Fatigue life and fracture assessment of SA 333 Gr. 6 carbon steel straight pipes with circumferential crack

被引:0
|
作者
Ramachandra Murthy, A. [1 ]
Vishnuvardhan, S. [1 ]
Saravanan, M. [1 ]
Kumar, Abhishek [1 ]
Gandhi, P. [1 ]
Singh, P.K. [2 ]
机构
[1] CSIR-Structural Engineering Research Centre, CSIR Campus, Taramani, Chennai,600 113, India
[2] Reactor Safety Division, Bhabha Atomic Research Centre, Mumbai,400 085, India
来源
关键词
Circumferential cracks - Collapse conditions - Crack growth life - Cracked pipe - Fatigue life assessment - Plastic collapse - Remaining life - Residual strength - Straight pipe - Stress-intensity factors;
D O I
暂无
中图分类号
学科分类号
摘要
It is known that damage tolerant evaluation has primarily two objectives, namely, crack growth life and residual strength. In the present study, remaining life and residual strength evaluation of SA 333 Gr. 6 carbon steel straight pipes with circumferential part through crack under cyclic loading has been carried out. The study involves evaluation of accurate crack driving force, i.e., Stress Intensity Factor (SIF), crack growth and remaining life of cracked pipe. SIF has been evaluated for the cracked pipes using French RCC-MR and R6 approaches. Crack growth life has been evaluated using Paris law. The predicted crack growth life has been compared with the previous experimental results and found to be close to each other with maximum difference of 13%. Residual strength has been determined by using (i) plastic collapse condition with yield stress and flow stress (ii) fracture toughness criterion and (iii) remaining life approach. The residual strength obtained using plastic collapse condition with yield stress is lower compared to other approaches. The predicted remaining life and residual strength are useful for safe operation of power plant structures based on fitness for purpose requirements. © 2023, Structural Engineering Research Centre. All rights reserved.
引用
收藏
页码:215 / 225
相关论文
共 21 条
  • [1] Fatigue Crack Growth and Fracture Studies on Stainless Steel Straight Pipes Having Circumferential Surface Crack
    Saravanan, M.
    Vishnuvardhan, S.
    Murthy, A. Ramachandra
    Gandhi, P.
    Mandal, Debasish
    Singh, P. K.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2024, 24 (03) : 1166 - 1180
  • [2] Influence of Geometrical Variables on Initiation Fracture Toughness (JIC) of Low Carbon High Manganese SA 333 Gr. 6 Steel
    Bansal, Sandeep
    Nath, S. K.
    Ghosh, P. K.
    Ray, S.
    ISIJ INTERNATIONAL, 2009, 49 (08) : 1253 - 1258
  • [3] Fatigue crack growth and fracture studies on straight pipes with circumferential surface notch
    Structural Engineering Research Centre, Council of Scientific, Industrial Research Campus, Chennai-600 113, India
    不详
    J Struct Eng, 2008, 5 (374-379):
  • [4] Influence of uniaxial ratchetting on low cycle fatigue behviour of SA 333 Gr. 6 C-Mn steel
    Sivaprasad, S.
    Paul, Surajit Kumar
    Gupta, Suneel Kumar
    Bhasin, Vivek
    Narasaiah, N.
    Tarafder, S.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2010, 87 (08) : 464 - 469
  • [5] Cyclic plastic deformation behavior in SA333 Gr. 6 C-Mn steel
    Paul, Surajit Kumar
    Sivaprasad, S.
    Dhar, S.
    Tarafder, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (24): : 7341 - 7349
  • [6] Evaluating a valid fracture specimen geometry for predicting geometry independent SZWc and JS']JSZW value in SA333 Gr. 6 carbon steel material
    Saxena, Sanjeev
    Dutta, B. K.
    Sasikala, G.
    ENGINEERING FRACTURE MECHANICS, 2015, 143 : 108 - 120
  • [7] Ratcheting and stress relaxation of SA333 Gr. 6 carbon steel samples under uniaxial multistep strain-controlled condition
    Das, P.
    Khutia, N.
    Dey, P. P.
    Arora, Punit
    Gupta, Suneel K.
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2021, 43 (06)
  • [8] Acoustic emission during fracture toughness tests of SA333 Gr.6 steel
    Mukhopadhyay, C. K.
    Sasikala, G.
    Jayakumar, T.
    Raj, Baldev
    ENGINEERING FRACTURE MECHANICS, 2012, 96 : 294 - 306
  • [9] Multi-objective cyclic plastic modelling of cyclic hardening and softening characteristics of nuclear piping SA333 gr. 6 carbon steel
    Das, P.
    Khutia, N.
    Dey, P. P.
    Arora, Punit
    Gupta, Suneel. K.
    INTERNATIONAL JOURNAL OF FATIGUE, 2024, 180
  • [10] Fracture studies on carbon steel straight pipes having off-centred circumferential through-wall crack under finite compliance
    Saravanan, M.
    Vishnuvardhan, S.
    Gandhi, P.
    Raghava, G.
    Khan, I. A.
    Bhasin, V
    Chattopadhyay, J.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2020, 182