
    Sardelli, J. A. P.
    Neto, C. Pagliosa
    da Luz, A. P.
    Pandolfelli, V. C.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (15) : 7335 - 7342
  • [8] Effect of SiO2 Micro-powders on the Properties of Alumina-based Ceramic Core
    Wang, Li-ge
    Zuo, Bin
    Zhu, Guang-zhi
    Wang, En-ze
    Zhang, Zheng-quan
    ADVANCES IN CHEMISTRY RESEARCH II, PTS 1-3, 2012, 554-556 : 731 - +
  • [9] Effect of CaO/SiO2 Slag Mass Ratio on Dissolution Rate of Alumina-based Refractory Ceramics
    ZENG Fanbo
    HUANG Ao
    WANG Xinlian
    LI Shenghao
    ZHANG Shuzhe
    QU Pengcheng
    GU Huazhi
    China's Refractories, 2023, 32 (01) : 30 - 34
  • [10] Microstructure and phase evolution of alumina-spinel self-flowing refractory castables containing nano-alumina particles
    Otroj, Sasan
    Daghighi, Arash
    CERAMICS INTERNATIONAL, 2011, 37 (03) : 1003 - 1009