Effect of solid solution of magnesia-alumina spinel on the microstructure and mechanical properties of CAC-bonded corundum castables

被引:0
|
作者
Zhao, Yaning [1 ]
Zhang, Zhongzhuang [1 ]
Hou, Qiqi [1 ]
Zeng, Jinyan [1 ]
Mu, Yuandong [1 ,3 ]
He, Jian [2 ]
Ye, Guotian [1 ]
Tian, Jiajia [1 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Henan Key Lab High Temp Funct Ceram, Zhengzhou 450001, Peoples R China
[2] Jiangsu Jingxin New Mat Co Ltd, Yangzhou 225000, Peoples R China
[3] China Construct Seventh Engn Div Corp Ltd, Zhengzhou 450004, Peoples R China
基金
中国国家自然科学基金;
关键词
Solid solution; Magnesia-alumina spinel; Corundum castables; Microstructure; Mechanical properties; REFRACTORY CASTABLES; HYDRATION KINETICS; MGAL2O4; SPINEL; CEMENT; DIFFUSION;
D O I
10.1016/j.ceramint.2024.12.410
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Magnesia-alumina spinel undergoes a solid solution reaction during firing, which potentially impact the microstructure as well as the mechanical properties of the CAC-bonded corundum castables. Moreover, spinels possessing the same chemical composition yet produced via different methods may exhibit diverse solid solution behaviors. Consequently, this study firstly compares the solid solution behaviors of sintered and fused spinel powders, both of which have an identical alumina content of 72 wt%, and then investigates the effect of solid solution on the microstructure and mechanical properties of CAC-bonded corundum castables. The results indicate that both sintered and fused spinel powders experience solid solution reactions during the firing process, leading to the formation of spinel-calcium hexaluminate (CA6) connection structures. This transformation alters the fracture behavior from intergranular to transgranular mode, thereby enhancing the mechanical properties of castables. When the spinel content is 10 wt%, the cold crushing strength of the castables containing sintered spinel reaches 235.9 MPa, which is 28.6 % higher than that of the castables without spinel. The spinel-CA6 connection structures increase with the elevation of the spinel content. Additionally, due to its smaller grain size, sintered spinel undergoes higher degree of solid solution reaction, forming tighter connection structures, which contributes to the improvement of the overall mechanical properties.
引用
收藏
页码:9791 / 9799
页数:9
相关论文
共 50 条
  • [1] The effect of the alumina-rich spinel exsolution on the microstructure of CAC-bonded castables
    Zhang, Zhongzhuang
    Hou, Qiqi
    Zhao, Yaning
    Zeng, Jinyan
    Mu, Yuandong
    He, Jian
    Luo, Zhongtao
    Ye, Guotian
    CERAMICS INTERNATIONAL, 2024, 50 (24) : 53396 - 53406
  • [2] Microstructure and properties of MgAlON-bonded magnesia, magnesia-alumina spinel and corundum materials
    Cheng, Zhu
    Sun, Jia-Lin
    Wu, Xue-Zhen
    Chen, Zhao-You
    Wang, Jin-Xiang
    Wan, Long-Gang
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2011, 33 (11): : 1378 - 1386
  • [3] Microstructure evolution during the heating process and its effect on the elastic properties of CAC-bonded alumina castables
    Wang, Yulong
    Li, Xiangcheng
    Zhu, Boquan
    Chen, Pingan
    CERAMICS INTERNATIONAL, 2016, 42 (09) : 11355 - 11362
  • [4] Effect of magnesium aluminum hydrotalcite on the properties of CAC-bonded castables
    Zhao, Zongqiang
    Zhou, Wenying
    Guo, Liu
    Ma, Junhua
    Jia, Quanli
    Zhai, Pengtao
    Li, Jianwei
    Chen, Liugang
    CERAMICS INTERNATIONAL, 2023, 49 (03) : 5382 - 5390
  • [5] Effect of curing temperature on volume stability of CAC-bonded alumina based castables
    Li, Ye
    Zhu, Lingling
    Liu, Kun
    Ding, Dafei
    Zhang, Ju
    Ye, Guotian
    CERAMICS INTERNATIONAL, 2019, 45 (09) : 12066 - 12071
  • [6] The microstructure and some properties of magnesia-alumina spinel materials with sialon matrix
    Czechowski, J.
    Czechowska, K.
    Wala, T.
    Podworny, J.
    INDUSTRIAL CERAMICS, 2010, 30 (02): : 105 - 112
  • [7] Mechanical property and phase evolution of the hydrates of CAC-bonded alumina castables during drying at 110 °C
    Li, Na
    Wang, Xiaoyu
    Mu, Yuandong
    Zhang, Ronghui
    Zhu, Lingling
    Ye, Guotian
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 266
  • [8] Effect of pH slurries on chemical mechanical polishing for magnesia-alumina spinel
    School of Mechanical and Power Engineering, Henan Polytechnic University, Jiaozuo
    454003, China
    不详
    453003, China
    不详
    100013, China
    Hongwai yu Jiguang Gongcheng Infrared Laser Eng., 1600,
  • [9] Optimized microstructure with nano-alumina and its effects on properties of corundum spinel castables
    Zhu, Hui
    Li, Xiangcheng
    Chen, Pingan
    Zhu, Boquan
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2019, 16 (06) : 2362 - 2372
  • [10] Regulation of Pore Structure and High-temperature Fracture Behavior of CAC-bonded Alumina-Spinel Castables Based on Hydration Design
    Wenjing LIU
    Ning LIAO
    Yawei LI
    China's Refractories, 2024, 33 (03) : 22 - 29