Study of the influence of mischmetal additions to Al-7Si-0.3Mg (LM 25/356) alloy

被引:0
|
作者
Regional Research Lab , Trivandrum, India [1 ]
机构
来源
关键词
Addition reactions - Chemical modification - Electric conductivity - Eutectics - Fracture toughness - Magnesium - Mechanical properties - Metallographic microstructure - Metals - Silicon - Strontium;
D O I
暂无
中图分类号
学科分类号
摘要
This article deals with the effect of 0.25-1.5 wt pct mischmetal (MM) addition on the mechanical properties, microstructure, electrical conductivity, and fracture behavior of cast Al-7Si-0.3Mg (LM 25/356) alloy. Modification of eutectic silicon by MM is compared with strontium modification in terms of microstructure, mechanical properties, and fading behavior. Loss of magnesium encountered on holding the molten alloy and its resultant effect on mechanical properties of alloys modified with MM and Sr are compared with those in the unmodified alloy.
引用
收藏
相关论文
共 50 条
  • [1] A study of the influence of mischmetal additions to Al-7Si-0.3Mg (LM 25/356) alloy
    Ravi, M
    Pillai, UTS
    Pai, BC
    Damodaran, AD
    Dwarakadasa, ES
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (05): : 1283 - 1292
  • [2] Inhibition of delayed ageing by trace additions in Al-7Si-0.3Mg Cast alloy
    Murali, S.
    Kashyap, K.T.
    Raman, K.S.
    Murthy, K.S.S.
    [J]. Scripta Metallurgica et Materialia, 1993, 29 (11): : 1421 - 1426
  • [3] The effect of Sn additions on the semi-solid microstructure of an Al-7Si-0.3Mg alloy
    Kliauga, AM
    Ferrante, M
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 337 (1-2): : 67 - 72
  • [4] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Pandee, Phromphong
    Gourlay, C. M.
    Belyakov, S. A.
    Ozaki, Ryota
    Yasuda, Hideyuki
    Limmaneevichitr, Chaowalit
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (10): : 4549 - 4560
  • [5] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Phromphong Pandee
    C. M. Gourlay
    S. A. Belyakov
    Ryota Ozaki
    Hideyuki Yasuda
    Chaowalit Limmaneevichitr
    [J]. Metallurgical and Materials Transactions A, 2014, 45 : 4549 - 4560
  • [6] Sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of copper at elevated temperature
    Kori, S. A.
    Prabhudev, M. S.
    [J]. WEAR, 2011, 271 (5-6) : 680 - 688
  • [7] Impression creep characterization of cast Al-7Si-0.3Mg alloy
    Rashno, S.
    Ranjbar, Khalil
    Reihanian, M.
    [J]. MATERIALS RESEARCH EXPRESS, 2019, 6 (08)
  • [8] Rheological Behavior of Al-7Si-0.3Mg Alloy at Mushy State
    Prosenjit Das
    Sudip K. Samanta
    Pradip Dutta
    [J]. Metallurgical and Materials Transactions B, 2015, 46 : 1302 - 1313
  • [9] Microscale deformation behavior of rheocast Al-7Si-0.3Mg alloy
    Das, Prosenjit
    Islam, Sk Tanbir
    Samanta, Sudip K.
    Das, Santanu
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2016, 230 (06) : 1041 - 1061
  • [10] Rheological Behavior of Al-7Si-0.3Mg Alloy at Mushy State
    Das, Prosenjit
    Samanta, Sudip K.
    Dutta, Pradip
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2015, 46 (03): : 1302 - 1313