A laser additive manufactured metastable Ti-10V-2Fe-3Al β-titanium alloy: Microstructure, mechanical properties, and deformation mechanisms

被引:2
|
作者
Wang, Wei [1 ]
Chen, Chaoyue [1 ]
Zhao, Ruixin [1 ]
Gludovatz, Bernd [2 ]
Lu, Xufei [3 ]
Zhang, Kai [4 ,5 ]
Shuai, Sansan [1 ]
Hu, Tao [1 ]
Xu, Songzhe [1 ]
Wang, Jiang [1 ]
Ren, Zhongming [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, State Key Lab Adv Special Steels, Shanghai 200444, Peoples R China
[2] Univ New South Wales UNSW Sydney, Sch Mech & Mfg Engn, Sydney, NSW 2052, Australia
[3] Univ Politecn Cataluna, CIMNE, Barcelona 08034, Spain
[4] Univ Shanghai Sci & Technol, Sch Mat Sci & Engn, Shanghai 20093, Peoples R China
[5] Monash Ctr Addit Mfg, Notting Hill, Vic 3168, Australia
基金
上海市自然科学基金; 中国国家自然科学基金;
关键词
Laser powder bed fusion; beta-titanium alloy; Precipitation; Deformation structures; Mechanical properties; INDUCED MARTENSITIC-TRANSFORMATION; TENSILE PROPERTIES; ENERGY DEPOSITION; BEHAVIOR; PHASE; STRESS; TI-6AL-4V; STABILITY; PARTS;
D O I
10.1016/j.msea.2023.145863
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present work, the deformation mechanism is investigated by tailoring the microstructure of a laser powder bed fusion (L-PBF) processed beta-type Ti-10V-2Fe-3Al (Ti1023) alloy. The microstructure analysis shows columnar beta grains with <001>//BD texture. The alpha phase appeared lath morphology after using laser power of 160 W and presented fine and intersected morphology at 200 W, and the shape of co clusters transformed from bulk to intersected acicular with increasing laser power. The Ti1023 alloy exhibits excellent mechanical properties with a total elongation of 18 % and high yield strength above 828 MPa. The existence of alpha '' phase as well as {332}< 113> and {112}<111> deformed twins were found in fractured microstructure at 160W, confirming the multiple deformation mechanisms consisting of dislocation slip, transformation-induced plasticity (TRIP), and twinning-induced plasticity (TWIP). By increasing the laser power, the deformation mechanisms are limited to dislocation slip. At last, the finite element analysis of the temperature and temperature gradient change reveals the underlying mechanism for microstructure evolution based on thermal history. This study provides a pathway to regulate L-PBF Ti1023 strengthening and work-hardening behavior by controlling the process parameters during the fabrication of the material.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Hot deformation mechanisms in metastable beta titanium alloy Ti-10V-2Fe-3Al
    Balasubrahmanyam, VV
    Prasad, YVRK
    MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (10) : 1222 - 1228
  • [2] Effect of Solution and Aging Treatments Parameters on Microstructure and Mechanical Properties of Laser Additive Manufactured Ti-10V-2Fe-3Al Metastable β
    Yi Zhang
    Zongge Jiao
    Xu Cheng
    Shuquan Zhang
    Jia Li
    Yudai Wang
    Xianzhe Ran
    JOM, 2024, 76 : 1913 - 1923
  • [3] Effect of Solution and Aging Treatments Parameters on Microstructure and Mechanical Properties of Laser Additive Manufactured Ti-10V-2Fe-3Al Metastable β
    Zhang, Yi
    Jiao, Zongge
    Cheng, Xu
    Zhang, Shuquan
    Li, Jia
    Wang, Yudai
    Ran, Xianzhe
    JOM, 2024, 76 (04) : 1913 - 1923
  • [4] Microstructure and mechanical properties of laser welded Ti-10V-2Fe-3Al (Ti1023) titanium alloy
    Chamanfar, Ahmad
    Huang, Meng-Fu
    Pasang, Timotius
    Tsukamoto, Masahiro
    Misiolek, Wojciech Z.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (04): : 7721 - 7731
  • [5] Isothermal hot deformation behaviour of metastable a titanium alloy Ti-10V-2Fe-3Al
    Robertson, D. G.
    McShane, H. B.
    1997, (13)
  • [6] Isothermal hot deformation behaviour of metastable beta titanium alloy Ti-10V-2Fe-3Al
    Robertson, DG
    McShane, HB
    MATERIALS SCIENCE AND TECHNOLOGY, 1997, 13 (07) : 575 - 583
  • [7] Influence of hot rolling deformation on microstructure and properties of Ti-10V-2Fe-3Al alloy
    Shang, Guo-Qiang
    Zhu, Zhi-Shou
    Kou, Hong-Chao
    Wang, Xin-Nan
    Fei, Yue
    Chang, Hui
    Li, Jin-Shan
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (03): : 108 - 113
  • [8] Effect of cold rolling deformation on the microstructure and properties of Ti-10V-2Fe-3Al alloy
    Qi, Lichun
    Qiao, Xueliang
    Huang, Lijun
    Huang, Xu
    Xiao, Wenlong
    Zhao, Xinqing
    MATERIALS CHARACTERIZATION, 2019, 155
  • [9] Effect of boron and carbon addition on microstructure and tribological properties of metastable beta titanium alloy, Ti-10V-2Fe-3Al
    Banoth, Ravinaik
    Chandravanshi, V.
    Bhattacharjee, A.
    Nandy, T. K.
    Rao, G. V. S. Nageswara
    MATERIALS TODAY-PROCEEDINGS, 2019, 18 : 2700 - 2707
  • [10] Effect of α Composite Layer on the Microstructure and Mechanical Properties of Ti-10V-2Fe-3Al Alloy
    Bai Xinfang
    Zhao Yongqing
    Zeng Weidong
    Jia Zhiqiang
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (01) : 12 - 17