The behavior of Sn whisker growth on Sn-0.7Cu-0.05Ni solder joint during thermal cycling

被引:0
|
作者
Hashim, Aimi Noorliyana [1 ,2 ]
Mohd Salleh, Mohd Arif Anuar [1 ,2 ]
Ramli, Muhammad Mahyiddin [3 ]
Al Bakri Abdullah, Mohd Mustafa [1 ,2 ]
Sandu, Andrei Victor [4 ,5 ,6 ]
Vizureanu, Petrica [4 ,7 ,8 ]
机构
[1] Univ Malaysia Perlis, Fac Chem Engn & Technol, Arau 02600, Perlis, Malaysia
[2] Univ Malaysia Perlis, Ctr Excellence Geopolymer & Green Technol, Arau 02600, Perlis, Malaysia
[3] Univ Malaysia Perlis, Sch Microelect Engn, Pauh Putra Campus, Arau 02600, Perlis, Malaysia
[4] Gheorghe Asachi Tech Univ Lasi, Fac Mat Sci & Engn, Blvd D Mangeron 71, Iasi 700050, Romania
[5] Romanian Inventors Forum, Str Sf P Movila 3, Iasi 700089, Romania
[6] Natl Inst Res & Dev Environm Protect INCDPM, Splaiul Independentei 294, Bucharest 060031, Romania
[7] Acad Romanian Scientists, 54 Splaiul Independentei St,Sect 5, Bucharest 050094, Romania
[8] Tech Sci Acad Romania, Dacia Blvd 26, Bucharest 030167, Romania
关键词
PHASE-STABILITY; TIN WHISKERS; EVOLUTION; NI; EXPANSION; MECHANISM; CU6SN5;
D O I
10.1007/s10854-024-13805-9
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The present study investigates the behavior of Sn whisker growth on Sn-0.7Cu-0.05Ni solder joints during thermal cycling conducted for 1500 cycles at temperature of - 40 (+ 0/- 10) degrees C and + 85 (+ 10/- 0) degrees C through industry standard practices JESD22-A121A established by the Joint Electron Device Engineering Council (JEDEC). Results determine that the growth rate of Sn whisker on the Sn-0.7Cu-0.05Ni solder joint was slower than the Sn-0.7Cu solder joint and consequently show that the 0.05% addition of Ni is able to suppress the growth of Sn whisker during thermal cycling. Furthermore, the stabilization of hexagonal eta-Cu6Sn5 of (Cu,Ni)6Sn5 IMC interfacial layer in Sn-0.7Cu-0.05Ni solder joints significantly contributes to a lower coefficient of thermal expansion (CTE) compared to Cu6Sn5 IMC interfacial layer, thereby reducing thermal mismatch stress for Sn whisker growth on the Sn0.7Cu0.05Ni solder joint. The implications of this study are substantial for effective approach to mitigate Sn whiskers growth through consistent inspection protocols and adherence to industry standard practices.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Effect of Isothermal Annealing on Sn Whisker Growth Behavior of Sn0.7Cu0.05Ni Solder Joint
    Hashim, Aimi Noorliyana
    Salleh, Mohd Arif Anuar Mohd
    Ramli, Muhammad Mahyiddin
    Abdullah, Mohd Mustafa Al Bakri
    Sandu, Andrei Victor
    Vizureanu, Petrica
    Sandu, Ioan Gabriel
    MATERIALS, 2023, 16 (05)
  • [2] Interfacial microstructure and properties of Sn-0.7Cu-0.05Ni/Cu solder joint with rare earth Nd addition
    Zeng, Guang
    Xue, Songbai
    Gao, Lili
    Zhang, Liang
    Hu, Yuhua
    Lai, Zhongmin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (25) : 7152 - 7161
  • [3] Relationship between free solder thickness to the solderability of Sn-0.7Cu-0.05Ni solder coating during soldering
    Ramli, M. I. I.
    Salleh, M. A. A. Mohd
    Sobri, F. A. Mohd
    Narayanan, P.
    Sweatman, K.
    Nogita, K.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (04) : 3669 - 3677
  • [4] Stabilisation of Cu6Sn5 by Ni in Sn-0.7Cu-0.05Ni lead-free solder alloys
    Nogita, Kazuhiro
    INTERMETALLICS, 2010, 18 (01) : 145 - 149
  • [5] Effect of Ni on the Suppression of Sn Whisker Formation in Sn-0.7Cu Solder Joint
    Hashim, Aimi Noorliyana
    Salleh, Mohd Arif Anuar Mohd
    Sandu, Andrei Victor
    Ramli, Muhammad Mahyiddin
    Yee, Khor Chu
    Mohd Mokhtar, Noor Zaimah
    Chaiprapa, Jitrin
    MATERIALS, 2021, 14 (04) : 1 - 15
  • [6] Effect of Zinc Additions on Sn-0.7Cu-0.05Ni Lead-Free Solder Alloy
    Saleh, N. A.
    Ramli, M. I. I.
    Salleh, M. A. A. Mohd
    JOINING AND WELDING SYMPOSIUM, 2017, 238
  • [7] Properties and microstructure of Sn-0.7Cu-0.05Ni solder bearing rare earth element Pr
    Zeng, Guang
    Xue, Songbai
    Zhang, Liang
    Gao, Lili
    Lai, Zhongmin
    Luo, Jiadong
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2011, 22 (08) : 1101 - 1108
  • [8] Effects of phosphorus on microstructure and fluidity of Sn-0.7Cu-0.05Ni lead-free solder
    Nogita, K.
    Gourlay, C. M.
    Read, J.
    Nishimura, T.
    Suenaga, S.
    Dahle, A. K.
    MATERIALS TRANSACTIONS, 2008, 49 (03) : 443 - 448
  • [9] Influence of Ni on the refinement and twinning of primary Cu6Sn5 in Sn-0.7Cu-0.05Ni
    Xian, J. W.
    Salleh, M. A. A. Mohd
    Belyakov, S. A.
    Su, T. C.
    Zeng, G.
    Nogita, K.
    Yasuda, H.
    Gourlay, C. M.
    INTERMETALLICS, 2018, 102 : 34 - 45
  • [10] Interfacial IMC Layer and Tensile Properties of Ni-Reinforced Cu/Sn-0.7Cu-0.05Ni/Cu Solder Joint: Effect of Aging Temperature
    Yang, Li
    Ge, Jinguo
    Zhang, Yaocheng
    Dai, Jun
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (09) : 2429 - 2439