Role of headspace environment for phase change carbonates on the corrosion of stainless steel 316L: High temperature thermal storage cycling in concentrated solar power plants

被引:7
|
作者
Yin, Yanting [1 ,2 ]
Rumman, Raihan [1 ,2 ]
Sarvghad, Madjid [3 ]
Bell, Stuart [3 ]
Ong, Teng-Cheong [3 ]
Jacob, Rhys [4 ,5 ]
Liu, Ming [4 ]
Flewell-Smith, Ross [4 ]
Sheoran, Shane [4 ]
Severino, John [4 ]
Belusko, Martin [4 ]
Bruno, Frank [4 ]
Will, Geoffrey [3 ]
Steinberg, Theodore A. [3 ]
Lewis, David A. [1 ,2 ]
Andersson, Gunther G. [1 ,2 ]
机构
[1] Flinders Univ S Australia, Flinders Inst Nanoscale Sci & Technol, Adelaide, SA 5042, Australia
[2] Flinders Univ S Australia, Coll Sci & Engn, Flinders Microscopy & Microanal, Adelaide, SA 5042, Australia
[3] Queensland Univ Technol, Sci & Engn Fac, Sch Mech, Med & Proc Engn, Brisbane, Qld, Australia
[4] Univ South Australia, Future Ind Inst, Mawson Lakes Blvd,Mawson Lakes, Adelaide, SA 5095, Australia
[5] Forschungszentrum Julich, Inst Energy & Climate Res, Microstruct & Properties Mat IEK-2, D-52425 Julich, Germany
关键词
MOLTEN-SALT; HOT CORROSION; INCONEL; 601; ENERGY; BEHAVIOR; SODIUM; ALLOYS; ALUMINUM; CATHODE; SYSTEMS;
D O I
10.1016/j.solmat.2022.112170
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The mechanisms leading to corrosion in stainless steel containments for thermal energy storage through phase change materials, such as carbonates and chlorides, are crucial for understanding the degradation of these steel alloys. A comprehensive study of this area will allow for down-selection of materials suitable for solar thermal energy storage (TES) operation at an elevated temperature range.Samples of stainless steel (SS) 316L were subjected to a cyclic heat environment of 550-750 degrees C in air and argon headspace environments, in the presence of a carbonate salt phase change material (PCM). A series of complementary microscopy, spectroscopy and diffractometry analytical techniques were applied to the corroded SS316L. Corrosion rate, interface formation and chemical products with respect to thermal cycling are presented with associated degradation mechanism explained and comparisons are made among different gas environments and varied immersion conditions.In the PCM under ambient air conditions, steel surfaces were mainly corroded by the penetration of oxidants from air, such as H2O or O2, along grain boundaries. SS316L samples demonstrated more severe degradation when exposed to air with a small fraction of PCM vapour present compared to when they were exposed to liquid or solid PCM. Cycling in Ar resulted in less corrosion in samples as opposed to when they were exposed to an air environment. In an Ar environment corrosion is driven via the formation of chromite, while the SS316L showed a less degradation when exposed to Ar with a small fraction of PCM vapour compared to when it was immersed in PCM. The mechanisms for degradation in air and in Ar are common in that the corrosion products of Cr and Ni dissolve in the PCM thus removing any layer that could protect against corrosion.The present study provides insight into corrosion of stainless-steel when exposed to carbonate salts, in air and inert gas environments, and contributes to down-selection of materials for solar thermal energy storage.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Probing High-Temperature Electrochemical Corrosion of 316 Stainless Steel in Molten Nitrate Salt for Concentrated Solar Power Plants
    Singh, Mahander Pratap
    Basu, Bikramjit
    Chattopadhyay, Kamanio
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (06) : 4902 - 4908
  • [2] Probing High-Temperature Electrochemical Corrosion of 316 Stainless Steel in Molten Nitrate Salt for Concentrated Solar Power Plants
    Mahander Pratap Singh
    Bikramjit Basu
    Kamanio Chattopadhyay
    Journal of Materials Engineering and Performance, 2022, 31 : 4902 - 4908
  • [3] Corrosion of 316L stainless steel in high temperature water and steam: Mechanisms of corrosion
    Hanbury, Rigel D.
    Was, Gary S.
    JOURNAL OF NUCLEAR MATERIALS, 2024, 599
  • [4] High temperature corrosion of stainless steel AISI 316L in molten nitrate salts based thermofluids for concentration solar plants
    Sandoval-Amador, Anderson
    Gimena Jaimes-Campos, Angie
    Xiomara Mogollon-Sanabria, Astrid
    Armando Estupinan-Duran, Hugo
    Yesid Pena-Ballesteros, Dario
    MATERIA-RIO DE JANEIRO, 2020, 25 (03):
  • [5] Influence of sigma phase on corrosion behavior of 316L stainless steel in high temperature and high pressure water
    Ding, Jie
    Han, En-Hou
    Zhang, Zhiming
    Wang, Siyan
    Wang, Jianqiu
    MATERIALS AT HIGH TEMPERATURES, 2017, 34 (01) : 78 - 86
  • [6] Effect of High Temperature on the Corrosion Behavior and Passive Film Composition of 316L Stainless Steel in Concentrated NaOH Solution
    Li, Chunliu
    Wang, Ruishu
    Jiang, Yuting
    Xie, Hongwei
    Liu, Biao
    Wang, Shaona
    Du, Hao
    Zhang, Yi
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2025, 172 (02)
  • [7] High temperature corrosion of wrought and wire arc additively manufactured 316L stainless steel in a simulated boiler environment
    Mannan, Muthu Shanmugam
    Jang, Changheui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 4278 - 4292
  • [8] Effect of pH on corrosion behavior of 316L stainless steel in hydrogenated high temperature water
    Wang, Jiazhen
    Wang, Jianqiu
    Ming, Hongliang
    Zhang, Zhiming
    Han, En-Hou
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (05): : 580 - 589
  • [9] The Corrosion Behavior of 316L Stainless Steel in H2S environment at high temperatures
    Zhang, Lei
    Tang, Xian
    Wang, Zhu
    Li, Ting
    Zhang, Ziru
    Lu, Minxu
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (09): : 8806 - 8819
  • [10] The role of lead-bismuth eutectic temperature in affecting fretting corrosion of 316L stainless steel
    Chen, Hui
    Feng, Zhipeng
    Mei, Guiyu
    Tan, Wei
    Zhu, Guorui
    WEAR, 2025, 572