Effect of Cooling Rate on Microstructure and Effective Grain Size for a Ni–Cr–Mo–B High-Strength Steel

被引:0
|
作者
Shouqing Zhang [1 ,2 ]
Xiaofeng Hu [1 ]
Haichang Jiang [1 ]
Lijian Rong [1 ]
机构
[1] CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research , Chinese Academy of Sciences
[2] School of Materials Science and Engineering , University of Science and Technology of China
关键词
D O I
暂无
中图分类号
TG142.1 [钢的组织与性能];
学科分类号
摘要
The effect of cooling rate on microstructure and effective grain size(EGS) of a Ni-Cr-Mo-B high-strength steel has been studied by dilatometer,field emission scanning electron microscopy(FESEM),transmission electron microscopy(TEM) and electron backscattered diffraction(EBSD).The results show that the microstructure of the Ni-Cr-Mo-B steel is dependent on cooling rate in the following sequence:lath martensite(LM),mixed LM and lath bainite(LB),mixed LB and granular bainite(GB) and GB.The critical cooling rates for appearance of LB and GB are about 10 ℃/s and 0.5 ℃/s,respectively.The LM(> 10 ℃/s) consists of few blocky regions with a width of several micros.Compared with the lath regions,the blocky regions in LM form at higher actual transformation temperatures during cooling.The blocky region area percentage in LM keeps almost constant about 8% at different cooling rates(> 10℃/s) due to similar martensite transformation starting temperature(M).The LB percentage in mixed LM/LB increases gradually with decreasing cooling rate(10-0.5 ℃/s).The EBSD results show that different microstructures have different EGS.The mixed LM/LB exhibits the smallest EGS due to the separation of the prior austenite grains by the pre-formed LB and the refinement of the LM.Meanwhile,the mixed LM/LB at different cooling rates(10-0.5 ℃/s) exhibits almost the same EGS because the LB and LM in the mixed LM/LB have a similar high-angle grain boundary density and similar EGS.Because the blocky regions contain few high-angle grain boundaries and have similar area percentages in the LM,the LM at different cooling rates(> 10 ℃/s) exhibits almost the same EGS.The ferrite in GB exhibits as a whole with few high-angle grain boundaries;thus,the mixed LB/GB exhibits the largest EGS.
引用
收藏
页码:1862 / 1872
页数:11
相关论文
共 50 条
  • [1] Effect of Cooling Rate on Microstructure and Effective Grain Size for a Ni–Cr–Mo–B High-Strength Steel
    Shouqing Zhang
    Xiaofeng Hu
    Haichang Jiang
    Lijian Rong
    Acta Metallurgica Sinica (English Letters), 2022, 35 : 1862 - 1872
  • [2] Effect of Cooling Rate on Microstructure and Effective Grain Size for a Ni-Cr-Mo-B High-Strength Steel
    Zhang, Shouqing
    Hu, Xiaofeng
    Jiang, Haichang
    Rong, Lijian
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2022, 35 (11) : 1862 - 1872
  • [3] Effect of finish cooling temperature on microstructure and mechanical properties of high-strength bainitic steels containing Cr, Mo, and B
    Sung, Hyo Kyung
    Lee, Dong Ho
    Shin, Sang Yong
    Lee, Sunghak
    Yoo, Jang Yong
    Hwang, Byoungchul
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 624 : 14 - 22
  • [4] Effect of Rolling and Heat Treatment Process Tempering on the Microstructure and Mechanical Performance of Cr-Ni-Mo High-Strength Ship Steel
    Meng, Fanxia
    Tian, Yong
    Ye, Qibin
    Wang, Zhaodong
    Wu, Di
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (10)
  • [5] Effect of Thickness Reduction on Residual Stress and Microstructure Inhomogeneity of Radial Forged Ni-Cr-Mo High-Strength Steel Tube
    Xu, Weisheng
    Yang, Jinghan
    Ji, Pengfei
    Lian, Yong
    Zhang, Jin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (06) : 5130 - 5138
  • [6] Effect of Thickness Reduction on Residual Stress and Microstructure Inhomogeneity of Radial Forged Ni-Cr-Mo High-Strength Steel Tube
    Weisheng Xu
    Jinghan Yang
    Pengfei Ji
    Yong Lian
    Jin Zhang
    Journal of Materials Engineering and Performance, 2022, 31 : 5130 - 5138
  • [7] Effect of cooling process on microstructure and properties of Si-Mn-Cr-Ni-Mo ultra high strength steel after rolling
    Heibei Key Laboratory of Modern Metallurgy Technology, North China University of Science and Technology, Tangshan, China
    不详
    Cailiao Rechuli Xuebao, 8 (161-166):
  • [8] Microstructure and Mechanical Properties of Welded Joint of a Fe-Cr-Ni-Mo Steel with High-Strength and High-Toughness
    Hu Xiaofeng
    Jiang Haichang
    Zhao Mingjiu
    Yan Desheng
    Lu Shanping
    Rong Lijian
    ACTA METALLURGICA SINICA, 2018, 54 (01) : 1 - 10
  • [9] Microstructure and Mechanical Properties of Inertia-Friction-Welded Fe-Cr-Ni-Mo High-Strength Steel
    Zai, Le
    You, Guoqiang
    Tong, Xin
    Ding, Yuhan
    Xu, Xuanxi
    Liu, Qing
    STEEL RESEARCH INTERNATIONAL, 2020, 91 (09)
  • [10] EFFECT OF COOLING RATE ON INTERCRITICALLY REHEATED MICROSTRUCTURE AND TOUGHNESS IN HIGH-STRENGTH LOW-ALLOY STEEL
    DAVIS, CL
    KING, JE
    MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (01) : 8 - 15