Improvement of gradient microstructure and properties of wire-arc directed energy deposition titanium alloy via laser shock peening

被引:12
|
作者
Qu, Guanda [1 ]
Guo, Wei [1 ]
Shi, Jiaxin [1 ]
He, Dongsheng [2 ]
Zhang, Yongxin [1 ]
Dong, Yihao [1 ,3 ]
Chi, Jiaxuan [4 ]
Shen, Zhikang [5 ]
Li, Ying [6 ]
Chen, Zhenlin [6 ]
Zhang, Hongqiang [1 ]
机构
[1] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
[2] Tsinghua Univ, Dept Mech Engn, Beijing 100084, Peoples R China
[3] China Univ Min & Technol, Sch Mech & Elect Engn, Beijing 100083, Peoples R China
[4] Beihang Univ, Sch Mat Sci & Engn, Beijing 100191, Peoples R China
[5] Southwest Univ, Coll Engn & Technol, Chongqing 400715, Peoples R China
[6] AECC Shenyang Liming Aeroengine Co Ltd, Shenyang 110043, Peoples R China
基金
中国国家自然科学基金;
关键词
Titanium alloy; Wire-arc directed energy deposition; Laser shock peening; Gradient structure; Fatigue life; GRAIN-REFINEMENT; RESIDUAL-STRESS; FATIGUE; MECHANISM; EVOLUTION; ORIGIN;
D O I
10.1016/j.msea.2024.147422
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Wire-arc directed energy deposition (WADED) technology has been widely used in the remanufacturing of titanium alloy structural components benefited from with the advantages such as high deposition efficiency and low cost. However, due to the coarse and anisotropic microstructure, the complex internal stresses and processing-induced rough surface significantly reduce fatigue performance and reliability of the remanufactured structural components. In this work, surface modification of titanium alloy WADED repair component was carried out via laser shock peening (LSP), and its gradient structure, microhardness, residual stress and fatigue performance and enhancement mechanism were systematically investigated. Results indicated that the different microstructure of each region led to different responses under the action of LSP, which was related to the change of dislocation density. LSP induced crystal defects such as high-density dislocations, twins and stacking faults on the surface. A variety of crystal defects gradually decreased with the depth from the strengthened surface, formed a gradient microstructure and significantly affected the microhardness and residual stress of the repaired components. The surface hardness and compressive residual stress of the repaired components were greatly increased after LSP and the hardened layer and compressive residual stress depth affected layer were 600 mu m and 800 mu m, respectively. The average fatigue life of the additive repair component increased by 197 % under the synergistic effect of compressive residual stress and gradient microstructure.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Gradient microstructure and prominent performance of wire-arc directed energy deposited magnesium alloy via laser shock peening
    Li, Xinzhi
    Fang, Xuewei
    Zhang, Mugong
    Zhang, Hongkai
    Duan, Yusong
    Huang, Ke
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2023, 188
  • [2] Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening
    Sun, Rujian
    Li, Liuhe
    Zhu, Ying
    Guo, Wei
    Peng, Peng
    Cong, Baoqiang
    Sun, Jianfei
    Che, Zhigang
    Li, Bo
    Guo, Chao
    Liu, Lei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 747 : 255 - 265
  • [3] Crack suppression in wire-arc directed energy deposition of a γ-TiAl alloy
    Wu, Dongsheng
    Xin, Jianwen
    Li, Fang
    Shen, Chen
    Wang, Lin
    Hua, Xueming
    Lei, Hu
    Ma, Ninshu
    JOURNAL OF MANUFACTURING PROCESSES, 2023, 107 : 155 - 165
  • [4] Effect of Laser Shock Peening on Microstructure and Residual Stress of Wire-Arc Additive Manufactured 2319 Aluminum Alloy
    Sun Rujian
    Zhu Ying
    Li Liuhe
    Guo Wei
    Peng Peng
    LASER & OPTOELECTRONICS PROGRESS, 2018, 55 (01)
  • [5] Simultaneous strength and ductility enhancement of wire-arc directed energy deposited Al-Cu alloy by interlayer laser shock peening
    Jing, Yandong
    Fang, Xuewei
    Geng, Yongliang
    Duan, Yusong
    Huang, Ke
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 887
  • [6] Tailoring interface properties in wire-arc directed energy deposited dissimilar aluminum alloys through interlayer laser shock peening
    Chang, Tianxing
    Zhang, Huwei
    Fang, Xuewei
    Ma, Minghua
    Zheng, Senmu
    Lu, Bingheng
    Huang, Ke
    VIRTUAL AND PHYSICAL PROTOTYPING, 2025, 20 (01)
  • [7] Recent progress in wire-arc and wire-laser directed energy deposition (DED) of titanium and aluminium alloys
    Nagalingam, Arun Prasanth
    Shamir, Muhammad
    Tureyen, Erkan Bugra
    Sharman, Adrian Richard Charles
    Poyraz, Ozgur
    Yasa, Evren
    Hughes, James
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2025, 136 (5-6): : 2035 - 2073
  • [8] Wire-arc directed energy deposition of magnesium alloys: microstructure, properties and quality optimization strategies
    Yi, Hao
    Wang, Qiao
    Cao, Huajun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 20 : 627 - 649
  • [9] Wire-Arc Directed Energy Deposition of Aluminum Alloy 7075 With Dispersed Nanoparticles
    Chi, Yitian
    Pan, Shauihang
    Liese, Maximillian
    Liu, Jingke
    Murali, Narayanan
    Soemardy, Ebryanto
    Li, Xiaochun
    JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2023, 145 (03):
  • [10] Microstructure and Mechanical Properties of an Advanced Ag-Microalloyed Aluminum Crossover Alloy Tailored for Wire-Arc Directed Energy Deposition
    Thomas Klein
    Aurel Arnoldt
    Manuel Gomes
    Pere Barriobero-Vila
    JOM, 2023, 75 : 4128 - 4137