Initiation and propagation mechanism of fatigue crack in ultra-thick titanium alloy vacuum electron beam welding joint

被引:0
|
作者
Long, Jian [1 ]
Zhang, Lin-Jie [1 ]
Liu, Yong-Qiang [2 ,3 ]
Deng, De-An [2 ]
Zhuang, Ming-Xiang [3 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
[2] Chongqing Univ, Sch Mat Sci & Engn, Chongqing 400044, Peoples R China
[3] AVIC Xian Aircraft Ind Grp Co Ltd, Xian 710089, Peoples R China
关键词
Electron beam welding; High-cycle fatigue; Thick-walled titanium alloy; Microstructures; Fatigue cracks; MICROSTRUCTURES; PLATES;
D O I
10.1016/j.engfailanal.2024.108534
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The investigation delved into the fatigue properties across various layers of joints in a 130-mmthick Ti6Al4V- damage tolerance titanium alloy, which had been fabricated through vacuum electron beam welding. Microstructures in welds are inhomogeneous along the thickness direction of joints. The fatigue properties of various layers of joints exhibit minimal differences, with the fatigue limit consistently exceeding 90 % of the base metal. The cracks always initiate on the sample surface, with numerous fatigue striations present on all fractures. Additionally, many dimples are observed in all fracture zones. The fatigue crack propagation mechanism is depicted as a series connection of micro-pores. Micro-pores are formed by inward pitting of material surfaces and nucleate in local plastic deformation zones of the material. Stress concentration of microstructures is an important cause for formation of local plastic deformation zones. After high cycle fatigue experiments, martensite lath-shaped alpha ' phase in microstructures in the weld is broken and the broken alpha ' phase pins the dislocations, resulting in microscopic stress concentration.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Stress corrosion crack sensitivity of ultra-thick TC4 titanium alloy electron beam welding joints
    Fang W.
    Xiao T.
    Zhang Y.
    Xu W.
    Yi Y.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 121 - 128
  • [2] Non-uniformity of fracture toughness of ultra-thick titanium alloy double-sided electron beam welding joint
    Long, Jian
    Zhang, Lin-Jie
    Liu, Yong-Qiang
    Deng, De-An
    Zhuang, Ming-Xiang
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 : 5115 - 5123
  • [3] Fatigue crack growth of titanium alloy joints by electron beam welding
    Qi, Hong-Yu
    Shi, Hao
    Li, Shao-Lin
    Yang, Xiao-Guang
    RARE METALS, 2014, 33 (05) : 516 - 521
  • [4] Fatigue crack growth of titanium alloy joints by electron beam welding
    Hong-Yu Qi
    Hao Shi
    Shao-Lin Li
    Xiao-Guang Yang
    Rare Metals, 2014, 33 (05) : 516 - 521
  • [5] Fatigue crack growth of titanium alloy joints by electron beam welding
    Hong-Yu Qi
    Hao Shi
    Shao-Lin Li
    Xiao-Guang Yang
    Rare Metals, 2014, 33 : 516 - 521
  • [6] Mechanism of fatigue crack initiation and propagation in commercially pure titanium and titanium alloy with bimodal harmonic structure
    Kikuchi S.
    Nakai Y.
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2019, 66 (02): : 97 - 102
  • [7] Study on crack generation mechanism of GH4251 vacuum electron beam welding joint
    Ma, Jincan
    Wang, Houqin
    Wang, Xiaobing
    Li, He
    Zhang, Binggang
    VACUUM, 2025, 233
  • [8] Simulation of Fatigue Crack Initiation of Electron Beam Welding Joint Based on Tanaka-Mura Model
    Liu, Xiao-Gang
    Zhu, Yang-Yang
    Shen, Shun
    Peng, Wei-Ping
    Tuijin Jishu/Journal of Propulsion Technology, 2022, 43 (02): : 98 - 106
  • [9] Initiation and propagation behaviors of small fatigue crack in titanium alloy TC4
    Zhu L.
    Hu X.T.
    Jiang R.
    Song Y.D.
    Qu S.D.
    Key Engineering Materials, 2019, 795 : 9 - 14
  • [10] SOME ASPECTS OF VARIABILITY IN FATIGUE CRACK INITIATION AND PROPAGATION IN THICK ALUMINUM-ALLOY SECTIONS
    MANN, JY
    PELL, RA
    MACHIN, AS
    INTERNATIONAL JOURNAL OF FATIGUE, 1986, 8 (02) : 59 - 66