Quasi-industrial Testing of Cooling Lubricants for Steel Wire Drawing.

被引:0
|
作者
Boor, Udo
机构
来源
Stahl und Eisen | 1982年 / 102卷 / 01期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Pretreated wire rod containing 0. 45-0. 5% C has been drawn in six steps from 5. 5 to 2 mm diameter. The drawing speed ranged between 1 and 12 m/sec. The friction coefficient/average surface pressure curve is the assessment criterion for a drawing lubricant.
引用
收藏
页码:13 / 18
相关论文
共 31 条
  • [1] QUASI-INDUSTRIAL TESTING OF COOLING LUBRICANTS FOR STEEL WIRE TESTING
    BOOR, U
    STAHL UND EISEN, 1982, 102 (01): : 29 - 34
  • [2] TESTING OF VARIOUS MATERIALS FOR THE PRODUCTION OF DIES FOR STEEL WIRE DRAWING.
    Felder, E.
    le Floc'H, A.
    Wire Industry, 1979, 46 (551): : 817 - 820
  • [3] Lime-Bearing Lubricants Improve Wire Drawing.
    Plasek, Bohumil
    Tittel, Viktor
    Drahtwelt Wurzburg, 1986, 72 (09): : 210 - 211
  • [4] Lubricants for steel wire drawing
    Anon
    Wire Industry, 1991, 58 (695): : 695 - 698
  • [5] LOW-MELTING GLASS LUBRICANTS FOR WARM WIRE DRAWING.
    Kopp, Reiner
    Maraite, Klaus-Dietmar
    Wireworld international, 1987, 29 (06): : 132 - 134
  • [6] Contributions to the Improvement of Hard Steel Wire Drawing.
    Plesia, I.
    Metalurgia Bucuresti, 1985, 37 (12): : 649 - 652
  • [7] METHODS FOR TESTING WIRE DRAWING LUBRICANTS
    KOPP, R
    PEHLE, HJ
    STAHL UND EISEN, 1984, 104 (05): : 241 - 244
  • [8] REDUCTION OF WEAR OF WIRE ROPES - QUASI-INDUSTRIAL INVESTIGATIONS ON IRON AND STEEL WORKS CRANES
    KRAUSE, H
    NEUMANN, P
    STAHL UND EISEN, 1980, 100 (01): : 1 - 4
  • [9] Potential Danger from Machinery in Steel Wire Drawing.
    Konodyba-Szymanski, Bogumil
    Drahtwelt Wurzburg, 1986, 72 (04): : 89 - 91
  • [10] NEW COOLING SYSTEM FOR HIGH-SPEED WIRE DRAWING.
    Nakamura, Y.
    Kawakami, H.
    Fujita, T.
    Yamada, Y.
    1600, (09):