Long-term High Temperature Aging on the Microstructure of T23 Water-cooled Wall Welds Influences

被引:0
|
作者
Yin, Shaohua [1 ,2 ]
Zhang, Zhenhua [3 ]
Sun, Zhiqiang [1 ]
Luo, Zhen [2 ]
机构
[1] Suzhou Nuclear Power Research Institute Co., Ltd., Suzhou,215004, China
[2] School of Materials Science and Engineering, Tianjin University, Tianjin,300350, China
[3] CHN Energy Xuzhou Power Co., Ltd., Xuzhou,221166, China
关键词
D O I
10.3901/JME.2024.12.277
中图分类号
学科分类号
摘要
Grain boundaries
引用
收藏
页码:277 / 286
相关论文
共 50 条
  • [1] Effect of long term high temperature aging on CGHAZ microstructure of T23 water wall welded joint
    Hanjie Xuebao/Transactions of the China Welding Institution, 2024, 45 (01): : 109 - 115
  • [2] Microstructure and mechanical properties of the T23 steel after long-term ageing at elevated temperature
    Zielinski, A.
    Golanski, G.
    Sroka, M.
    Skupien, P.
    MATERIALS AT HIGH TEMPERATURES, 2016, 33 (02) : 154 - 163
  • [3] High Temperature Corrosion of Water Wall Materials T23 and T24 in Simulated Furnace Atmospheres
    Zhao Qinxin
    Zhang Zhixiang
    Cheng Dingnan
    Wang Yungang
    Deng Xiang
    CHINESE JOURNAL OF CHEMICAL ENGINEERING, 2012, 20 (04) : 814 - 822
  • [4] Effect of long-term aging on the microstructure and mechanical properties of T23 steel weld metal without post-weld heat treatment
    Wang, Xue
    Li, Yong
    Li, Huijun
    Lin, Sanbao
    Ren, Yaoyao
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 252 : 618 - 627
  • [5] Influence of long-term aging at elevated temperature on welds with carbon migration
    Li, Kejian
    Cai, Zhipeng
    Li, Yifei
    Hu, Mengjia
    Pan, Jiluan
    Qinghua Daxue Xuebao/Journal of Tsinghua University, 2015, 55 (10): : 1051 - 1055
  • [6] Investigation on high temperature corrosion of water-cooled wall tubes at a 300 MW boiler
    Xiong, Xiaohe
    Liu, Xing
    Tan, Houzhang
    Deng, Shuanghui
    JOURNAL OF THE ENERGY INSTITUTE, 2020, 93 (01) : 377 - 386
  • [7] High-temperature corrosion prediction model of water-cooled wall for boiler peak regulation
    Deng L.
    Yuan M.
    Yang J.
    Yue Y.
    Jiang J.
    Che D.
    Che, Defu (dfche@xjtu.edu.cn), 1600, Chemical Industry Press Co., Ltd. (43): : 925 - 936
  • [8] Experimental study on high temperature gaseous hydrogen fluoride corrosion of boiler water-cooled wall pipes
    Zhang, Jigang
    Liu, Zijun
    Cheng, Kun
    Jia, Lianqin
    Han, Kuihua
    ENVIRONMENTAL TECHNOLOGY, 2024,
  • [9] Pulverized coal combustion technology for resistance to water-cooled wall high temperature corrosion and industrial experimental study
    Zhang, Ze
    Wu, Shaohua
    Yao, Zheng
    Chen, Lizhe
    Zhu, Qunyi
    Qin, Yukun
    Dongli Gongcheng/Power Engineering, 1999, 19 (05): : 353 - 356
  • [10] LONG-TERM ECONOMIC IMPORTANCE OF GAS-COOLED HIGH TEMPERATURE REACTORS
    KRAMER, H
    SCHULTEN, R
    WAGEMANN, K
    NUKLEONIK, 1968, 11 (01): : 44 - &