Fabrication of hypereutectic Al-Si alloy with improved mechanical and thermal properties by hot extrusion

被引:6
|
作者
Ding, Chao [1 ,2 ]
Hao, Huali [3 ]
Lu, Zhouguang [2 ]
Yu, Changyang [2 ]
Wu, Xinzhi [2 ]
Yu, Peng [4 ]
Ye, Shulong [1 ,2 ]
机构
[1] Shenzhen MSU BIT Univ, Fac Mat Sci, Shenzhen 518172, Peoples R China
[2] Southern Univ Sci & Technol, Dept Mat Sci & Engn, Shenzhen 518055, Peoples R China
[3] Wuhan Univ, Sch Civil Engn, Wuhan 420072, Peoples R China
[4] Shenzhen ElementPlus Mat Technol Co Ltd, Shenzhen 518107, Peoples R China
关键词
Hypereutectic Al-Si alloys; Hot extrusion; Microstructure; Thermal properties; Mechanical properties; TENSILE PROPERTIES; EUTECTIC SI; MICROSTRUCTURE; COMPOSITES; ALUMINUM; CONDUCTIVITY;
D O I
10.1016/j.matchar.2023.113026
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Silicon phase in hypereutectic Al-Si powders appears as primary Si and eutectic Si. Due to the poor thermal stability of eutectic Si, the material suffers from pores, stress concentration and dislocation packing during hot extrusion process, resulting in low density and poor thermal properties. In order to eliminate the eutectic Si, a heat treatment is conducted on Al-20Si powder before hot extrusion. Because of the Ostwald ripening effect, the eutectic Si and dislocations in the powder are replaced by isolated Si lumps and a clear Al matrix. As a result, the formability and thermal properties of the material are greatly improved. The extruded samples made from the treated powder present high relative densities 99.7-100%, ultimate tensile strength (UTS) 167-170 MPa, elongations 8.8-10.8% and thermal conductivities (TCs) 191-195 Wm- 1 K-1 and low coefficient of thermal expansions (CTEs) 13.8-14.5 x 10-6/K. The excellent mechanical and thermal properties are attributed to the elimination of eutectic Si from the treated powder and as-extruded alloys. In addition, hot extrusion introduces in-situ Al2O3 in the Si surface, Al grain boundary and Al grains, which is beneficial to reducing and stabilizing the CTE of the material. Moreover, it hinders Ostwald ripening and thus growth of the Si particles during the service of the material.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Effect of hot extrusion process on microstructure and mechanical properties of hypereutectic Al-Si alloys
    Li Runxia
    Yu Fuxiao
    Zuo Liang
    [J]. CHINA FOUNDRY, 2011, 8 (01) : 145 - 149
  • [2] Effect of hot extrusion process on microstructure and mechanical properties of hypereutectic Al-Si alloys
    Li Runxia1
    2.Northeastern University
    [J]. China Foundry, 2011, 8 (01) : 145 - 149
  • [3] Mechanical properties of hypereutectic Al-Si alloy by semisolid processing
    李树索
    赵爱民
    毛卫民
    钟雪友
    [J]. Transactions of Nonferrous Metals Society of China, 2000, (04) : 441 - 444
  • [4] Mechanical properties of hypereutectic Al-Si alloy by semisolid processing
    Li, SS
    Zhao, AM
    Mao, WM
    Zhong, XY
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2000, 10 (04) : 441 - 444
  • [5] Improved mechanical and frictional properties of hypereutectic Al-Si alloy by modifying Si phase with La addition
    Peng, Jianfei
    Wang, Wanlin
    Yuan, Shuaijie
    Zhan, Yan
    Zeng, Jie
    Gan, Peiyuan
    Ji, Junyu
    [J]. MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [6] A method for improving the mechanical properties of a hypereutectic Al-Si alloy by introducing the α-Al phase
    Luo, Song
    Wei, Xiaowei
    [J]. INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2016, 107 (05) : 422 - 428
  • [7] Cooling thermal parameters, microstructural spacing and mechanical properties in a directionally solidified hypereutectic Al-Si alloy
    Reyes, Rodrigo V.
    Kakitani, Rafael
    Costa, Thiago A.
    Spinelli, Jose E.
    Cheung, Noe
    Garcia, Amauri
    [J]. PHILOSOPHICAL MAGAZINE LETTERS, 2016, 96 (06) : 228 - 237
  • [8] Rapidly solidified hypereutectic Al-Si alloys prepared by powder hot extrusion
    李元元
    张大童
    NGAI Tungwai Leo
    张卫文
    [J]. Transactions of Nonferrous Metals Society of China, 2002, (05) : 878 - 881
  • [9] Hot Deformation Behavior of A390 Hypereutectic Al-Si Alloy
    Hu, Xiaogang
    Yang, Bicheng
    Xu, Jun
    Wang, Haijun
    [J]. MATERIALS PERFORMANCE, MODELING AND SIMULATION, 2013, 749 : 88 - 95
  • [10] Characterization of precipitates in a hot-deformed hypereutectic Al-Si alloy
    He, Kezhun
    Yu, Fuxiao
    Zhao, Dazhi
    Zuo, Liang
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 539 : 74 - 81