Preparation of (BN-SiC)n composite coatings on SiC fibers and tensile properties of monofilament

被引:0
|
作者
Jia L. [1 ]
Wang M. [1 ]
Xu H. [1 ]
Li A. [1 ]
Peng Y. [1 ]
机构
[1] Research Center for Composite Materials, School of Materials Science and Engineering, Shanghai University, Shanghai
关键词
Chemical vapor deposition; Composite coatings; Microstructure; Monofilament tensile; SiC;
D O I
10.13801/j.cnki.fhclxb.20181025.003
中图分类号
学科分类号
摘要
In order to prepare an ideal interphase of continuous fiber reinforced ceramic composite, three types of (BN-SiC)n composite coatings were deposited on the surface of SiC fibers by chemical vapor deposition (CVD). The microstructure of the (BN-SiC)n coatings was characterized. The monofilament tensile properties of SiC fibers with various (BN-SiC)n coatings were investigated. The results show that the (BN-SiC)n coatings deposited on the SiC fibers are dense and uniform. The tensile strength of SiC fibers monofilament decreases with the increasing coating layers. The SiC fibers with single BN coating have the high monofilament strength retention of about 70% and the maximum elongation of about 2.3%. Compared to the original SiC fiber, the monofilament tensile properties of SiC fibers with (BN-SiC)1 and (BN-SiC)2 composite coatings decrease obviously, and the tensile strength retention rates are 42.1% and 32.3%, respectively. © 2019, Editorial Office of Acta Materiae Compositae Sinica. All right reserved.
引用
收藏
页码:1873 / 1878
页数:5
相关论文
共 31 条
  • [1] Donald I.W., Mcmillan P.W., Ceramic-matrix composites, Journal of Materials Science, 11, 5, pp. 949-972, (1976)
  • [2] Zhang L., Cheng L., Discussion on strategies of sustainable development of continuous fiber reinforced ceramic matrix composites, Acta Materiae Compositae Sinica, 24, 2, pp. 1-6, (2007)
  • [3] Jiao J., Chen M., New Generation of high-temperature material for engine: Preparation, property and application of ceramic matrix composite, Aeronautical Manufacturing Technology, 7, pp. 62-69, (2014)
  • [4] Li J., Zhang L., Cheng L., Et al., Interfacial zone in continuous fiber-reinforced ceramic composites, Rare Metal Materials and Engineering, 36, 9, pp. 1539-1544, (2007)
  • [5] Ren J., Zhao Y., Zhang M., The progress of fiber reinforced ceramic matrix composite interface and toughening mechanism, Industrial Technology and Occupational Education, 2, pp. 3-6, (2013)
  • [6] Cai L., Ma Q., Liu H., Et al., Research progress in interfacial zone of continuous fiber reinforced SiC composites, Bulletin of the Chinese Ceramic Society, 32, 5, pp. 878-883, (2013)
  • [7] Shi Y., Huang M., Yang W., Et al., Influence of fiber pre-coating on mechanical properties and interfacial structures of SiC(f)/SiC composites, Journal of Inorganic Materials, 16, 5, pp. 883-888, (2001)
  • [8] Mueller W.M., Moosburger-Will J., Sause M.G.R., Et al., Quantification of crack area in ceramic matrix composites at single-fiber push-out testing and influence of pyrocarbon fiber coating thickness on interfacial fracture toughness, Journal of the European Ceramic Society, 35, 11, pp. 2981-2989, (2015)
  • [9] Roger R.N., Pailler J.F., Lamon J.L., Single- and multi-layered interphases in SiC/SiC composites exposed to severe environmental conditions: An overview, International Journal of Applied Ceramic Technology, 7, 3, pp. 263-275, (2010)
  • [10] Zhang X., Deng J., Wang L., Et al., Phase transformation in BN films by nitrogen-protected annealing at atmospheric pressure, Applied Surface Science, 254, 21, pp. 7109-7113, (2008)