Study on microstructure of heavily drawn pearlite steel wire

被引:0
|
作者
Tu, Yi-You
Jiang, Jian-Qing
Cai, Lei
Bian, Jian-Chun
机构
[1] Jiangsu Key Laboratory for Advanced Metallic Materials, Southeast University, Nanjing 211189 Fasten Group, Jiangyin 214433, China
[2] Fasten Group, Jiangyin 214433, China
来源
Kang T'ieh/Iron and Steel (Peking) | 2008年 / 43卷 / 07期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:72 / 75
相关论文
共 50 条
  • [1] Cementite decomposition in heavily drawn pearlite steel wire
    Hono, K
    Ohnuma, M
    Murayama, M
    Nishida, S
    Yoshie, A
    Takahashi, T
    SCRIPTA MATERIALIA, 2001, 44 (06) : 977 - 983
  • [2] Comment on "Cementite decomposition in heavily drawn pearlite steel wire"
    Gavriljuk, V
    SCRIPTA MATERIALIA, 2002, 46 (02) : 175 - 177
  • [3] A modified pearlite microstructure to overcome the strength-plasticity trade-off of heavily drawn pearlitic wire
    Zhou, Lichu
    Fang, Feng
    Kumagai, Masayoshi
    Pickering, Ed
    Zhang, Xiaodan
    SCRIPTA MATERIALIA, 2022, 206
  • [4] Strength anisotropy and residual stress in drawn pearlite steel wire
    Suzuki, T
    Tomota, Y
    Isaka, M
    Moriai, A
    Minakawa, N
    Morii, Y
    ISIJ INTERNATIONAL, 2004, 44 (08) : 1426 - 1430
  • [5] Structure and mechanical behavior of heavily drawn pearlite and martensite in a high carbon steel
    Shiota, Y
    Tomota, Y
    Moriai, A
    Kamiyama, T
    METALS AND MATERIALS INTERNATIONAL, 2005, 11 (05) : 371 - 376
  • [6] Structure and mechanical behavior of heavily drawn pearlite and martensite in a high carbon steel
    Y. Shiota
    Y. Tomota
    A. Moriai
    T. Kamiyama
    Metals and Materials International, 2005, 11 : 371 - 376
  • [7] Mechanical and thermal stability of heavily drawn pearlitic steel wire
    Aernoudt, E
    Sevillano, JG
    Delrue, H
    VanHumbeeck, J
    Watte, P
    Lefever, I
    LAYERED MATERIALS FOR STRUCTURAL APPLICATIONS, 1996, 434 : 119 - 126
  • [8] Effect of hydrogen on ductility and toughness in heavily drawn steel wire
    Kawabe, Nozomu
    Murai, Teruyuki
    Wire Journal International, 1999, 32 (08): : 82 - 90
  • [9] Evolution of strength and microstructure during annealing of heavily cold-drawn 6.3 GPa hypereutectoid pearlitic steel wire
    Li, Y. J.
    Choi, P.
    Goto, S.
    Borchers, C.
    Raabe, D.
    Kirchheim, R.
    ACTA MATERIALIA, 2012, 60 (09) : 4005 - 4016
  • [10] Atom probe tomography characterization of heavily cold drawn pearlitic steel wire
    Li, Y. J.
    Choi, P.
    Borchers, C.
    Chen, Y. Z.
    Goto, S.
    Raabe, D.
    Kirchheim, R.
    ULTRAMICROSCOPY, 2011, 111 (06) : 628 - 632