Investigation of Precipitation Behavior of a Novel Ni-Fe-Based Superalloy during High-Temperature Aging Treatment

被引:1
|
作者
Cheng, Jun [1 ]
Li, Kejian [1 ]
Yang, Zhengang [1 ]
Huo, Xin [2 ]
Fan, Manjie [2 ]
Li, Songlin [2 ]
Li, Shengzhi [2 ]
Liu, Qu [1 ]
Ma, Qingxian [1 ]
Cai, Zhipeng [1 ]
机构
[1] Tsinghua Univ, Dept Mech Engn, Beijing 100084, Peoples R China
[2] Shanghai Elect Power Generat Equipment Co Ltd, Shanghai Turbine Plant, Shanghai 200240, Peoples R China
基金
国家重点研发计划;
关键词
Ni-Fe-based superalloy; advanced ultra-supercritical; high-temperature aging treatment; precipitation behavior; grain boundary migration; MICROSTRUCTURAL EVOLUTION; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; INCONEL; 740H; ALLOY; CREEP; DEFORMATION; STABILITY; BOUNDARY; CARBIDE;
D O I
10.3390/ma17194875
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The precipitation behavior of a novel Ni-Fe-based superalloy developed for advanced ultra-supercritical (A-USC) coal-fired power plant applications during high-temperature aging treatment was investigated. The results showed that the major precipitates in the novel alloy were randomly distributed MC carbides, M23C6 carbides at grain boundaries, and the gamma '-Ni3 (Al, Ti) phase in grain interiors after aging. MC remained relatively stable during both short-term and long-term aging. M23C6 quickly precipitated and exhibited a discrete distribution at grain boundaries during short-term aging, and partly developed into continuous films during long-term aging. After uniform precipitation, the shape of gamma ' remained spherical, and the size kept increasing with aging time according to the Lifshitz-Slyozov-Wagner (LSW) model. The hardness of the novel alloy was mainly associated with the precipitation behavior of gamma '; as gamma ' gradually precipitated, the hardness steadily increased; after complete precipitation, as the size of gamma ' increased, the hardness first increased and then decreased, reaching the peak hardness when the average radius of gamma ' achieved the critical size. In addition, the novel alloy exhibited abnormal coarsening behavior at grain boundaries during both short-term and long-term aging. The coarsened grain boundaries were actually precipitate-free zones (PFZs) and the coarsened and elongated rod-like particles inside were identified as gamma ' precipitates. The mechanism of strain-induced grain boundary migration and the discontinuous coarsening reaction is proposed for the formation of PFZs. Furthermore, PFZs were considered to be potential crack sources during the creep rupture test, leading to earlier failure of the material.
引用
收藏
页数:22
相关论文
共 50 条
  • [1] Fatigue behavior of welded joints of a Ni-Fe-based superalloy
    Huang, Xin
    Qi, Hongyu
    Li, Shaolin
    Yang, Xiaoguang
    Shi, Duoqi
    WELDING IN THE WORLD, 2025, 69 (03) : 657 - 669
  • [2] Oxide-Scale Evolution on a New Ni-Fe-Based Superalloy at High Temperature
    Zhang, Huawei
    Yang, Zhi
    Wu, Zhaoyu
    Hong, Xiaoyu
    Li, Zhong
    Xu, Yulai
    Li, Jun
    Ni, Gaojin
    Xiao, Xueshan
    OXIDATION OF METALS, 2019, 92 (1-2): : 49 - 65
  • [3] Research of the microstructure and precipitation strengthening in a high-temperature Fe-Ni superalloy
    Ducki, K. J.
    TECHNOLOGIES AND PROPERTIES OF MODERN UTILISED MATERIALS (TPMUM 2012), 2012, 35
  • [4] Microstructure Modeling of a Ni-Fe-Based Superalloy During the Rotary Forging Process
    A. Loyda
    G. M. Hernández-Muñoz
    L. A. Reyes
    P. Zambrano-Robledo
    Journal of Materials Engineering and Performance, 2016, 25 : 2128 - 2137
  • [5] Microstructure Modeling of a Ni-Fe-Based Superalloy During the Rotary Forging Process
    Loyda, A.
    Hernandez-Munoz, G. M.
    Reyes, L. A.
    Zambrano-Robledo, P.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (06) : 2128 - 2137
  • [6] Effects of High-Temperature Aging on Precipitation and Corrosion Behavior of a Ni-Cr-Mo-Based Hastelloy C276 Superalloy
    Chi Zhang
    Liwen Zhang
    Yan Cui
    Qiyan Feng
    Congqian Cheng
    Journal of Materials Engineering and Performance, 2020, 29 : 2026 - 2034
  • [7] Effects of High-Temperature Aging on Precipitation and Corrosion Behavior of a Ni-Cr-Mo-Based Hastelloy C276 Superalloy
    Zhang, Chi
    Zhang, Liwen
    Cui, Yan
    Feng, Qiyan
    Cheng, Congqian
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (03) : 2026 - 2034
  • [8] Evolution of residual stress in dissimilar welded rotor joint of novel Ni-Fe-based/Ni-based superalloy during welding and heat treatment
    Zhang, Wuhua
    Yang, Zhengang
    Huo, Xin
    Li, Kejian
    Liu, Qu
    Wu, Yao
    Fan, Manjie
    Cai, Zhipeng
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2025,
  • [9] THE CHARACTERISTIC OF DEFORMABILITY OF Fe-Ni SUPERALLOY DURING HIGH-TEMPERATURE DEFORMATION
    Ducki, Kazimierz
    Mendala, Jacek
    Wojtynek, Lilianna
    27TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2018), 2018, : 348 - 353
  • [10] Evolution of the microstructure and microhardness of a new wrought Ni-Fe based superalloy during high temperature aging
    Zhao, Xinbao
    Dang, Yingying
    Yin, Hongfei
    Yuan, Yong
    Lu, Jintao
    Yang, Zhen
    Gu, Yuefeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 644 : 66 - 70