Study on the material flow behavior, microstructure evolution and strengthening mechanism of arc-assisted friction stir weld of Ti6321 alloy

被引:1
|
作者
Sun, Guangda [1 ,2 ]
Zhou, Li [1 ,2 ]
Li, Yuxuan [2 ]
Yan, Zhongxian [2 ]
Song, Xiaoguo [1 ,2 ]
Gao, Fuyang [3 ]
Liu, Xiangqian [3 ]
Liao, Zhiqian [3 ]
机构
[1] Harbin Inst Technol, State Key Lab Precis Welding & Joining Mat & Struc, Harbin 150001, Peoples R China
[2] Harbin Inst Technol Weihai, Shandong Prov Key Lab Special Welding Technol, Weihai 264209, Peoples R China
[3] Luoyang Ship Mat Res Inst, Luoyang 471000, Peoples R China
关键词
Ti6321; alloy; Arc assisted friction stir welding; Defect suppression; Microstructural evolution; Failure mechanism; TITANIUM-ALLOY; ALPHA-TITANIUM; JOINT; TRANSFORMATION; DEFORMATION; STRESS; PHASE; ZONE;
D O I
10.1016/j.msea.2024.147455
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, 6 mm thick Ti6321 alloy plates were butt welded using conventional friction stir welding (FSW) and arc-assisted friction stir welding (AAFSW). The defect formation and suppression, microstructure evolution, and plastic deformation and failure mechanisms of the joints were systematically studied. The results showed that a defect-free joint could be achieved with a significant reduction of 50 % in both axial and forward forces for AAFSW. The formation of the bottom defect was attributed to the non-convergence of vertical flow components and the circumferential flow along the pin. The applied arc enhances the material flow along the thickness direction, thereby promoting the transformation of the microstructure at the bottom of the stir zone (SZ) from a bimodal structure to a fully lamellar structure. Texture analysis reveals a shift from B and Y2 to C1 components with increased heat input and strain. Plastic deformation in the SZ is primarily dominated by slip, accompanied by twinning deformation in both joints. And the mechanism involving dislocation decomposition and stacking fault formation leading to dynamic phase transformations has been further confirmed. The AAFSW joint exhibits a more uniform hardness distribution and higher joint efficiency (96 %) with an average ultimate tensile strength (UTS) of 771 MPa and an elongation of 7.8 %. The joint failure mechanism is influenced by microhardness and uncoordinated plastic deformation arising from dislocation slip and twinning effects along the thickness. These insights confirm that AAFSW is a new choice for achieving efficient and high-quality connections in medium- thick Ti alloys.
引用
收藏
页数:19
相关论文
共 30 条
  • [1] Microstructure evolution of friction stir welding of Ti6321 titanium alloy based on the weld temperature below microstructure transformation temperature
    Gao, Fuyang
    Guo, Yufan
    Yu, Wei
    Jiang, Peng
    Liao, Zhiqian
    MATERIALS CHARACTERIZATION, 2021, 177
  • [2] Mechanism Study on Microstructure and Properties of Ti6321 Alloy Welding by Transverse Magnetic Field
    Ding, Laifa
    Zhang, Zheng
    Zeng, Zhibin
    Qin, Binhao
    Vladyslav, Khaskin
    Chen, Lijia
    Zhang, Yupeng
    Wang, Haiyan
    METALS AND MATERIALS INTERNATIONAL, 2025,
  • [3] Material flow and microstructure evolution on the flow path of friction stir lap welded aluminium alloy
    Han, Yang
    Jiang, Xiaoqing
    Yuan, Tao
    Chen, Shujun
    Gong, Wentao
    Li, Xiaoxu
    Yu, Zhanliang
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2023, 28 (01) : 72 - 80
  • [4] Microstructure Evolution and Strengthening Mechanism of the Probeless Friction Stir Spot Welding of a Al-Li Alloy
    Chu Q.
    Yang X.
    Li W.
    Fan W.
    Zou Y.
    Hao S.
    Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2024, 60 (02): : 150 - 158
  • [5] Additive friction stir deposition of Al-Ce alloy:Microstructure evolution, strengthening and fracture mechanism
    Hu, Jinbing
    He, Wenjie
    Wan, Yuting
    Qi, Liang
    Chen, Jiqiang
    Guo, Xunzhong
    Ye, Jieyun
    Zhao, Hongjin
    Liang, Xiaoxia
    Lv, Wancheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1017
  • [6] Assessment of Corrosion and Macrostructural Behavior of Ti6321/SS 310 Butt Joints: In Situ Study of Similar and Dissimilar Joints via Friction Stir Welding Technique
    Sujith, K. Sai
    Ravi, S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [7] Recrystallization behavior and strengthening mechanism of friction stir welded T-joint of Ti80 titanium alloy
    Su, Yu
    Yang, Xiawei
    Zhao, Wenwei
    Gao, Fuyang
    Ma, Shitong
    Meng, Tingxi
    Yin, Shuo
    Li, Wenya
    MATERIALS CHARACTERIZATION, 2024, 216
  • [8] Material Flow and Microstructure Evolution in Corner Friction Stir Welding of 5083 Al Alloy Using AdStir Technique
    Masaki, Kunitaka
    Saito, Hiroshi
    Nezaki, Koji
    Kitamoto, Shoko
    Sato, Yutaka S.
    Kokawa, Hiroyuki
    FRICTION STIR WELDING AND PROCESSING X, 2019, : 181 - 188
  • [9] A study of material flow behavior in thickness direction in friction stir welding of 7075 alloy plate
    Guo, Zhenghua
    Liu, Wenlong
    Li, Chengzhong
    Cui, Junhua
    Zhao, Gangyao
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING, PTS 1-3, 2013, 652-654 : 2315 - 2319
  • [10] Evolution of microstructure and properties in 2219 aluminum alloy produced by wire arc additive manufacturing assisted by interlayer friction stir processing
    Wei, Jingxun
    He, Changshu
    Zhao, Yan
    Qie, Mofan
    Qin, Gaowu
    Zuo, Liang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 868