Structural State Stability of Superlightweight MA21 Magnesium-lithium Alloy.

被引:0
|
作者
Koryagin, Yu.D.
Il'in, S.I.
机构
关键词
METALLOGRAPHY; -; Microstructures;
D O I
暂无
中图分类号
学科分类号
摘要
The instability of the structural state and mechanical properties of MA21 alloy occurring after prolonged storage or at high temperatures is caused mainly by a transition of the metastable theta phase to the equilibrium AlLi phase, and also by the dissolution and coagulation of dispersed hardening phases (MgLi//2Al and AlLi). To obtain an optimal combination of properties, heating of MA21 alloy prior to quenching and deformation should be carried out at temperatures no lower than 350 degree C, while the maximum temperature of subsequent agings or process heatings should not exceed 100 degree C with the minimum possible holding (1 to 3 hours).
引用
收藏
页码:94 / 97
相关论文
共 50 条
  • [1] INCREASING THE CORROSION RESISTANCE OF MA21 MAGNESIUM-LITHIUM ALLOY BY SURFACE LASER TREATMENT.
    Kalimullin, R.Kh.
    Berdnikov, A.T.
    Protection of Metals (English translation of Zaschita Metallov), 1986, 22 (02): : 223 - 225
  • [2] INCREASING THE CORROSION-RESISTANCE OF MA21 MAGNESIUM-LITHIUM ALLOY BY SURFACE LASER TREATMENT
    KALIMULLIN, RK
    BERDNIKOV, AT
    PROTECTION OF METALS, 1986, 22 (02): : 223 - 225
  • [3] THE EFFECT OF SURFACE LASER TREATMENT ON THE CREEP OF THE MAGNESIUM LITHIUM ALLOY MA21
    KALIMULLIN, RK
    VALUEV, VV
    BERDNIKOV, AT
    METAL SCIENCE AND HEAT TREATMENT, 1986, 28 (9-10) : 668 - 670
  • [4] EFFECT OF SURFACE LASER TREATMENT ON THE CREEP OF THE MAGNESIUM-LITHIUM ALLOY MA21.
    Kalimullin, R.Kh.
    Valuev, V.V.
    Berdnikov, A.T.
    Metal Science and Heat Treatment (English Translation of Metallovedenie i Termicheskaya Obrabotka, 1986, 28 (9-10): : 668 - 670
  • [5] The kinetics of phosphate film formation on the type MA 21 magnesium-lithium alloys
    L. A. Isaicheva
    N. M. Trepak
    L. K. Il’ina
    A. L. L’vov
    Protection of Metals, 2006, 42 : 389 - 393
  • [6] The kinetics of phosphate film formation on the type MA 21 magnesium-lithium alloys
    Isaicheva, L. A.
    Trepak, N. M.
    Il'ina, L. K.
    L'vov, A. L.
    PROTECTION OF METALS, 2006, 42 (04): : 389 - 393
  • [7] PROPERTIES OF ALLOY MA21 AFTER LASER TREATMENT
    KALIMULLIN, RK
    SPIRIDONOV, VB
    BERDNIKOV, AT
    ROMANOV, AA
    PAUTKINA, GN
    METAL SCIENCE AND HEAT TREATMENT, 1988, 30 (5-6) : 338 - 348
  • [8] Black anodizing of a magnesium-lithium alloy
    Thermal Systems Group, Bangalore, India
    Met Finish, 4 (7pp):
  • [9] Performance of a magnesium-lithium alloy as an anode for magnesium batteries
    Sivashanmugam, A
    Kumar, TP
    Renganathan, NG
    Gopukumar, S
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2004, 34 (11) : 1135 - 1139
  • [10] Performance of a magnesium-lithium alloy as an anode for magnesium batteries
    Sivashanmugam, A.
    Kumar, T. Prem
    Renganathan, N.G.
    Gopukumar, S.
    Journal of Applied Electrochemistry, 2004, 34 (11): : 1135 - 1139