摘要
Inhibition of localized corrosion of Ni-Ti superelastic alloy in 0.1 M NaOCl solution has been attempted by adding Na2CO3. The addition of Na2CO3 scarcely affects the pitting potential. Nevertheless, at a more noble than pitting potential, the increase in current density is inhibited by increasing the amount of Na2CO3 added. In the immersion test for 24 h, with the addition of 0.01 M or 0.05 M Na2CO3, the corrosion potential often shifts rapidly in the less noble direction similarly to that observed without Na2CO3 addition, but it tends to shift back in the noble direction in a short time. By increasing the amount of Na2CO3 added to 0.1 M, the corrosion potential is stabilized at the noble potential. The mass losses due to localized corrosion are significantly inhibited by the addition even of 0.01 M Na2CO3. With the addition of Na2CO3 above 0.05 M, only very small corrosion pits are observed on the surface of the specimen. The relative XPS peak intensity of OH- increases with the amount of Na2CO3 added. The present results indicate that the addition of Na2CO3 is effective in the inhibition of the localized corrosion in NaOCl solution.
引用
收藏
页码:585 / 592
页数:8
相关论文
共 50 条
  • [1] Inhibition of Localized Corrosion of Ni–Ti Superelastic Alloy in Sodium Hypochlorite Solution by Sodium Carbonate Addition
    Ryosuke Hayashi
    Ken’ichi Yokoyama
    Shape Memory and Superelasticity, 2023, 9 : 585 - 592
  • [2] Inhibition of localized corrosion of Ni-Ti superelastic alloy in NaCl solution by hydrogen charging
    Yokoyama, Ken'ichi
    Hirata, Yuki
    Inaba, Toshiaki
    Mutoh, Kenichiro
    Sakai, Jun'ichi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 639 : 365 - 372
  • [3] Inhibition of localized corrosion of Ni-Ti superelastic alloy in NaCl solution by hydrogen charging
    Yokoyama, Ken'Ichi
    Hirata, Yuki
    Inaba, Toshiaki
    Mutoh, Kenichiro
    Sakai, Jun'Ichi
    Journal of Alloys and Compounds, 2015, 639 : 365 - 372
  • [4] Corrosion behaviour of a superelastic Ni-Ti alloy
    Vandenkerckhove, R
    Chandrasekaran, M
    Vermaut, P
    Portier, R
    Delaey, L
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 378 (1-2): : 532 - 536
  • [5] Countermeasure for corrosion and hydrogen embrittlement of Ni-Ti superelastic alloy in acidic fluoride solution by adding sodium bicarbonate and hydrogen peroxide
    Yamaguchi, Naoya
    Yokoyama, Ken'ichi
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2021, 56 (05) : 419 - 426
  • [6] Inhibition of hydrogen embrittlement of Ni-Ti superelastic alloy in acid fluoride solution by hydrogen peroxide addition
    Yokoyama, Ken'ichi
    Yazaki, Yushin
    Sakai, Jun'ichi
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2011, 98A (03) : 404 - 411
  • [7] Corrosion and Mechanical Degradation of Ni-Ti Superelastic Alloy in Neutral Fluoride Solution
    Toshio Ogawa
    Hirokaze Takada
    Kuniaki Maruoka
    Journal of Materials Engineering and Performance, 2018, 27 : 4010 - 4015
  • [8] Corrosion and Mechanical Degradation of Ni-Ti Superelastic Alloy in Neutral Fluoride Solution
    Ogawa, Toshio
    Takada, Hirokaze
    Maruoka, Kuniaki
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (08) : 4010 - 4015
  • [9] Effects of temperature, phase, elastic deformation and transformation on inhibition of localized corrosion of hydrogen-charged Ni-Ti superelastic alloy in NaCl solution
    Nishimoto, Shigekazu
    Yokoyama, Ken'ichi
    Inaba, Toshiaki
    Mutoh, Kenichiro
    Sakai, Jun'ichi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 682 : 22 - 28
  • [10] Hydrogen embrittlement of Ni-Ti superelastic alloy in fluoride solution
    Yokoyama, K
    Kaneko, K
    Moriyama, K
    Asaoka, K
    Sakai, J
    Nagumo, M
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2003, 65A (02) : 182 - 187