Research progress on dissimilar materials joining

被引:0
|
作者
Feng J. [1 ]
机构
[1] State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin
基金
中国国家自然科学基金;
关键词
Arc welding; Brazing; Dissimilar materials; Electron beam welding; Friction stir welding; Laser welding;
D O I
10.7527/S1000-6893.2021.26413
中图分类号
学科分类号
摘要
Dissimilar material structures could realize the combination of dissimilar materials with excellent performance, which improves the flexibility in design and production and meets the demand for function and properties in modern engineering structures. These structures have been widely used in many fields due to their higher technological and economic value. Therefore, reliable joining of dissimilar materials is becoming increasingly important. Nevertheless, the great difference in physical and chemical properties between dissimilar materials poses a huge challenge to achieve reliable joining. This work reviewed the research status and development on brazing, laser welding, electron beam welding, arc welding, and friction stir welding of dissimilar materials in China and abroad. Based on this, summaries and prospects about dissimilar joining are given, which provides a reference for research interests and technology breakthrough in the future study. © 2022, Beihang University Aerospace Knowledge Press. All right reserved.
引用
收藏
相关论文
共 168 条
  • [1] EUSTATHOPOULOS N, LANDRY K., Dynamics of wetting in reactive metal/ceramic systems: Linear spreading, Acta Materialia, 44, 10, pp. 3923-3932, (1996)
  • [2] DEZELLUS O, HODAJ F, EUSTATHOPOULOS N., Chemical reaction-limited spreading: the triple line velocity versus contact angle relation, Acta Materialia, 50, 19, pp. 4741-4753, (2002)
  • [3] MORTENSEN A, DREVET B, EUSTATHOPOULOS N., Kinetics of diffusion-limited spreading of sessile drops in reactive wetting, Scripta Materialia, 36, 6, pp. 645-651, (1997)
  • [4] YANG L, SHEN P, LIN Q, Et al., Effect of Cr on the wetting in Cu/graphite system, Applied Surface Science, 257, 14, pp. 6276-6281, (2011)
  • [5] SAIZ E, TOMSIA A P., Kinetics of high-temperature spreading, Current Opinion in Solid State and Materials Science, 9, 4-5, pp. 167-173, (2005)
  • [6] CHIHIRO I, SHUN-ICHIRO T., Reactive wetting of Ag-Cu-Ti on SiC in HRTEM, Acta Materialia, 46, 7, pp. 2381-2386, (1998)
  • [7] NOMURA M, ICHIMORI T, IWAMOTO C, Et al., Structure of wetting front in the Ag-Cu-Ti/SiC reactive system, Journal of Materials Science, 35, 16, pp. 3953-3958, (2000)
  • [8] GREMILLARD L, SAIZA E, CHEVALIERB J, Et al., Wetting and strength in the tin-silver-titanium/sapphire system, Zeitschrift Für Metallkunde, 95, 4, pp. 261-265, (2004)
  • [9] FU W, SONG X G, ZHAO Y X, Et al., Effect of Ti content on the wetting behavior of Sn0.3Ag0.7Cu/AlN system, Materials & Design, 115, pp. 1-7, (2017)
  • [10] SONG X, PASSERONE A, FU W, Et al., Wetting and spreading behavior of Sn-Ti alloys on SiC, Materialia, 3, pp. 57-63, (2018)