Simultaneous Application of Oxalic Acid and Sodium Dithionite for Synchronous Removal of Iron and Silica from Low-Grade Bauxite: Kinetics and Mechanism

被引:2
|
作者
Zonouz, Tohid Razzaghi [1 ]
Rezai, Bahram [1 ]
Bahri, Zahra [2 ]
Jahromi, Ahmad Azargoon [3 ]
机构
[1] Amirkabir Univ Technol, Dept Min & Met Engn, Tehran 158754413, Iran
[2] ACECR Tarbiat Modares, Inst Mineral Proc, Dept Control & Modeling Mineral Proc Syst, Tehran 1411883684, Iran
[3] Yazd Univ, Dept Min & Met Engn, Yazd 8915818411, Iran
关键词
Low-grade bauxite; Alkaline leaching; Pretreatment; Kinetics; Activation energy; MAGNETIC SEPARATION; DIASPORIC BAUXITE; KAOLINITE; DISSOLUTION; BENEFICIATION; REDUCTION; TRANSFORMATION; DIGESTION; MINERALS; ALUMINUM;
D O I
10.1007/s40831-023-00661-w
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Bauxite is widely used to produce alumina. There are many bauxite resources with high iron content. These resources could not be processed and utilized efficiently due to the high concentration of iron (Fe). The alkaline leaching process has been proposed to remove iron from these bauxite resources. Therefore, in this study, the alkaline leaching process was employed, and the effects of sodium dithionite (on the decomposition of iron oxides), sodium carbonate (adjustment of the solution pH), and oxalic acid (on the prevention of precipitation of Fe2+ complexes and the decomposition of kaolinite) were investigated using a central composite design. The results showed that 77 and 54% of iron and silica were removed under optimum operating conditions. These conditions included the use of oxalic acid at a dosage of 24 g and sodium dithionite at a concentration of 0.08 M, reaction time of 75 min, solid content of 10%, pH of 8-8.2, and stirring speed of 700 rpm. The kinetics modeling indicated that the alkaline leaching of iron from high-iron bauxite was controlled by the product layer diffusion mechanism. In addition, the calculated activation energy was 18.8 kJ/mol. The removal mechanism was studied by X-ray diffraction, X-ray fluorescence, and Fourier transform infrared spectroscopy analysis.
引用
收藏
页码:511 / 521
页数:11
相关论文
共 50 条
  • [1] Simultaneous Application of Oxalic Acid and Sodium Dithionite for Synchronous Removal of Iron and Silica from Low-Grade Bauxite: Kinetics and Mechanism
    Tohid Razzaghi Zonouz
    Bahram Rezai
    Zahra Bahri
    Ahmad Azargoon Jahromi
    Journal of Sustainable Metallurgy, 2023, 9 : 511 - 521
  • [2] Extracting silica and alumina from low-grade bauxite
    Viktor L. Rayzman
    Andrei V. Aturin
    Ilya Z. Pevzner
    Viktor M. Sizyakov
    Leonid P. Ni
    Igor K. Filipovich
    JOM, 2003, 55 : 47 - 50
  • [3] Leaching for iron removal from low-grade bauxite ore to access refractory instruction
    Jalili, Zahra
    Bahrami, Ataallah
    Ghadri, Masoud
    Akhgar, Behzad Nemati
    Kazemi, Fatemeh
    RUDARSKO-GEOLOSKO-NAFTNI ZBORNIK, 2022, 37 (01): : 55 - 64
  • [4] Flotation enhancement of low-grade bauxite using oxalic acid as surface pretreatment agent
    Li, Huaxia
    Chai, Wencui
    Cao, Yijun
    Yang, Shichong
    APPLIED SURFACE SCIENCE, 2022, 577
  • [5] Leaching kinetics of iron from low grade kaolin by oxalic acid solutions
    Martinez-Luevanos, A.
    Rodriguez-Delgado, M. G.
    Uribe-Salas, A.
    Carrillo-Pedroza, F. R.
    Osuna-Alarcon, J. G.
    APPLIED CLAY SCIENCE, 2011, 51 (04) : 473 - 477
  • [6] Removal of iron from silica sand by leaching with oxalic acid
    Taxiarchou, M
    Panias, D
    Douni, I
    Paspaliaris, I
    Kontopoulos, A
    HYDROMETALLURGY, 1997, 46 (1-2) : 215 - 227
  • [7] Simultaneous application of oxalic acid and dithionite for enhanced extraction of arsenic bound to amorphous and crystalline iron oxides
    Lee, Myeong Eun
    Jeon, Eun-Ki
    Tsang, Daniel C. W.
    Baek, Kitae
    JOURNAL OF HAZARDOUS MATERIALS, 2018, 354 : 91 - 98
  • [8] Leaching Kinetics of Lanthanide in Sulfuric Acid from Low Grade Bauxite
    Kusrini, Eny
    Usman, Anwar
    Trisko, Nici
    Harjanto, Sri
    Rahman, Arif
    MATERIALS TODAY-PROCEEDINGS, 2019, 18 : 462 - 467
  • [9] Removal of Potassium and Iron in Low Grade Bauxite by a Calcination-Acid Leaching Process
    Li, Zhuang
    Cao, Yijun
    Jiang, Yuanli
    Han, Guihong
    Fan, Guixia
    Chang, Luping
    MINERALS, 2018, 8 (04)
  • [10] Beneficiation Strategies for Removal of Silica and Alumina from Low-Grade Hematite-Goethite Iron Ores
    Nunna, V.
    Suthers, S. P.
    Pownceby, M. I.
    Sparrow, G. J.
    MINERAL PROCESSING AND EXTRACTIVE METALLURGY REVIEW, 2022, 43 (08): : 1049 - 1067