Creep Failure Behavior in the Weak Areas of 12Cr1MoV Main Steam Pipe Elbow Utilized in Thermal Power Plants

被引:0
|
作者
Wang, Shutao [1 ]
Shi, Renqiang [1 ]
Wu, Jian [2 ]
Yang, Chao [1 ]
Liu, Huan [2 ]
机构
[1] Jiangsu Frontier Elect Power Technol Co Ltd, Nanjing 211100, Peoples R China
[2] Hohai Univ, Coll Mat Sci & Engn, Changzhou 213200, Peoples R China
关键词
12Cr1MoV steel; main steam pipe; elbow; creep; microstructure; STRESS RUPTURE; PLASTIC-FLOW; ALLOY; EVOLUTION; CARBIDES; STEEL;
D O I
10.3390/ma18040812
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The main steam pipe elbow is a critical metallic component in thermal power plants. Due to prolonged exposure to high temperatures and pressures, it experiences microstructural degradation and creep damage, thereby affecting its service life. Currently, there is debate regarding the location of the weakest region within the elbow, with uncertainty over whether it lies in the inner arc or neutral plane area. This study investigates the microstructure and creep properties of both the inner arc and neutral surface regions of an elbow that has been in operation for 183,088 h, aiming to identify the actual weak region and explore the underlying creep damage mechanisms. The results indicate that under identical temperature and stress conditions, samples from the neutral plane region exhibit significantly higher creep rates and shorter creep rupture times compared to those from the inner arc region. This suggests that the creep life in the vicinity of the inner surface in the neutral plane is markedly lower than that in the inner arc region. Microstructural analysis before and after creep fracture reveals that key factors influencing the creep performance of 12Cr1MoV elbows include carbide size, precipitation amount and distribution, grain size and morphology, as well as the stability and uniformity of grain orientation. Specifically, the growth of intragranular precipitates, the accumulation and non-uniform distribution of grain boundary carbides, and the non-uniform distribution of grain sizes all contribute to the rapid formation of creep cracks and premature material failure. This study concludes that the weakest region in the elbow is located at the inner surfaces of the neutral plane. Future inspections and life assessments of thermal power plant elbows should therefore focus on this area to enhance the accuracy of life evaluations and ensure the safety of thermal power plants.
引用
收藏
页数:19
相关论文
共 15 条
  • [1] Fatigue-creep interaction of 12Cr1MoV main steam pipe
    Chen, Guoliang
    Shu, Guogang
    Zhongguo Dianji Gongcheng Xuebao/Proceedings of the Chinese Society of Electrical Engineering, 1990, 10 (01): : 1 - 10
  • [2] INVESTIGATION OF THE TEMPERATURE-FORCE DEPENDENCE OF THE RATE OF CREEP OF 12CR1MOV STEAM PIPE STEEL
    TRUSOV, LP
    TRUNIN, II
    DOBROVOLSKII, VE
    ROSHCHUPKIN, AD
    THERMAL ENGINEERING, 1981, 28 (11) : 627 - 630
  • [3] Combined creep-fatigue behaviour of a 12Cr1MoV steel used in power plants
    Wang, Xiang
    Kong, Qingping
    Tong, Shihua
    Jiang, Xianmei
    Ren, Weiping
    Jinshu Xuebao/Acta Metallurgica Sinica, 1988, 24 (02):
  • [4] Rupture analysis of 12Cr1MoV super-heater tubes in power plants
    Mohtadi-Bonab, M. A.
    Javaheri, Vahid
    Totonchi-Maleki, F.
    ENGINEERING FAILURE ANALYSIS, 2023, 153
  • [5] Effect of High Temperature Hot Corrosion on the Compression Creep Behavior of 12Cr1MoV Alloys
    He, Jianjun
    Xiong, Weizhou
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2017, 36 (10) : 1011 - 1023
  • [6] INFLUENCE OF THE JOINT EFFECT OF THERMAL FATIGUE AND CREEP ON THE STRUCTURE AND NATURE OF FRACTURE OF 12CR1MOV STEEL
    TULYAKOV, GA
    BEREZINA, TG
    SOKOLYANSKII, BM
    KARASEV, VV
    KENDYSH, VN
    THERMAL ENGINEERING, 1979, 26 (10) : 571 - 572
  • [7] Aging behavior descriptions for main steam pipes made of 12Cr1MoV and 15CrMo steels by Larson-Miller parameter
    Yang, Rui-Cheng
    Wang, Hui
    Yang, Hai-Tang
    Chen, Kui
    Yuan, Xiao-Bo
    Cailiao Kexue yu Gongyi/Material Science and Technology, 2002, 10 (04): : 395 - 398
  • [8] Study on Tensile Creep Behavior of 12Cr1MoV Alloy Steel under High-Temperature Alkali Metal Salt Environment for Solar Thermal Power Generation
    He, Jianjun
    Yang, Kaijun
    Wang, Gang
    Li, Wei
    Bao, Jiangyong
    Chen, Jian
    INTERNATIONAL JOURNAL OF PHOTOENERGY, 2020, 2020
  • [9] FEATURES OF THE STRUCTURE AND NATURE OF FAILURE OF BENDS OF 12CR1MOV STEEL STEAMLINES WHEN WORKING UNDER CREEP CONDITIONS
    BEREZINA, TG
    ASHIKHMINA, LA
    THERMAL ENGINEERING, 1981, 28 (10) : 606 - 609
  • [10] Effect of repair welding on the creep behavior of a 12Cr1MoV/GTR-2CM/P91 dissimilar joint
    Zhao, Y. P.
    Gong, J. M.
    Jiang, Y.
    Li, Q. N.
    Wang, X. W.
    PRESSURE VESSEL TECHNOLOGY: PREPARING FOR THE FUTURE, 2015, 130 : 509 - 516