共 34 条
- [1] WU Q H, WENG L, ZHAO Y, Et al., On the tensile mechanical characteristics of fine-grained granite after heating/cooling treatments with different cooling rates, Engineering Geology, 253, pp. 94-110, (2019)
- [2] SHE S G, LIN P., Several progress and challenges of Chinese rock engineering, Chinese Journal of Rock Mechanics and Engineering, 33, 3, pp. 433-457, (2014)
- [3] YU L Y, SU H J, JING H W, Et al., Experimental study of the mechanical behavior of sandstone affected by blasting, International Journal of Rock Mechanics & Mining Sciences, 93, pp. 234-241, (2017)
- [4] FAN X, CHEN R, LIN H, Et al., Cracking and failure in rock specimen containing combined flaw and hole under uniaxial compression, Advances in Civil Engineering, pp. 1-15, (2018)
- [5] GONG S X, MEGUID S A., A general solution to the antiplane problem of an arbitrarily located elliptical hole near the tip of a main crack, International Journal of Fracture, 28, 2, pp. 249-263, (1991)
- [6] MEGUID S A, WANG X D., The dynamic interaction of a crack with a circular hole under antiplane loading, Journal of the Mechanics and Physics of Solids, 43, 22, pp. 1857-1871, (1995)
- [7] YANG R S, ZUO J J, FANG S Z, Et al., Experimental study on the effect of circular hole defect on the growth behavior of explosive crack, Vibration and Impact, 37, 12, pp. 174-178, (2018)
- [8] LI M, ZHU Z M, LIU R F, Et al., Effect of void on dynamic propagation behavior of explosive crack, Journal of Geotechnical Engineering, 40, 12, pp. 2191-2199, (2018)
- [9] WANG Q Z, FENG F, NI M, Et al., Measurement of mode Ⅰ and mode Ⅱ rock dynamic fracture toughness with cracked straight through flattened Brazilian disc impacted by split Hopkinson pressure bar, Engineering Fracture Mechanics, 78, 12, pp. 2455-2469, (2011)
- [10] WANG M, ZHU Z M, DONG Y Q, Et al., Study of mixed-mode Ⅰ/Ⅱ fractures using single cleavage semicircle specimens under impacting loads [J], Engineering Fracture Mechanics, 177, pp. 33-44, (2017)