Evaluation of 3-Point and 4-Point Bending Tests for Tensile Strength Assessment of GFRP Bars

被引:1
|
作者
Lochan, Philip Prakash [1 ]
Polak, Maria Anna [1 ]
机构
[1] Univ Waterloo, Dept Civil & Environm Engn, 200 Univ Ave West, West Waterloo, ON N2L 3G1, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
glass fiber reinforced polymer bars; tensile strength; modulus of rupture; testing; 3-point bending; 4-point bending; Weibull weakest link model;
D O I
10.3390/ma17215261
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Glass Fiber Reinforced Polymer (GFRP) bars are used as reinforcement for structural concrete, especially in cases where corrosion of traditional steel reinforcement is a problem. The tensile strength of these reinforcing bars is the primary characteristic on which the design of concrete members reinforced with GFRP bars relies. Determination of the tensile strength of the bars using a direct tensile test is a time and resource-intensive task and therefore is not routinely conducted for quality control. The tensile strength can also be measured from flexure tests, which are much simpler than direct tensile tests, and use appropriate correlation formulations. In this paper, the applicability of flexure testing for the identification of bars' tensile strength is investigated by conducting and analyzing both 3-point and 4-point flexure testing. The correlation formulations are presented that allow the determination of tensile strength from the modulus of rupture. The Weibull weakest link model and the assumption of the same flaw distribution in tensile and flexure tests is adopted. The results of the 3-point and the 4-point bending are presented and compared. Comparisons are also conducted to select direct tensile test results. The work shows that 3-point and 4-point bending tests provide very similar results, with the difference between the results being 2% to 10%, suggesting both tests can be used for tensile strength determination of GFRP bars.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Comparison of 3-point and 4-point bending tests for the determination of the residual flexural strength
    Weber, Fabian
    Anders, Steffen
    BETON- UND STAHLBETONBAU, 2021, 116 : 48 - 58
  • [2] BRITTLE RING TEST - A COMPARISON WITH THE 3-POINT AND 4-POINT BENDING TESTS
    FREY, T
    GROZ, K
    HOLLER, J
    ZEHM, K
    CFI-CERAMIC FORUM INTERNATIONAL, 1995, 72 (06): : 333 - 337
  • [3] Stress distribution in a 4-point or 3-point bending probe
    Meyer-Piening, HR
    MECHANICS OF SANDWICH STRUCTURES, 1998, : 105 - 112
  • [4] Effects of adherends’ misalignment on the strength of single-lap joints under 3-point and 4-point bending tests
    Andrea Corrado
    Wilma Polini
    The International Journal of Advanced Manufacturing Technology, 2022, 123 : 3819 - 3829
  • [5] Effects of adherends' misalignment on the strength of single-lap joints under 3-point and 4-point bending tests
    Corrado, Andrea
    Polini, Wilma
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 123 (11-12): : 3819 - 3829
  • [6] STRAIN RATES FOR 3-POINT AND 4-POINT FLEXURE TESTS
    LAND, PL
    JOURNAL OF MATERIALS SCIENCE, 1979, 14 (11) : 2760 - 2761
  • [7] FRACTOGRAPHY OF BOROSILICATE GLASS TESTED IN 3-POINT AND 4-POINT BENDING
    DIELHOF, MH
    DORTMANS, LJMG
    DEWITH, G
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1993, 12 (03) : 215 - 220
  • [8] AN APPROACH TO THE EVALUATION OF 3-POINT AND 4-POINT LADDER DIAGRAMS
    USSYUKINA, NI
    DAVYDYCHEV, AI
    PHYSICS LETTERS B, 1993, 298 (3-4) : 363 - 370
  • [9] FAILURE MECHANISMS IN 3-POINT AND 4-POINT SHORT BEAM BENDING TESTS OF UNIDIRECTIONAL GLASS EPOXY
    CUI, WC
    WISNOM, MR
    JONES, M
    JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 1992, 27 (04): : 235 - 243
  • [10] STRENGTH TESTS OF FLAT GLASS BY MEANS OF 4-POINT BENDING
    BLANK, K
    DURKOP, D
    DURCHHOLZ, M
    GRUTERS, H
    HELMICH, G
    SENGER, W
    GLASTECHNISCHE BERICHTE-GLASS SCIENCE AND TECHNOLOGY, 1994, 67 (01): : 9 - 15