Effect of bismuth deficiency with K substitution for Na on piezoelectric properties and crystal structure of Bi0.5-x(Na0.8-yK0.2+y)0.5TiO3-3x/2 (0 ≤ x ≤ 0.015, 0 ≤ y ≤ 0.1) ceramics

被引:0
|
作者
Kan, Akinori [1 ,2 ]
Araki, Kentaro [2 ]
Ogawa, Hirotaka [3 ]
机构
[1] Meijo Univ, Dept Vehicle & Mech Engn, Nagoya 4688502, Japan
[2] Meijo Univ, Grad Sch Sci & Technol, Nagoya 4688502, Japan
[3] Nagoya Ind Sci Res Inst, Dept Res, Nagoya 4640819, Japan
关键词
Ceramics; Solid state reactions; Crystal structure; Piezoelectricity; FIELD-INDUCED STRAIN; A-SITE; PHASE-TRANSITIONS; TITANATE; SPECTROSCOPY; TEMPERATURE; DIFFRACTION; PERFORMANCE; SYSTEM; RAMAN;
D O I
10.1016/j.jallcom.2023.172089
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The piezoelectric properties and crystal structure of Bi0.5- x(Na0.8-yK0.2+y)(0.5)TiO3-3x/2 (0 <= x <= 0.015, 0 <= y <= 0.1) ceramics were characterized in this study. The crystal-structure refinement for Bi0.5- x(Na0.8-yK0.2+y)(0.5)TiO3-3x/2 was carried out using synchrotron X-ray diffraction data and Rietveld analysis and revealed the coexistence of rhombohedral (R3c) and tetragonal (P4mm) phases for the compositions with 0 <= x <= 0.015, although the fraction of these phases was almost independent of the composition x (49% for the rhombohedral phase and 51% for the tetragonal phase at x = 0.015). The Bi deficiency led to an increase in the lattice distortion of rhombohedral phase and a decrease in the that of tetragonal phase. The piezoelectric constant (d(33)) value decreased from 151.5 to 120.6 pC/N as x was increased from 0 to 0.015, and a shift of the depolarization temperature to higher temperatures was also confirmed by in situ d(33) measurements. These results are attributed to an increase in the lattice distortion of rhombohedral phase enhanced by the Bi deficiency. The K substitution for Na in Bi-0.485(Na0.8-yK0.2+y)(0.5)TiO2.9775 led to the formation of a morphotropic phase boundary (MPB) in the composition range 0 <= y <= 0.06, resulting in an increase in the fraction of the tetragonal phase. Although a decrease in the mechanical quality factor (Q(m)) was observed for K-rich compositions, the highest d(33) value of 195.4 pC/N with a mechanical coupling factor of 32.9% was obtained for the Bi-0.485(Na0.76K0.24)(0.5)TiO2.9775 (y = 0.04) ceramic because of the enhancement of the tetragonality in the MPB region, resulting in the onset of depolarization at similar to 170 degrees C.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Structure, dielectric, and ferroelectric properties of (1-x)Bi0.5Na0.5TiO3-X K0.5Na0.5NbO3 (0 ≤ x ≤ 0.1) solid solution
    Aissa, Mohamed
    Zannen, Moneim
    Hadouchi, Mohammed
    Kacem, Hend
    Belhadi, Jamal
    Alzahrani, Hassan A. H.
    Aissa, Abdallah
    El Marssi, Mimoun
    Majdoub, Mustapha
    Lahmar, Abdelilah
    CERAMICS INTERNATIONAL, 2023, 49 (16) : 26369 - 26379
  • [2] High thermal stability of piezoelectric properties in (Na0.5Bi0.5TiO3)x-(BaTiO3)y-(Na0.5K0.5NbO3)1-x-y ceramics
    Gupta, Shashaank
    Priya, Shashank
    APPLIED PHYSICS LETTERS, 2013, 102 (01)
  • [3] Piezoelectric and dielectric properties of [Bi0.5(Na1-x-y-zKxLiyAgz)0.5]TiO3 piezoelectric ceramics
    Lin, Dun-Min
    Xiao, Ding-Quan
    Zhu, Jian-Guo
    Yu, Ping
    FERROELECTRICS, 2007, 358 : 999 - 1004
  • [4] Dielectric and piezoelectric properties of (Na0.8K0.2)0.5Bi0.5TiO3 ceramics
    Li, YM
    Chen, W
    Xu, Q
    Zhou, J
    Liao, MS
    JOURNAL OF INORGANIC MATERIALS, 2004, 19 (04) : 817 - 822
  • [5] Phase transitions, dielectric and piezoelectric properties of [(Na0.5Bi0.5)1-xLix]TiO3 (x=0-0.1) ceramics
    Ilina, T. S.
    Kislyuk, A. M.
    Kiselev, D. A.
    Politova, E. D.
    Kaleva, G. M.
    Mosunov, A., V
    Sadovskaya, N., V
    FERROELECTRICS, 2021, 574 (01) : 144 - 155
  • [6] Structural, electrical, and strain properties of stoichiometric 1-x-y(Bi0.5Na0.5) TiO3-x(Bi0.5K0.5TiO3)-y(Na0.5K0.5)NbO3 solid solutions
    Singh, Amrita
    Chatterjee, Ratnamala
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (02)
  • [7] Structure and electrical properties of Bi0.5Na0.5TiO3-Y0.5Na0.5TiO3-BaTiO3 lead-free piezoelectric ceramics
    Lin, Dunmin
    Kwok, K. W.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2010, 21 (03) : 291 - 297
  • [8] Structure and electrical properties of Bi0.5Na0.5TiO3-Y0.5Na0.5TiO3-BaTiO3 lead-free piezoelectric ceramics
    Dunmin Lin
    K. W. Kwok
    Journal of Materials Science: Materials in Electronics, 2010, 21 : 291 - 297
  • [9] Enhanced energy-storage properties of (1-x)[(1-y)(Bi0.5Na0.5)TiO3-y (Bi0.5K0.5)TiO3]-x(K0.5Na0.5)NbO3 lead-free ceramics
    Hao, Jigong
    Xu, Zhijun
    Chu, Ruiqing
    Li, Wei
    Du, Juan
    Fu, Peng
    SOLID STATE COMMUNICATIONS, 2015, 204 : 19 - 22
  • [10] Structure, microstructure and electrical properties of (1-x-y)Bi0.5Na0.5TiO3-xBi0.5K0.5TiO3-yBi0.5Li0.5TiO3 lead-free piezoelectric ceramics
    Yang, Zupei
    Hou, Yuting
    Pan, Hong
    Chang, Yunfei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 480 (02) : 246 - 253