Improvement of the Properties of Mild Steel for Hot Strip.

被引:0
|
作者
Lang, Cestmir [1 ]
Stich, Guenter [1 ]
Meyer, Lutz [1 ]
机构
[1] Thyssen Stahl AG, Duisburg, West Ger, Thyssen Stahl AG, Duisburg, West Ger
来源
Stahl und Eisen | 1986年 / 106卷 / 03期
关键词
STEEL - Cold Working;
D O I
暂无
中图分类号
学科分类号
摘要
The mechanical properties and ageing resistance of StW 24 hot strip steel depend to a large extent on the degree of fixation of the dissolved nitrogen. At coiling temperatures below 650 degree C, only a small fraction of nitrogen is precipitated as aluminiumnitride and the hot strip features a relatively low ageing resistance. Coiling temperatures higher than 720 degree C result actually in an improved properties after ageing, however, the dispersion of the mechanical properties over the strip length increases also. A stable fixation of nitrogen independently of the coiling temperature is ensured by stoichiometric addition of titanium relation to the nitrogen content. This results in improved cold deformability, ageing stability and consistency of the properties.
引用
收藏
页码:68 / 74
相关论文
共 50 条
  • [1] Continuous Hot Pickling of Wide Steel Strip.
    Wuttke, Rudolf
    Baender Bleche Rohre, 1982, 23 (01): : 5 - 6
  • [2] HEAT TRANSFER DURING HOT ROLLING OF STEEL STRIP.
    Devadas, C.
    Samarasekera, I.V.
    Ironmaking and Steelmaking, 1986, 13 (06): : 311 - 321
  • [3] FLATNESS AND PROFILE CONTROL IN HOT AND COLD ROLLING OF STEEL STRIP.
    Yarita, Ikuo
    Kitamura, Kunio
    Kataoka, Kenji
    Nakagawa, Kichizaemon
    Kawasaki Steel Technical Report, 1980, (01): : 60 - 69
  • [4] MONITORING THE MECHANICAL PROPERTIES OF LONGERON HOT-ROLLED 30T STEEL STRIP.
    Mel'gui, M.A.
    Ivanov, F.D.
    Shidlovskaya, E.A.
    Matyuk, V.F.
    Merkalov, V.A.
    The Soviet journal of nondestructive testing, 1980, 16 (06): : 415 - 418
  • [5] Continuous Hardening of Steel Strip.
    Dedek, Vladimir
    Hutnicke Listy, 1973, 28 (01): : 31 - 39
  • [6] Study of the Brittleness of 3% Si Hot-Rolled Steel Strip.
    Pirvu, Gh.
    Miron, V.
    Ionescu, Florentina
    Gheorghisor, G.
    Florea, Al.
    Samoilesicu, S.
    Galati, C.S.
    1600, (37):
  • [7] CONTINUOUS ANNEALING OF STEEL STRIP.
    Pitt, Rodney
    Steel Times, 1986, 214 (01): : 28 - 40
  • [8] IMPROVEMENT OF THE PROPERTIES OF LOW-CARBON STEEL HOT WIDE STRIP
    LANG, C
    STICH, G
    MEYER, L
    STAHL UND EISEN, 1986, 106 (03): : 122 - 128
  • [9] IMPROVEMENT IN MECHANICAL PROPERTIES OF STEEL STRIP IN CONTINUOUS HOT ROLLING.
    ZHELEZNOV, YU.D.
    GRIGORYAN, G.G.
    SHATALOV, R.L.
    ALDUNIN, A.V.
    RASSOMAKHIN, G.V.
    1981, V 11 (N 7): : 416 - 418
  • [10] Surface Cracks in Hot Rolled, Low-Carbon Rimmed Steel Strip.
    Pereira, Luiz Carlos
    Mahtuk, Jorge Orlando
    Pereira, Carlos Alberto
    Bukalil, Roberto Hid
    De Faria Barros, Antonio Lafayette
    Metalurgia ABM, 1985, 41 (326): : 9 - 14