Superior mechanical properties and corrosion resistance of laser powder bed fusion 7075 Al/TC4 alloy through microstructure design

被引:1
|
作者
Yu, Zhenglei [1 ,2 ]
Zhang, Jian [1 ,2 ,3 ]
Liu, Xin [1 ]
Mao, Chunling [4 ]
Li, Panpan [1 ,2 ,3 ]
Wang, Qingyang [1 ,2 ]
Yang, Kongyuan [1 ,6 ]
Chi, Haojie [1 ,2 ,3 ]
Xu, Zezhou [1 ,2 ,3 ]
Cheng, Fei [5 ]
Guo, Yunting [7 ]
Xu, Yingchao [8 ]
Ren, Luquan [1 ,2 ]
机构
[1] Jilin Univ, Natl Key Lab Automot Chassis Integrat & Bion, Changchun 130022, Peoples R China
[2] Jilin Univ, Key Lab Bion Engn, Minist Educ, Changchun 130022, Peoples R China
[3] Jilin Univ, Weihai Inst Bion, Weihai 264402, Peoples R China
[4] Changchun Vocat Inst Technol, Changchun 130000, Peoples R China
[5] Jilin Univ, Sch Mech & Aerosp Engn, Changchun 130022, Peoples R China
[6] Changchun Univ Sci & Technol, Changchun 130022, Peoples R China
[7] Northeast Forestry Univ, Coll Mech & Elect Engn, Harbin 150042, Peoples R China
[8] China FAW Grp Co Ltd, Natl Key Lab Adv Vehicle Integrat & Control, Changchun 130013, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
Additive manufacturing; 7075 Al alloy; Grain refinement; Mechanical property; Corrosion resisting property; GRAIN-REFINEMENT; MAGNESIUM ALLOY; AL-ALLOYS; ALUMINUM; BEHAVIOR; SIZE; STRENGTH;
D O I
10.1016/j.jmrt.2024.10.170
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 7075 Al alloy fabricated using laser powder bed fusion (L-PBF) technology exhibits coarse columnar grains and significant thermal cracking, which hinders it from meeting mechanical and corrosion resistance standards. In this study, 2 wt% micron-sized the Ti6Al4V (TC4) powder was mechanically mixed into 7075 Al alloy powder, resulting in the fabrication of an Al alloy characterized by fine equiaxed grains through the L-PBF process. The resulting alloy sample exhibited no cracks, with an average grain size of 2.016 nm. During solidification, Al3Ti cubic particles formed in situ, serving as heterogeneous nucleation sites, while the Ti element, which possesses a high growth limiting factor (Q value), further facilitates the heterogeneous nucleation of grains. The mechanical properties of the alloy were significantly improved, achieving an ultimate tensile strength of 369.204 MPa and an elongation at break of 9.371%, which is more than nine times greater than that of the L-PBF 7075 Al alloy. Furthermore, the corrosion current density decreased from 9.096E-06 to 2.089E-06, indicating a marked enhancement in the alloy's corrosion resistance. This method has the potential to be applied to the L-PBF of other low-weldability, high-strength Al alloys, thereby laying the groundwork for expanding the industrial applications of L-PBF.
引用
收藏
页码:4884 / 4898
页数:15
相关论文
共 50 条
  • [1] Structure design of porous TC4 alloy with excellent mechanical properties prepared by laser-powder bed fusion
    Zhang, Lei
    Li, Fei
    Yang, Yujie
    Li, Zonghao
    Li, Zhenhua
    He, Zhenyuan
    Jiang, Yehua
    VACUUM, 2024, 220
  • [2] Microstructure evolution and corrosion mechanism of in situ synthesized TiC/TC4 alloy nanocomposites fabricated by laser powder bed fusion
    Bai, Peikang
    Huo, Pengcheng
    Zhao, Zhanyong
    Du, Wenbo
    Zhang, Zhen
    Wang, Liqing
    CERAMICS INTERNATIONAL, 2023, 49 (02) : 2752 - 2764
  • [3] Microstructure and Mechanical Properties of Laser Repaired TC4 Titanium Alloy
    Zhao Zhuang
    Chen Jing
    Tan Hua
    Zhao Xiaolin
    Huang Weidong
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (07) : 1792 - 1797
  • [4] Microstructure, mechanical properties, aging behavior, and corrosion resistance of a laser powder bed fusion fabricated Al-Zn-Mg-Cu-Ta alloy
    Li, Xinwei
    Li, Dawang
    Li, Gan
    Cai, Qizhou
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 832
  • [5] In situ design of ultrafine-grained 7075 Al alloy with laser powder bed fusion
    He, Xi
    Li, Gan
    Huang, Yuhe
    Huang, Zhun
    Wang, Tao
    Li, Xinggang
    Zhu, Qiang
    MATERIALS LETTERS, 2023, 344
  • [6] Influence of Powder Bed Temperature on the Microstructure and Mechanical Properties of Ti-6Al-4V Alloy Fabricated via Laser Powder Bed Fusion
    Xing, Lei-Lei
    Zhang, Wen-Jing
    Zhao, Cong-Cong
    Gao, Wen-Qiang
    Shen, Zhi-Jian
    Liu, Wei
    MATERIALS, 2021, 14 (09)
  • [7] Microstructure and Corrosion Resistance of Ti6Al4V Manufactured by Laser Powder Bed Fusion
    Luo, Yiwa
    Wang, Mingyong
    Zhu, Jun
    Tu, Jiguo
    Jiao, Shuqiang
    METALS, 2023, 13 (03)
  • [8] Effect of Ni on microstructure and mechanical properties of Al-Mg-Si alloy for laser powder bed fusion
    Luo, Yi-mou
    Wang, Jian-ying
    Wen, Tao
    Yang, Fei-peng
    Zhu, Meng-zhen
    He, Na
    Zheng, Jian-ming
    Shan, Ling
    Yang, Hai-lin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2024, 34 (11) : 3521 - 3535
  • [9] Microstructure and mechanical properties of a hypereutectic Al-Si-Cu alloy manufactured by laser powder bed fusion
    Bobel, Andrew
    Kim, Yoojin
    Casalena, Lee
    Maddalena, Roger
    Sachdev, Anil K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 901
  • [10] Laser powder bed fusion of Al-Mg-Zr alloy: Microstructure, mechanical properties and dynamic precipitation
    Xu, Rong
    Li, Ruidi
    Yuan, Tiechui
    Zhu, Hongbin
    Wang, Minbo
    Li, Jinfeng
    Zhang, Wen
    Cao, Peng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 859