Highly Stable Ni-B/Honeycomb-Structural Al2O3 Catalysts for Dry Reforming of Methane

被引:0
|
作者
Luo, Yuhao [1 ]
Su, Tongming [1 ]
Chen, Liuyun [1 ]
Ji, Hongbing [1 ,2 ]
Qin, Zuzeng [1 ]
机构
[1] Guangxi Univ, Sch Chem & Chem Engn, 100 Daxue Rd, Nanning 530004, Peoples R China
[2] Zhejiang Univ Technol, Inst Green Petr Proc & Light Hydrocarbon Convers, Coll Chem Engn, 288 Liuhe Rd, Hangzhou 310023, Peoples R China
基金
中国国家自然科学基金;
关键词
Honeycomb-structural; Dry reforming of methane; Stability; Intrinsic kinetics; Coke tolerance; CARBON DEPOSITION; ENHANCED ACTIVITY; RESISTANCE;
D O I
10.1002/asia.202400700
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Two-component catalysts have garnered significant attention in the field of catalysis due to their ability to inhibit Ni sintering. In the present work, honeycomb-structuralstructured Al2O3-supported Ni and B were prepared to enhance coke tolerance during dry reforming of methane (DRM). Transmission electron microscopy (TEM) results revealed that the average particle sizes on Ni/Al2O3 and Ni-0.16B/Al2O3 were 7.6 nm and 4.2 nm, respectively, indicating that B can effectively inhibit Ni sintering. After a 100-hour reaction, the conversion of CH4 and CO2 on Ni/Al2O3 decreased by approximately 5 %, whereas on Ni-0.16B/Al2O3, there was no significant decrease in CH4 and CO2 conversion, with values of approximately 81.6 % and 87.2 %, respectively. In situ DRIFT spectra demonstrated that Ni-0.16B/Al2O3 enhanced the activation of CO2, thus improving the catalyst's stability. A Langmuir-Hinshelwood-Hougen-Watson (LHHW) model was developed for intrinsic kinetics, and the resulting kinetic expressions were well-fitted fit to the experimental data, with R-2 values exceeding 0.9. ActivationThe activation energies were also calculated. The outstanding stability of Ni-0.16B/Al2O3 can be attributed to its stable honeycomb structure and B ' s ability to significantly inhibit Ni sintering, reduce catalyst particle size, and enhance coke tolerance.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Stabilizing Ni on honeycomb-structural Al2O3 with enhanced coke tolerance for dry reforming of methane
    Luo, Yuhao
    Su, Tongming
    Song, Peng
    Chen, Liuyun
    Xie, Xinling
    Luo, Xuan
    Ji, Hongbing
    Qin, Zuzeng
    MOLECULAR CATALYSIS, 2024, 562
  • [2] Stable Ni/Al2O3 catalysts for methane dry reforming Effects of pretreatment
    Alberto Becerra
    Marta Dimitrijewits
    Carlos Arciprete
    Adolfo Castro Luna
    Granular Matter, 2001, 3 : 79 - 81
  • [3] Stable Ni/Al2O3 catalysts for methane dry reforming -: Effects of pretreatment
    Becerra, A
    Dimitrijewits, M
    Arciprete, C
    Luna, AC
    GRANULAR MATTER, 2001, 3 (1-2) : 79 - 81
  • [4] Methane reforming reactions over stable Ni/θ-Al2O3 catalysts
    Roh, HS
    Jun, KW
    Dong, WS
    Baek, SC
    Park, SE
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2002, 8 (05) : 464 - 471
  • [5] Highly stable ytterbium promoted Ni/γ-Al2O3 catalysts for carbon dioxide reforming of methane
    Amin, Mohamad Hassan
    Mantri, Kshudiram
    Newnham, Jarrod
    Tardio, James
    Bhargava, Suresh K.
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2012, 119 : 217 - 226
  • [6] Dry reforming of methane to test passivation stability of Ni/ Al2O3 catalysts
    Franz, Robert
    Tichelaar, Frans D.
    Uslamin, Evgeny A.
    Pidko, Evgeny A.
    APPLIED CATALYSIS A-GENERAL, 2021, 612
  • [7] Ni-Re alloy catalysts on Al2O3 for methane dry reforming
    Cichy, Marcin
    Panczyk, Monika
    Slowik, Grzegorz
    Zawadzki, Witold
    Borowiecki, Tadeusz
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (37) : 16528 - 16543
  • [8] A study of refractory carbon deposits on Ni/Al2O3 catalysts for dry reforming of methane
    Kwon, Yongtak
    Eichler, J. Ehren
    Floto, Michael E.
    Smith, Lettie A.
    Satkoski, Aaron M.
    Mullins, C. Buddie
    CHEMISTRYSELECT, 2023, 8 (08):
  • [9] Preparation of nanocrystalline Ni/Al2O3 catalysts with the microemulsion method for dry reforming of methane
    Shiraz, Mohammad Hossein Aboonasr
    Rezaei, Mehran
    Meshkani, Fereshteh
    CANADIAN JOURNAL OF CHEMICAL ENGINEERING, 2016, 94 (06): : 1177 - 1183
  • [10] Effects of alumina morphology on dry reforming of methane over Ni/Al2O3 catalysts
    Shen, Dongyang
    Huo, Miaomiao
    Li, Lin
    Lyu, Shuai
    Wang, Juhan
    Wang, Xiaoyan
    Zhang, Yuhua
    Li, Jinlin
    CATALYSIS SCIENCE & TECHNOLOGY, 2020, 10 (02) : 510 - 516