Oxidation behavior of several Ti-Al alloys at 900°C in air

被引:0
|
作者
Schmitz-Niederau, M. [1 ]
Schütze, M. [2 ]
机构
[1] Lurgi Ol Gas Chemie GmbH, D-60295 Frankfurt/Main, Germany
[2] Karl-Winnacker-Inst. der D., D-60061 Frankfurt/Main, Germany
来源
Oxidation of Metals | 1999年 / 52卷 / 03期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:225 / 240
相关论文
共 50 条
  • [1] The oxidation behavior of several Ti-Al alloys at 900°C in air
    Schmitz-Niederau, M
    Schütze, M
    OXIDATION OF METALS, 1999, 52 (3-4): : 225 - 240
  • [2] The Oxidation Behavior of Several Ti-Al Alloys at 900°C in Air
    M. Schmitz-Niederau
    M. Schutze
    Oxidation of Metals, 1999, 52 : 225 - 240
  • [3] OXIDATION OF TI-AL ALLOYS
    KAHVECI, AI
    WELSCH, G
    WASIELEWSKI, GE
    JOURNAL OF METALS, 1988, 40 (07): : A49 - A49
  • [4] OXIDATION OF TI-AL ALLOYS
    KAHVECI, AI
    LIU, Z
    WELSCH, G
    WASIELEWSKI, G
    JOURNAL OF METALS, 1987, 39 (07): : A7 - A7
  • [5] Cracking and healing of oxide scales on Ti-Al alloys at 900°C
    Lurgi Ol Gas Chemie GmbH, D-60295 Frankfurt/Main, Germany
    不详
    Oxid Met, 3 (241-276):
  • [6] Cracking and healing of oxide scales on Ti-Al alloys at 900°C
    Schmitz-Niederau, M
    Schütze, M
    OXIDATION OF METALS, 1999, 52 (3-4): : 241 - 276
  • [7] Cracking and Healing of Oxide Scales on Ti-Al Alloys at 900°C
    Martin Schmitz-Niederau
    Michael Schutze
    Oxidation of Metals, 1999, 52 : 241 - 276
  • [8] OXIDATION BEHAVIOR OF BINARY TI-AL ALLOYS IN HIGH-TEMPERATURE AIR ENVIRONMENT
    SHIDA, Y
    ANADA, H
    MATERIALS TRANSACTIONS JIM, 1993, 34 (03): : 236 - 242
  • [9] The nitriding behavior of Ti-Al alloys at 1000 °C
    J. Magnan
    G. C. Weatherly
    M. -C. Cheynet
    Metallurgical and Materials Transactions A, 1999, 30 : 19 - 29
  • [10] The nitriding behavior of Ti-Al alloys at 1000 °C
    Magnan, J
    Weatherly, GC
    Cheynet, MC
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (01): : 19 - 29