Tribological behavior of hot-pressed boron carbide with oxidation

被引:0
|
作者
WANG Ling sen
机构
关键词
oxidation; boron carbide; friction factor; boron oxide; boron acid;
D O I
暂无
中图分类号
O613 [非金属元素及其化合物];
学科分类号
070301 ; 081704 ;
摘要
The oxidation behavior at 973 1 273 K and the effect of oxidation on the room temperature tribological properties of hot pressed boron carbide ceramic were investigated. Oxidized samples were studied by X ray diffractometer and scanning electron microscopy. It is demonstrated that the oxidation results in the formation of a thin transparent B 2O 3 film, and the oxide film is severely cracked during cooling due to the thermal expansion mismatch between the oxide film and B 4C substrate. B 2O 3 reacts with moisture in air to form boric acid, which is a kind of solid lubricant. The sliding friction factors of oxidized B 4C pair are about 0.05 0.08, compared to 0.25 0.35 of the as received B 4C pair. When the oxidation temperature is up to 1 273 K, severe unstability and increase of friction factor are observed. Visual inspection of the wear track reveals that the lubricant film is broken and some debris particles occur on and around the rubbing surfaces, because the friction interface is rough by the severe etching of grain boundaries.
引用
收藏
页码:89 / 93
页数:5
相关论文
共 50 条
  • [1] Tribological behavior of hot-pressed boron carbide with oxidation
    Wang, LS
    Wu, F
    Zhang, JS
    Fan, Y
    Liu, BW
    Gao, Y
    [J]. JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2001, 8 (02): : 89 - 93
  • [2] Tribological behavior of hot-pressed boron carbide with oxidation
    Ling-sen Wang
    Fang Wu
    Jin-sheng Zhang
    Yi Fan
    Bo-wei Liu
    You Gao
    [J]. Journal of Central South University of Technology, 2001, 8 : 89 - 93
  • [3] Tribological properties of hot-pressed boron carbide ceramic
    吴芳
    王零森
    张金生
    樊毅
    刘伯威
    高游
    [J]. Transactions of Nonferrous Metals Society of China, 2001, (01) : 119 - 122
  • [4] Tribological properties of hot-pressed boron carbide ceramic
    Wu, F
    Wang, LS
    Zhang, JS
    Fan, Y
    Liu, BW
    Gao, Y
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2001, 11 (01) : 119 - 122
  • [5] OXIDATION OF HOT-PRESSED BORON-CARBIDE
    EFIMENKO, LN
    LIFSHITS, EV
    OSTAPENKO, IT
    SNEZHKO, IA
    SHEVYAKOVA, EP
    [J]. SOVIET POWDER METALLURGY AND METAL CERAMICS, 1987, 26 (04): : 318 - 321
  • [6] Tribological properties of hot-pressed boron carbide ceramic
    [J]. Wu, F., 2001, Allerton Press Inc. (11):
  • [7] Oxidation of hot-pressed silicon carbide
    Kim, JJ
    [J]. JOURNAL OF MATERIALS SCIENCE LETTERS, 1996, 15 (19) : 1687 - 1689
  • [8] HIGH-TEMPERATURE OXIDATION OF HOT-PRESSED BORON-CARBIDE
    LAVRENKO, VA
    GOGOTSI, IG
    FRANTSEVICH, IN
    [J]. DOKLADY AKADEMII NAUK SSSR, 1984, 275 (01): : 114 - 117
  • [9] Effect of grain size on tribological behavior of hot-pressed boron carbide sliding against alumina balls
    Zhou, Zhihui
    Xia, Jie
    Wang, Minbo
    Li, Ruidi
    Yuan, Tiechui
    [J]. INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (03) : 2136 - 2150
  • [10] Precipitation of AlN in a commercial hot-pressed boron carbide
    Xie, Kelvin Y.
    Livi, Kenneth
    McCauley, James W.
    Hemker, Kevin J.
    [J]. SCRIPTA MATERIALIA, 2015, 101 : 95 - 98