Effects of mechanical surface pre-treatment on integrity and corrosion of bare and coated AA6082 substrates

被引:1
|
作者
Blawert, Carsten [1 ]
Serdechnova, Maria [1 ]
Bertram, Jan [2 ]
Momber, Andreas [2 ]
Konchakova, Natalia [1 ]
Hoche, Daniel [1 ]
Zheludkevich, Mikhail L. [1 ,3 ]
机构
[1] Helmholtz Zentrum Hereon, Inst Surface Sci, Max Planck Str 1, D-21502 Geesthacht, Germany
[2] Muehlhan Holding GmbH, Sachsenstr 8, D-20097 Hamburg, Germany
[3] CAU Kiel Univ, Fac Engn, Kaiserstr 2, D-24143 Kiel, Germany
关键词
Blast-cleaning; Coating adhesion; Cyclic corrosion test; Corrosion and adhesion measurements; Marine corrosion; AA6082; ALUMINUM-ALLOY; HARDNESS; 2024-T4;
D O I
10.1016/j.jmrt.2024.06.097
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, two classes of surface pre-treatment methods, namely three blast-cleaning methods with different abrasive materials (for initial preparation) and three mechanical methods (for repair applications) were applied to study their effects on surface morphology, composition, and corrosion of AA6082 substrates in artificial seawater. Coating adhesion and coating corrosion protection ability were investigated by applying a single-layer epoxy coating (250 mu m dry film thickness) onto the substrates. The mechanical methods delivered cleaner surfaces with more regular surface morphologies, whereas the blast-cleaning methods revealed less clean surfaces and more irregular surface morphologies. The latter methods promoted the detrimental embedment of abrasive particles into the substrates. The corrosion performance of the pre-treated substrates was worse after blast-cleaning compared to mechanical treatments. However, all methods met the adhesion requirements for offshore applications. Regarding coating degradation, only the filiform corrosion test delivered meaningful results, whereas the duration of the cyclic corrosion test (3000 h) was too short to distinguish between the different methods because of neglectable degradation. Mechanical interlocking and isotropic surface morphologies are found to be more important for coating performance than a cleaner surface, and the remains of blasting material were neglectable too.
引用
收藏
页码:844 / 859
页数:16
相关论文
共 50 条
  • [1] Pre-Corrosion and Surface Treatments Effects on the Fatigue Life of AA6082 T6
    Abdulstaar, Mustafa
    Mhaede, Mansour
    Wagner, Lothar
    ADVANCED ENGINEERING MATERIALS, 2013, 15 (10) : 1002 - 1006
  • [2] Adhesive joining of aluminium AA6082: The effects of resin and surface treatment
    Borsellino, C.
    Di Bella, G.
    Ruisi, V. F.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2009, 29 (01) : 36 - 44
  • [3] Adhesive joining of aluminium AA6082: The effects of resin and surface treatment
    Borsellino, C.
    Di Bella, G.
    Ruisi, V.F.
    International Journal of Adhesion and Adhesives, 2009, 29 (01): : 36 - 44
  • [4] Effects of pre-anodizing and phosphates on energy consumption and corrosion performance of PEO coatings on AA6082
    Mohedano, M.
    Mingo, B.
    Mora-Sanchez, H.
    Matykina, E.
    Arrabal, R.
    SURFACE & COATINGS TECHNOLOGY, 2021, 409 (409):
  • [5] A Study on the Synergistic Effect of ECAP and Aging Treatment on the Mechanical Properties of AA6082
    Baig, Muneer
    El-Danaf, Ehab
    Mohammed, Jabair Ali
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (12) : 5252 - 5261
  • [6] A Study on the Synergistic Effect of ECAP and Aging Treatment on the Mechanical Properties of AA6082
    Muneer Baig
    Ehab El-Danaf
    Jabair Ali Mohammed
    Journal of Materials Engineering and Performance, 2016, 25 : 5252 - 5261
  • [7] Corrosion Behavior of Laser-Brazed Surface Made by Joining of AA6082 and Galvanized Steel
    Narsimhachary, D.
    Rai, P. K.
    Shariff, S. M.
    Padmanabham, G.
    Mondal, K.
    Basu, A.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (04) : 2115 - 2127
  • [8] Corrosion Behavior of Laser-Brazed Surface Made by Joining of AA6082 and Galvanized Steel
    D. Narsimhachary
    P. K. Rai
    S. M. Shariff
    G. Padmanabham
    K. Mondal
    A. Basu
    Journal of Materials Engineering and Performance, 2019, 28 : 2115 - 2127
  • [9] The effect of post-weld heat treatment on the mechanical properties of AA6082 to welds
    Feng, F
    Li, ZF
    ALUMINUM 2001: PROCEEDINGS OF THE TMS 2001 ANNUAL MEETING ALUMINUM AUTOMOTIVE AND JOINING SYMPOSIA, 2001, : 129 - 138
  • [10] Effects of cryogenic temperature and pre-stretching on mechanical properties and deformation characteristics of a peak-aged AA6082 extrusion
    Xu, Zebing
    Roven, Hans J.
    Jia, Zhihong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 679 : 379 - 390