Experimental investigation on impact performances of GLARE laminates

被引:0
|
作者
Chen Qi [1 ]
Guan Zhidong [1 ]
Li Zengshan [1 ]
Ji Zhaojie [1 ]
Zhuo Yue [1 ]
机构
[1] School of Aeronautic Science and Engineering, Beihang University
关键词
Concentrated quasi-static indentation force; Delamination; GLARE laminate; Impact; Indentation;
D O I
暂无
中图分类号
V257 [金属和非金属复合材料];
学科分类号
0805 ; 080502 ;
摘要
An experimental investigation was carried out on the damage resistance to a concentrated quasi-static indentation force and low-velocity impact of four kinds of glass-reinforced aluminum laminates(GLARE for short). Compared with the experimental results of the CFRP(Carbon Fiber Reinforced Plastics) laminates, the performance of GLARE was determined. By means of concentrated quasi-static indentation force test, typical force–displacement response,the maximum contact force and dent depth were received. Through drop-weight low-velocity impact tests, impact force histories, indentation depths(through a new method) and dissipated energy were obtained. The test results show that the force–displacement response of GLARE 4laminates under the concentrated quasi-static indentation force has an obvious flat roof and the failure is instantaneous, which are different from CFRP laminates. The indention will be visible once the impact happens. C-scan results find that there is no delamination besides the impact area after both the concentrated quasi-static indentation and low-velocity impact. The dissipated energy approximately equals the impact energy.
引用
收藏
页码:1784 / 1792
页数:9
相关论文
共 50 条
  • [1] Experimental investigation on impact performances of GLARE laminates
    Chen Qi
    Guan Zhidong
    Li Zengshan
    Ji Zhaojie
    Zhuo Yue
    [J]. CHINESE JOURNAL OF AERONAUTICS, 2015, 28 (06) : 1784 - 1792
  • [2] Experimental investigation on impact performances of GLARE laminates
    Chen Qi
    Guan Zhidong
    Li Zengshan
    Ji Zhaojie
    Zhuo Yue
    [J]. Chinese Journal of Aeronautics., 2015, 28 (06) - 1792
  • [3] Investigation of blast response of GLARE laminates: comparison against experimental results
    Kotzakolios, T.
    Vlachos, D. E.
    Kostopoulos, V.
    [J]. PLASTICS RUBBER AND COMPOSITES, 2011, 40 (6-7) : 349 - 355
  • [4] Soft impact of GLARE fiber metal laminates
    Li, Kaikai
    Qin, Qinghua
    Cui, Tianning
    Han, Qigang
    Peng, Jixiang
    Sha, Zhendong
    Zhang, Wei
    [J]. International Journal of Impact Engineering, 2023, 178
  • [5] An experimental investigation of the impact response of composite laminates
    Aktas, Mehmet
    Atas, Cesim
    Icten, Buelent Murat
    Karakuzu, Ramazan
    [J]. COMPOSITE STRUCTURES, 2009, 87 (04) : 307 - 313
  • [6] Multiple Impact Damage in GLARE Laminates: Experiments and Simulations
    Lee, Sang-Eui
    Kim, Dong-Uk
    Cho, Yong-Jun
    Seo, Hyoung-Seock
    [J]. MATERIALS, 2021, 14 (24)
  • [7] LOW-ENERGY IMPACT ISSUES IN GLARE LAMINATES
    Bienias, Jaroslaw
    Jakubczak, Patryk
    Surowska, Barbara
    [J]. COMPOSITES THEORY AND PRACTICE, 2013, 13 (03): : 165 - 169
  • [8] Delamination in GLARE laminates under low velocity impact
    Kakati, Sasanka
    Chakraborty, D.
    [J]. COMPOSITE STRUCTURES, 2020, 240
  • [9] Ballistic impact of GLARE™ fiber-metal laminates
    Fatt, MSH
    Lin, CF
    Revilock, DM
    Hopkins, DA
    [J]. COMPOSITE STRUCTURES, 2003, 61 (1-2) : 73 - 88
  • [10] Impact damage tolerance and fatigue durability of GLARE laminates
    Seo, Hyoungseock
    Hahn, H. T.
    Yang, Jenn-Ming
    [J]. JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 2008, 130 (04): : 0410021 - 0410026