Influence of Waste Magnesite Particle Reinforcement on the Mechanical, Corrosive and Wear Behaviour of 6061 Aluminium Composites

被引:1
|
作者
Saminathan, Matheshwaran [1 ]
Ayyappan, Solaiyappan [2 ]
机构
[1] Annapoorana Engn Coll, Dept Mech Engn, Salem 636308, Tamil Nadu, India
[2] Govt Coll Technol, Dept Mech Engn, Coimbatore 641013, Tamil Nadu, India
来源
CHIANG MAI JOURNAL OF SCIENCE | 2024年 / 51卷 / 03期
关键词
aluminium; 6061; alloy; waste magnesite (WM); stir casting method; mechanical properties; wear behaviour; electrochemical corrosion; METAL-MATRIX COMPOSITES; STIRRING SPEED; MICROSTRUCTURE; TIME;
D O I
10.12982/CMJS.2024.037
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
In this study, waste magnesite (WM) particles with different weight fractions (2.5%, 5%, and 7.5%) were used as particulate material in 6061 aluminium alloy to produce composites with improved properties. The composite material was manufactured using a stir-casting method. A surface morphology investigation confirms the uniform distribution and good interfacial bonding of the WM particles within the alloy base. The addition of 5% WM particles was found to improve the values of tensile strength of 146.68 MPa, hardness of 131.6 HV and coefficient of friction of 0.565. Incorporating 7.5% WM was found to give a low wear of 161 mu m and a corrosion current of 8.5 x 10(-6) A. The results obtained confirm that such a proportion of WM particles in Al 6061 alloy provides excellent anticorrosion protection, wear properties, and good mechanical properties. Adding 5% WM to Al 6061 improves overall performance characteristics among other ratios.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Effect of TiN particulate reinforcement on corrosive behaviour of aluminium 6061 composites in chloride medium
    Murthy, H. C. Ananda
    Raju, V. Bheema
    Shivakumara, C.
    BULLETIN OF MATERIALS SCIENCE, 2013, 36 (06) : 1057 - 1066
  • [2] Effect of TiN particulate reinforcement on corrosive behaviour of aluminium 6061 composites in chloride medium
    H C ANANDA MURTHY
    V BHEEMA RAJU
    C SHIVAKUMARA
    Bulletin of Materials Science, 2013, 36 : 1057 - 1066
  • [3] Investigation on mechanical and tribological properties of magnesite reinforced aluminium 6061 composites
    Ayyappan, S.
    Saminathan, M.
    Selvarasan, R.
    MATERIALS RESEARCH EXPRESS, 2022, 9 (07)
  • [4] Influence of single and multiple particle size variation on mechanical and wear behaviour of aluminium silicon carbide composites
    Adebisi, A. A.
    Maleque, M. A.
    Ali, M. Y.
    Bello, K. A.
    PROCEEDINGS OF MALAYSIAN INTERNATIONAL TRIBOLOGY CONFERENCE 2015, 2015, : 139 - 141
  • [5] Effect of reinforcement on wear behaviour of aluminium hybrid composites
    Radhika, N.
    Subramanian, R.
    TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2013, 7 (01) : 36 - 41
  • [6] Effect of particulate reinforcement on wear behaviour of aluminium matrix composites
    Korkut, MH
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (01) : 73 - 81
  • [7] Study of corrosive-erosive wear behaviour of Al6061/albite composites
    Sharma, S. C.
    Krishna, M.
    Murthy, H. N. Narasimha
    Tarachandra, R.
    Satyamoorthy, M.
    Bhattacharyya, D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 425 (1-2): : 305 - 311
  • [8] Wear behaviour on ceramic particle reinforced aluminium matrix composites
    Busquets-Mataix, D
    Martínez, N
    Amigó, V
    Salvador, MD
    Ferrer, C
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2004, 43 (02): : 299 - 303
  • [9] Mechanical and wear behaviour of aluminium metal matrix hybrid composites
    Kumar, Siddesh N. G.
    Ravindranath, V. M.
    Shankar, G. S. Shiva
    INTERNATIONAL CONFERENCE ON ADVANCES IN MANUFACTURING AND MATERIALS ENGINEERING (ICAMME 2014), 2014, 5 : 908 - 917
  • [10] Solutionizing Effects during Corrosive Wear in 6061 Aluminum and Composites
    Varma S.K.
    Andrews S.
    Journal of Materials Engineering and Performance, 1997, 7 (1) : 33 - 47